US5516583A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Adhesive for tamper evident seals
Assignee: EIDP Inc
•
Filing: 1994-08-29
•
Granted: 1996-05-14
•
Expires: 2014-08-29
Abstract
Abstract The inventive adhesive composition provides a whitening effect upon peeling. The composition comprises (A) ethylene vinyl acetate polymer, ethylene acrylate polymer or mixtures thereof; (B) a styrene polymer, and optionally (C) a polyolefin.
Inventors
- 👤 David D. Zhang
- 👤 I-Hwa Lee
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-31 20:51
CPC Classifications
C; C09; C09J; C09J123/00; C09J123/02; C09J123/04; C09J123/08; C08; C08L; C08L2666/00; C08L2666/02; C08L2666/04; Y; Y10; Y10T; Y10T428/00; Y10T428/28; Y10T428/2852; Y10T428/2878; Y10T428/2891
Claims Analysis
Total Claims: 2
Claim 1
Independent Claim
155 words
An adhesive resin composition consisting essentially of: (A) 50 to 90 wt % ethylene-vinyl acetate polymer having a vinyl acetate content of greater than 7 wt % and less than 20 wt % of the total ethylene-vinyl acetate polymer, an ethylene-acrylate polymer or mixtures thereof; (B) 10 to 50 wt % of a styrene homopolymer, or a styrene copolymer derived from: 4-n-butylstyrene; 4-t-butylstyrene; 2,4-diisopropylstyrene; 2,5-dimethylstyrene, hydroxystyrene; 3,4-diethylstyrene, 2-hydroxymethylstyrene; 4-methylstyrene; or 2-methylstyrene, with the weight percent being based on components (A) and (B) and (C) optionally, one or more modifying polymers produced by means of a Ziegler-type catalyst or a metallocene type catalyst and having a melt flow rate of 0.1 to 50 g/10 min., a density of about 0.820 to 0.970 g/cc and a melting point of about 60° to 170° C., said modifying polymers being a member of the group consisting of: an ethylene homopolymer, an ethylene copolymer; propylene homopolymer and a propylene copolymer.
Claim 2
Dependent Claim
155 words
An adhesive resin composition consisting essentially of: (A) 50 to 90 wt % ethylene-vinyl acetate polymer having a vinyl acetate content of greater than 7 wt % and less than 20 wt % of the total ethylene-vinyl acetate polymer, an ethylene-acrylate polymer or mixtures thereof; (B) 10 to 50 wt % of a styrene homopolymer, or a styrene copolymer derived from: 4-n-butylstyrene; 4-t-butylstyrene; 2,4-diisopropylstyrene; 2,5-dimethylstyrene, hydroxystyrene; 3,4-diethylstyrene, 2-hydroxymethylstyrene; 4-methylstyrene; or 2-methylstyrene, with the weight percent being based on components (A) and (B) and (C) optionally, one or more modifying polymers produced by means of a Ziegler-type catalyst or a metallocene type catalyst and having a melt flow rate of 0.1 to 50 g/10 min., a density of about 0.820 to 0.970 g/cc and a melting point of about 60° to 170° C., said modifying polymers being a member of the group consisting of: an ethylene homopolymer, an ethylene copolymer; propylene homopolymer and a propylene copolymer.
References Cited (Backward Citations)
US3644252A
Cited
US4361237A
Cited
US5037700A
Cited
US4427744A
Cited
US4670349A
Cited
US4772650A
Cited
US4910085A
Cited
US4855335A
Cited
US4861677A
Cited
US4931327A
Cited
US5319016A
Cited
US5225482A
Cited
US5250349A
Cited
US5270358A
Cited
US5178946A
Cited
US5252395A
Cited
US5310060A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1999-05-14 | 1999-11-13 | 2000-05-14 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2003-05-14 | 2003-11-13 | 2004-05-14 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2007-05-14 | 2007-11-13 | 2008-05-14 | $7700.00 | Window Closed / Lapsed |