US5521113A Expired / Lapsed US ⏱️ 0.0 years remaining

Process for forming a butting contact through a gate electrode

Assignee: United Microelectronics Corp
•
Filing: 1995-03-16
•
Granted: 1996-05-28
•
Expires: 2015-03-16
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An SRAM cell includes a semiconductor substrate doped with a dopant of a first type, a highly doped region in the substrate implanted with a dopant of opposite type, a gate oxide layer on the substrate, a first conductive layer formed upon the gate oxide layer, a dielectric layer deposited over the first conductive layer, an opening in the gate oxide layer, the first conductive layer, and the dielectric layer, and a second conductive layer deposited upon the dielectric layer.

Inventors

  • 👤 Chen-Chiu Hsue
  • 👤 Sun-Chieh Chien

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-01 19:07
CPC Classifications
H; H10; H10B; H10B10/00; H10B10/15; Y; Y10; Y10S; Y10S148/00; Y10S148/02

Claims Analysis

Total Claims: 22
Claim 1
Independent Claim 402 words
A method of manufacture of an SRAM cell comprising: forming a gate oxide layer on a semiconductor substrate doped with a dopant of a first conductivity type with a field oxide region on at least one end of said gate oxide layer, forming a first mask over said semiconductor substrate including said field oxide region and said gate oxide layer with a mask opening located over said gate oxide layer, performing a first ion implantation of ions through said mask opening into said substrate to form a first highly doped region of an opposite conductivity type from said dopant of said first conductivity type in said substrate located below said gate oxide layer, removing said first mask, forming a first conductive layer upon said gate oxide layer, forming a first electrode mask over said first conductive layer leaving unwanted portions of said first conductive layer exposed, etching away said unwanted portions of said first conductive layer exposing portions of said gate oxide layer below said unwanted portions of said first conductive layer providing a first gate electrode of said SRAM cell formed from said first conductive layer over said first highly doped region, said gate electrode having a top surface, forming a spacer on said exposed gate oxide at an edge of said first gate electrode, removing said first electrode mask and forming a lightly doped region adjacent to said first highly doped region, then depositing a blanket dielectric layer over said cell including said top surface of said first gate electrode, forming a third mask over said dielectric layer with an opening therein leaving an unwanted portion of said dielectric layer exposed said opening being located above said top surface of said gate electrode, etching through said opening in third mask to remove said unwanted portion of said dielectric layer thereby exposing a newly exposed portion of said top surface of said first gate electrode, and then etching through said newly exposed portion of said first gate electrode thereby exposing a newly exposed portion of said gate oxide layer and then etching through said newly exposed portion of said gate oxide layer down to said first highly doped region in said substrate thereby forming a butting contact opening therein, forming a second conductive layer upon said dielectric layer extending down through said butting contact opening into contact with said first gate electrode and into contact with said first highly doped region.
Claim 2
Independent Claim 402 words
A method of manufacture of an SRAM cell comprising: forming a gate oxide layer on a semiconductor substrate doped with a dopant of a first conductivity type with a field oxide region on at least one end of said gate oxide layer, forming a first mask over said semiconductor substrate including said field oxide region and said gate oxide layer with a mask opening located over said gate oxide layer, performing a first ion implantation of ions through said mask opening into said substrate to form a first highly doped region of an opposite conductivity type from said dopant of said first conductivity type in said substrate located below said gate oxide layer, removing said first mask, forming a first conductive layer upon said gate oxide layer, forming a first electrode mask over said first conductive layer leaving unwanted portions of said first conductive layer exposed, etching away said unwanted portions of said first conductive layer exposing portions of said gate oxide layer below said unwanted portions of said first conductive layer providing a first gate electrode of said SRAM cell formed from said first conductive layer over said first highly doped region, said gate electrode having a top surface, forming a spacer on said exposed gate oxide at an edge of said first gate electrode, removing said first electrode mask and forming a lightly doped region adjacent to said first highly doped region, then depositing a blanket dielectric layer over said cell including said top surface of said first gate electrode, forming a third mask over said dielectric layer with an opening therein leaving an unwanted portion of said dielectric layer exposed said opening being located above said top surface of said gate electrode, etching through said opening in third mask to remove said unwanted portion of said dielectric layer thereby exposing a newly exposed portion of said top surface of said first gate electrode, and then etching through said newly exposed portion of said first gate electrode thereby exposing a newly exposed portion of said gate oxide layer and then etching through said newly exposed portion of said gate oxide layer down to said first highly doped region in said substrate thereby forming a butting contact opening therein, forming a second conductive layer upon said dielectric layer extending down through said butting contact opening into contact with said first gate electrode and into contact with said first highly doped region.
Claim 3
Dependent Claim 81 words
The method of claim 1 wherein after removing of said first electrode mask, performing a lightly doped ion implantation forming a lightly doped region in said substrate adjacent to said first highly doped region using said first gate electrode as a self-aligned mask, said doping of said lightly doped region including a dose of N-type ions implanted within the range between about 1×10 13 /cm 2 and about 5×10 13 /cm 2 at between about 40 keV and about 80 keV.
Claim 4
Dependent Claim 19 words
A method in accordance with claim 1 wherein said dopant of said first conductivity type is P type impurity.
Claim 5
Dependent Claim 24 words
A method in accordance with claim 3 wherein said dopant of said opposite conductivity type from said first conductivity type is N type impurity.
Claim 6
Dependent Claim 33 words
A method in accordance with claim 2 wherein a spacer is formed adjacent to the edge of said first conductive layer, on said gate oxide layer subsequent to said lightly doped ion implantation.
Claim 7
Dependent Claim 62 words
A method in accordance with claim 5 wherein additional dopants are implanted into said substrate adjacent to said lightly doped region aside from said spacer using said first gate electrode combined with said spacer as a self-aligned mask to protect portions of said substrate including said first highly doped region and a portion of said lightly doped region from said additional dopants.
Claim 8
Dependent Claim 21 words
A method in accordance with claim 6 wherein said first highly doped region is formed adjacent to said field oxide regions.
Claim 9
Independent Claim 347 words
A method of manufacture of an SRAM cell comprising: forming a gate oxide layer on a semiconductor substrate doped with a dopant of a first conductivity type, forming a first mask over said semiconductor substrate including said gate oxide layer with a mask opening located over said gate oxide layer, performing a first ion implantation of ions through said mask opening into said substrate to form a first highly doped region of an opposite conductivity type from said first conductivity type of dopant in said semiconductor substrate located below said gate oxide layer, removing said first mask, forming a first conductive layer upon said gate oxide layer, forming a gate electrode mask over said first conductive layer leaving unwanted portions of said first conductive layer exposed, etching away said unwanted portions of said first conductive layer exposing portions of said gate oxide layer below said unwanted portions of said first conductive layer providing a gate electrode of said SRAM cell, said gate electrode having a top surface, removing said gate electrode mask, forming a spacer on said exposed gate oxide at an edge of said gate electrode, and forming a highly doped region adjacent to said first highly doped region, forming an additional blanket dielectric layer over said cell covering said cell including said gate electrode and said lightly doped region, forming a third mask over said additional blanket dielectric layer with an opening therein leaving an unwanted portion of said additional blanket dielectric layer exposed, said opening being located above said top surface of said gate electrode, etching through said opening in said third mask an opening through said unwanted portion of said additional blanket dielectric layer, a hole therebelow through said gate electrode and a hole therebelow through said gate oxide layer down to said first highly doped region in said substrate through said opening in said third mask forming a butting contact opening therein, and forming a second conductive layer upon said additional blanket dielectric layer extending down through said butting contact opening into contact with gate electrode and said first highly doped region.
Claim 10
Independent Claim 347 words
A method of manufacture of an SRAM cell comprising: forming a gate oxide layer on a semiconductor substrate doped with a dopant of a first conductivity type, forming a first mask over said semiconductor substrate including said gate oxide layer with a mask opening located over said gate oxide layer, performing a first ion implantation of ions through said mask opening into said substrate to form a first highly doped region of an opposite conductivity type from said first conductivity type of dopant in said semiconductor substrate located below said gate oxide layer, removing said first mask, forming a first conductive layer upon said gate oxide layer, forming a gate electrode mask over said first conductive layer leaving unwanted portions of said first conductive layer exposed, etching away said unwanted portions of said first conductive layer exposing portions of said gate oxide layer below said unwanted portions of said first conductive layer providing a gate electrode of said SRAM cell, said gate electrode having a top surface, removing said gate electrode mask, forming a spacer on said exposed gate oxide at an edge of said gate electrode, and forming a highly doped region adjacent to said first highly doped region, forming an additional blanket dielectric layer over said cell covering said cell including said gate electrode and said lightly doped region, forming a third mask over said additional blanket dielectric layer with an opening therein leaving an unwanted portion of said additional blanket dielectric layer exposed, said opening being located above said top surface of said gate electrode, etching through said opening in said third mask an opening through said unwanted portion of said additional blanket dielectric layer, a hole therebelow through said gate electrode and a hole therebelow through said gate oxide layer down to said first highly doped region in said substrate through said opening in said third mask forming a butting contact opening therein, and forming a second conductive layer upon said additional blanket dielectric layer extending down through said butting contact opening into contact with gate electrode and said first highly doped region.
Claim 11
Dependent Claim 41 words
The method of claim 8 wherein after removing said first electrode mask a second ion implantation is performed forming a lightly doped region in said substrate adjacent to said first highly doped region using said gate electrode as a self-aligned mask.
Claim 12
Dependent Claim 150 words
A method in accordance with claim 9 wherein following removing of said gate electrode mask a dielectric spacer layer is deposited over said semiconductor substrate, etching said dielectric spacer layer to form a spacer from said dielectric spacer layer at an end of said gate electrode and to strip portions of said gate oxide layer, performing an additional ion implantation of ions to said substrate to form a second highly doped region of an opposite conductivity type from said first conductivity type located in said substrate below said gate oxide layer, aside from said spacer using said gate electrode combined with said spacer as a self-aligned mask to protect portions of said substrate including said first highly doped region from said additional ions, and when said additional blanket dielectric layer is deposited said additional blanket dielectric layer covers said spacer and said lightly doped region and second highly doped region.
Claim 13
Dependent Claim 19 words
A method in accordance with claim 8 wherein said dopant of said first conductivity type is P type impurity.
Claim 14
Dependent Claim 19 words
A method in accordance with claim 8 wherein said dopant of said opposite conductivity type is N type impurity.
Claim 15
Dependent Claim 44 words
A method in accordance with claim 1 wherein said first ion implantation includes a dose of arsenic (As) ions implanted within the range between about 5×10 14 /cm 2 and about 5×10 15 /cm 2 at between about 50 keV and about 120 keV.
Claim 16
Dependent Claim 44 words
A method in accordance with claim 8 wherein said first ion implantation includes a dose of arsenic (As) ions implanted within the range between about 5×10 14 /cm 2 and about 5×10 15 /cm 2 at between about 50 keV and about 120 keV.
Claim 17
Dependent Claim 115 words
A method in accordance with claim 1 wherein said first ion implantation includes a dose of arsenic (As) ions implanted within a range between about 5×10 14 /cm 2 and about 5×10 15 /cm 2 at between about 50 keV and about 120 keV, following removing said first electrode mask by forming a lightly doped region in said substrate adjacent to said first highly doped region using said first electrode as a self-aligned mask, said lightly doped region being formed by ion implantation with a dose of P 31 ions implanted within a range between about 1×10 13 /cm 2 and about 5×10 13 /cm 2 at between about 40 keV and about 80 keV.
Claim 18
Dependent Claim 115 words
A method in accordance with claim 8 wherein said first ion implantation includes a dose of arsenic (As) ions implanted within a range between about 5×10 14 /cm 2 and about 5×10 15 /cm 2 at between about 50 keV and about 120 keV, following removing said gate electrode mask by forming a lightly doped region in said substrate adjacent to said first highly doped region using said first electrode as a self-aligned mask, said lightly doped region being formed by ion implantation with a dose of P 31 ions implanted within a range between about 1×10 13 /cm 2 and about 5×10 13 /cm 2 at between about 40 keV and about 80 keV.
Claim 19
Dependent Claim 229 words
A method in accordance with claim 1 wherein said first ion implantation includes a dose of arsenic (As) ions implanted within the range between about 5×10 14 /cm 2 and about 5×10 15 /cm 2 at between about 50 keV and about 120 keV, then after removing said first electrode mask, forming a lightly doped region in said substrate adjacent to said first highly doped region, said lightly doped region being formed by ion implantation with a dose of P 31 ions implanted within a range between about 1×10 13 /cm 2 and about 5×10 13 /cm 2 at between about 40 keV and about 80 keV using said first electrode as a self-aligned mask, performing a second highly doped ion implantation of ions into said substrate to form a second highly doped region of an opposite conductivity type to said first conductivity type located in said substrate below said gate oxide layer, aside from said spacer using said first electrode combined with said spacer as a self-aligned mask to protect portions of said substrate including said lightly doped region from an additional level of dopant, and said second highly doped region is formed by ion implantation with a dose of arsenic (As) ions implanted within a range between about 1×10 15 /cm 2 and about 5×10 15 /cm 2 at between about 50 keV and about 100 keV.
Claim 20
Dependent Claim 33 words
A method in accordance with claim 9 wherein a spacer is formed adjacent to the edge of said first conductive layer, on said gate oxide layer subsequent to said lightly doped ion implantation.
Claim 21
Independent Claim 419 words
A method of manufacture of an SRAM cell comprising: forming a gate oxide layer on a semiconductor substrate doped with a dopant of a first conductivity type with field oxide regions on either end of said gate oxide layer, forming a first mask over said field oxide regions and said gate oxide layer with a first mask opening located over said gate oxide layer, performing an ion implantation of second conductivity type impurities through said first mask opening into said substrate to form a first highly doped region of second conductivity type impurities located below said gate oxide layer, removing said first mask, forming a conductive gate electrode layer of said SRAM cell upon said gate oxide layer, forming a gate electrode mask over said conductive gate electrode layer leaving unwanted areas of said conductive gate electrode layer exposed, etching away said unwanted areas of said conductive gate electrode layer to form a gate electrode with a patterned edge superjacent said first highly doped second conductivity type region, ion implanting a lightly doped second conductivity type region in said substrate adjacent to said first highly doped second conductivity type region and said patterned edge of said first gate electrode which serves as a self-aligned mask, forming a dielectric spacer on said patterned edge of said gate electrode, performing an ion implantation of second conductivity type impurities forming a second highly doped region of second conductivity type impurities in said substrate adjacent to said first highly doped second conductivity type region and said patterned edge and said spacer with said second highly doped region of second conductivity type impurities located contiguous to said lightly doped second conductivity type region on the other side from said first highly doped second conductivity type region, depositing a dielectric layer after forming said second highly doped second conductivity type region, forming a second mask over said dielectric layer with an opening therein leaving an unwanted portion of said dielectric layer exposed, etching through said opening in said second mask to remove said unwanted portion of said dielectric layer and then etching through an exposed portion of said gate electrode and then etching through an exposed portion of said gate oxide layer down to said first highly doped second conductivity type region in said substrate thereby forming a butting contact opening therein, forming a conductive layer upon said dielectric layer extending down through said butting contact opening into contact with said gate electrode and into contact with said first highly doped second conductivity type region.
Claim 22
Independent Claim 419 words
A method of manufacture of an SRAM cell comprising: forming a gate oxide layer on a semiconductor substrate doped with a dopant of a first conductivity type with field oxide regions on either end of said gate oxide layer, forming a first mask over said field oxide regions and said gate oxide layer with a first mask opening located over said gate oxide layer, performing an ion implantation of second conductivity type impurities through said first mask opening into said substrate to form a first highly doped region of second conductivity type impurities located below said gate oxide layer, removing said first mask, forming a conductive gate electrode layer of said SRAM cell upon said gate oxide layer, forming a gate electrode mask over said conductive gate electrode layer leaving unwanted areas of said conductive gate electrode layer exposed, etching away said unwanted areas of said conductive gate electrode layer to form a gate electrode with a patterned edge superjacent said first highly doped second conductivity type region, ion implanting a lightly doped second conductivity type region in said substrate adjacent to said first highly doped second conductivity type region and said patterned edge of said first gate electrode which serves as a self-aligned mask, forming a dielectric spacer on said patterned edge of said gate electrode, performing an ion implantation of second conductivity type impurities forming a second highly doped region of second conductivity type impurities in said substrate adjacent to said first highly doped second conductivity type region and said patterned edge and said spacer with said second highly doped region of second conductivity type impurities located contiguous to said lightly doped second conductivity type region on the other side from said first highly doped second conductivity type region, depositing a dielectric layer after forming said second highly doped second conductivity type region, forming a second mask over said dielectric layer with an opening therein leaving an unwanted portion of said dielectric layer exposed, etching through said opening in said second mask to remove said unwanted portion of said dielectric layer and then etching through an exposed portion of said gate electrode and then etching through an exposed portion of said gate oxide layer down to said first highly doped second conductivity type region in said substrate thereby forming a butting contact opening therein, forming a conductive layer upon said dielectric layer extending down through said butting contact opening into contact with said gate electrode and into contact with said first highly doped second conductivity type region.

References Cited (Backward Citations)

US4785341A Cited
US5422499A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-05-28 1999-11-27 2000-05-28 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-05-28 2003-11-27 2004-05-28 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-05-28 2007-11-27 2008-05-28 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag