US5486949A Expired / Lapsed US ⏱️ 0.0 years remaining

Birefringent interference polarizer

Assignee: 3M Innovative Properties Co
•
Filing: 1990-11-26
•
Granted: 1996-01-23
•
Expires: 2010-11-26
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A birefringent interference polarizer which may be fabricated from readily available materials using established coextrusion techniques is provided. The polarizer has a level of light absorption near zero and can be fabricated to polarize and reflect light of specific wavelengths while transmitting light of other wavelengths. The polarizer includes multiple alternating oriented layers of at least first and second polymeric materials having respective nonzero stress optical coefficients which are sufficiently different to produce a refractive index mismatch between the first and second polymeric materials in a first plane which is different from the refractive index mismatch between the first and second polymeric materials in a second plane normal to the first plane. The refractive index mismatch in the first plane is preferably at least 0.03.

Inventors

  • 👤 Walter J. Schrenk
  • 👤 John A. Wheatley
  • 👤 Victor S. Chang

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 10:03
CPC Classifications
B; B32; B32B; B32B27/00; B32B27/06; B32B27/08; G; G02; G02B; G02B5/00; G02B5/30; B32B27/18; B32B27/20; B32B27/36; B32B33/00; B32B7/00; B32B7/02; B32B7/023; G02B1/00; G02B1/04; G02B1/08; G02B5/08; G02B5/0816; G02B5/0825; G02B5/0841; G02B5/0883; G02B5/20; G02B5/26; G02B5/3025; G02B5/3033; G02B5/3041; G02B5/305; B32B2307/00; B32B2307/40; B32B2307/418; B32B2307/50; B32B2307/514; B32B2307/516; B32B2367/00; B32B2369/00; G02F; G02F1/00; G02F1/01; G02F1/13; G02F1/133; G02F1/1333; G02F1/1335; G02F1/133528; G02F1/133545; Y; Y10; Y10S; Y10S359/00; Y10S359/90

Claims Analysis

Total Claims: 12
Claim 1
Independent Claim 98 words
A method of making a birefringent interface polarizer comprising the steps of: providing at least first and second polymeric materials having respective nonzero stress optical coefficients, coextruding said first and second polymeric materials in multiple alternating layers in which said layers increase in thickness to produce a player thickness gradient, and stretching said layers such that said first and second polymeric materials become oriented and produce a refractive index mismatch in a first plane which is different from the refractive index mismatch between said first and second polymeric materials in a second plane normal to said first plane.
Claim 2
Independent Claim 98 words
A method of making a birefringent interface polarizer comprising the steps of: providing at least first and second polymeric materials having respective nonzero stress optical coefficients, coextruding said first and second polymeric materials in multiple alternating layers in which said layers increase in thickness to produce a player thickness gradient, and stretching said layers such that said first and second polymeric materials become oriented and produce a refractive index mismatch in a first plane which is different from the refractive index mismatch between said first and second polymeric materials in a second plane normal to said first plane.
Claim 3
Dependent Claim 43 words
The method of claim 1 in which said first and second polymeric materials have a glass transition temperature and wherein said stretching step is carried out at a temperature above the glass transition temperature but below the melting temperature of said polymeric materials.
Claim 4
Dependent Claim 20 words
The method of claim 1 in which said first and second polymeric materials have substantially equal refractive indices when unoriented.
Claim 5
Dependent Claim 46 words
The method of claim 1 in which said refractive index mismatch in one of said planes increases while said refractive index mismatch in the other plane decreases such that said oriented first and second polymeric materials have substantially equal refractive indices in one of said planes.
Claim 6
Dependent Claim 16 words
The method of claim 1 in which said first and second polymeric materials are uniaxially oriented.
Claim 7
Dependent Claim 28 words
The method of claim 1 in which said first polymeric material has a positive stress optical coefficient and said second polymeric material has a negative stress optical coefficient.
Claim 8
Dependent Claim 19 words
The method of claim 1 in which said refractive index mismatch in the first plane is at least 0.03.
Claim 9
Dependent Claim 22 words
The method of claim 1 in which the optical thickness of each layer is from about 0.09 micrometers to about 0.70 micrometers.
Claim 10
Dependent Claim 22 words
The method of claim 1 in which said first polymeric material is selected from the group consisting of polycarbonates and polyethylene terephthalates.
Claim 11
Dependent Claim 33 words
The method of claim 1 in which said second polymeric material is selected from the group consisting of polystyrene, copolymers of styrene and acrylonitrile, copolymers of styrene and methyl methacrylate, and polyethylene naphthalate.
Claim 12
Dependent Claim 15 words
The method of claim 1 in which said second polymeric material is a syndiotactic polystyrene.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1999-01-22 1999-07-24 2000-01-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2003-01-22 2003-07-24 2004-01-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2007-01-22 2007-07-24 2008-01-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag