Silicone latex solvent thickening

Assignee: Dow Silicones Corp
•
Filing: 1996-02-05
•
Granted: 1997-09-09
•
Expires: 2016-02-05
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The viscosity of a solvent is modified by thickening the solvent with a silicone latex. A silicone latex having a plurality of crosslinked polysiloxane particles is first prepared by mixing the siloxane polymer, a surfactant, and water; emulsifying the mixture to a gel phase; diluting the emulsion with water; adding a cure package (i.e., a catalyst, a crosslinker, or both, or a self catalytic crosslinker); and then without removing the water from the latex and after the particles of siloxane polymer in the latex have been cured, mixing the latex and solvent to thicken the solvent, forming viscous liquids, gels, and pastes. These latex thickened solvent compositions have beneficial properties such as clarity, shelf stability, and ease of preparation; and therefore have wide areas of application, especially as additives in antiperspirants, deodorants, and other personal care applications.

Inventors

  • 👤 Michael Philip Louis Hill
  • 👤 Eric Jude Joffre
  • 👤 Linda Moy Madore

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 07:55
CPC Classifications
A; A61; A61K; A61K8/00; A61K8/18; A61K8/72; A61K8/84; A61K8/89; A61K8/895; A61K8/30; A61K8/58; A61K8/585; A61K8/891; A61Q; A61Q19/00; B; B01; B01J; B01J19/00; B01J19/06; C; C08; C08J; C08J3/00; C08J3/02; C08J3/09; C09; C09D; C09D7/00; C09D7/40; C09D7/43; C09D7/44; A61Q13/00; A61Q15/00; A61Q5/00; A61Q5/12; C08J2383/00; C08J2383/04; C08L; C08L83/00; C08L83/04

Claims Analysis

Total Claims: 17
Claim 1
Independent Claim 216 words
A method of modifying the viscosity of a solvent, the method comprising (I) adding a silicone latex containing water and a plurality of cured crosslinked polysiloxane particles to a solvent after the particles have been cured and without removing the water from the cured particles in the latex; and (II) mixing the latex containing the water and the cured particles and the solvent together to thicken the solvent; the latex being prepared by a method comprising: (A) mixing (i) 100 weight parts of a siloxane polymer having a viscosity of greater than 5,000 mPa.s but less than 500,000 mPa.s at 25° C., (ii) 0.5-10 weight parts of a surfactant, and (iii) 0.5-25 weight parts of water, (B) emulsifying the mixture into a gel phase having a siloxane polymer content of at least 80% by weight; (C) diluting the emulsion with further water to a siloxane polymer content of at least 75% by weight, (D) adding 0.00001-20 weight parts catalyst either before or after the emulsification, or before or after the dilution; (E) adding 0.1-20 weight parts crosslinker either before or after the emulsification, or before or after the dilution; or in place of adding (D) and (E), adding 1-5 weight parts self catalytic crosslinker either before or after the emulsification, or before or after the dilution.
Claim 2
Independent Claim 216 words
A method of modifying the viscosity of a solvent, the method comprising (I) adding a silicone latex containing water and a plurality of cured crosslinked polysiloxane particles to a solvent after the particles have been cured and without removing the water from the cured particles in the latex; and (II) mixing the latex containing the water and the cured particles and the solvent together to thicken the solvent; the latex being prepared by a method comprising: (A) mixing (i) 100 weight parts of a siloxane polymer having a viscosity of greater than 5,000 mPa.s but less than 500,000 mPa.s at 25° C., (ii) 0.5-10 weight parts of a surfactant, and (iii) 0.5-25 weight parts of water, (B) emulsifying the mixture into a gel phase having a siloxane polymer content of at least 80% by weight; (C) diluting the emulsion with further water to a siloxane polymer content of at least 75% by weight, (D) adding 0.00001-20 weight parts catalyst either before or after the emulsification, or before or after the dilution; (E) adding 0.1-20 weight parts crosslinker either before or after the emulsification, or before or after the dilution; or in place of adding (D) and (E), adding 1-5 weight parts self catalytic crosslinker either before or after the emulsification, or before or after the dilution.
Claim 3
Dependent Claim 24 words
A method according to claim 1 in which the latex has a solids content of siloxane polymer of at least 90 percent by weight.
Claim 4
Dependent Claim 129 words
A method according to claim 1 in which the siloxane polymer has the formula X 3-n R n --YO--(R 1 2 SiO) z --Y--R n X 3-n where n is 0, 1, 2 or 3; z is an integer from 500-5,000; X is hydrogen, a vinyl group, a hydroxyl group, a condensable or hydrolyzable group; Y is a silicon atom, the group .tbd.Si--(CH 2 ) m --SiR 1 2 --, or the group .tbd.Si--(CH 2 ) m --SiR 1 2 OSiR 1 2 (CH 2 )m--SiR 1 2 --, where m is 1-8; R is selected from the group consisting of aliphatic alkyl, aminoalkyl, polyaminoalkyl, epoxyalkyl, alkenyl, and an aromatic group; and R 1 is selected from the group consisting of X, aliphatic alkyl, alkenyl, and an aromatic group.
Claim 5
Dependent Claim 70 words
A method according to claim 3 in which the siloxane polymer has at least two vinyl groups per molecule bonded to a silicon atom, the crosslinker having an average of at least two silicon-bonded hydrogen atoms and being a silicon hydride crosslinker present in an amount sufficient to provide at least one hydrogen atom for each vinyl group in the siloxane polymer, and the catalyst is a noble metal catalyst.
Claim 6
Dependent Claim 31 words
A method according to claim 1 in which the self catalyzing crosslinker has at least one catalytic leaving group selected from the group consisting of acetoxy, amide, acetamide, aminoxy, and oxime.
Claim 7
Dependent Claim 46 words
A method according to claim 5 in which the self catalyzing crosslinker is a compound of the formula ##STR8## where R is the same or a different alkyl group of 1-8 carbon atoms; a is zero or a positive integer, and b is greater than two.
Claim 8
Dependent Claim 28 words
A method according to claim 1 in which the surfactant is selected from the group consisting of nonionic surfactants, cationic surfactants, anionic surfactants, amphoteric surfactants, and mixtures thereof.
Claim 9
Dependent Claim 50 words
A method according to claim 1 in which the solvent is selected from the group consisting of aromatic hydrocarbons, aliphatic hydrocarbons, alcohols, aldehydes, ketones, amines, esters, ethers, glycols, glycol ethers, alkyl halides, aromatic halides, petroleum hydrocarbons, lubricating oils, fatty oils, organic polysiloxanes, functional polysiloxanes, volatile methyl siloxanes, and mixtures thereof.
Claim 10
Dependent Claim 14 words
A latex thickened solvent composition prepared according to the method described in claim 1.
Claim 11
Dependent Claim 26 words
A latex thickened solvent composition according to claim 9 containing 5-40 percent by weight of the silicone latex and 60-95 percent by weight of the solvent.
Claim 12
Dependent Claim 92 words
A personal care product containing the latex thickened solvent composition of claim 9 selected from the group consisting of antiperspirants, deodorants, skin creams, skin care lotions, moisturizers, acne removers, wrinkle removers, facial cleansers, bath oils, perfumes, colognes, sachets, sunscreens, pre-shave lotions, after-shave lotions, shaving soaps, shaving lathers, hair shampoos, hair conditioners, hair sprays, mousses, permanents, depilatories, cuticle coats, make-ups, color cosmetics, foundations, blushes, lipsticks, eyeliners, mascaras, oil removers, cosmetic removers, delivery systems for oil and water soluble substances, and powders; including products in the form of sticks, gels, lotions, aerosols, and roll-ons.
Claim 13
Dependent Claim 25 words
A method of treating hair or skin comprising applying to the hair or skin a composition containing the latex thickened solvent composition of claim 9.
Claim 14
Dependent Claim 32 words
A product containing the latex thickened solvent composition of claim 9 and a material selected from the group consisting of crosslinked silicone rubber particles, pharmaceuticals, biocides, herbicides, pesticides, water, and water-soluble substances.
Claim 15
Dependent Claim 46 words
A method of modifying rheological, physical, or energy absorbing properties, of silicone or organic phases selected from the group consisting of sealants, paints, coatings, greases, adhesives, antifoams, and potting compounds, comprising incorporating therein the latex thickened solvent composition of claim 9 containing crosslinked silicone rubber particles.
Claim 16
Dependent Claim 20 words
A method of filling or insulating an electrical cable comprising incorporating therein the latex thickened solvent composition of claim 9.
Claim 17
Dependent Claim 21 words
A method of stabilizing in-ground soil or water barriers comprising incorporating into soil the latex thickened solvent composition of claim 9.

References Cited (Backward Citations)

US4743670A Cited
EP0304946A2 Cited
US5266321A Cited
US5064894A Cited
US4980167A Cited
US5092922A Cited
US4990556A Cited
US5089253A Cited
EP0545002A1 Cited
US5399342A Cited
EP0647672A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 2000-09-08 2001-03-10 2001-09-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2004-09-08 2005-03-10 2005-09-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2008-09-08 2009-03-10 2009-09-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag