← Back to Patent Explorer
US5425839A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for rapidly etching material on a semiconductor device

Assignee: Texas Instruments Inc
•
Filing: 1992-05-14
•
Granted: 1995-06-20
•
Expires: 2012-05-14
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Apparatus and methods for precise processing of thin materials in a process chamber by the use of ellipsometer monitoring is disclosed. The process includes rapidly etching a layer 42 of material covering a semiconductor device. The process includes placing the semiconductor wafer 14 into a processing chamber 10. In a typical operation, the wafer 14 will include a selected substrate 32 having a first thin layer 30 of material covering the substrate 32 and then a second layer 42 of a different material covering the first layer 30. A process such as reactive ion anisotropic etching which rapidly etches the second layer 42 is initiated and this etching is monitored in situ by an ellipsometer in combination with a controller 28 to determine the thickness of the second layer 42' which has been achieved. Once the desired amount of second layer 42 remains, the rapid etching process stops to leave a residual layer 42' such as about 250 Å or in a preferred embodiment a thickness equivalent to about one molecular layer. A second chemical isotropic etching process step then starts which may be substantially ineffective at etching the first layer 30 of material and which etching process consequently is typically substantially slower than the first etching process. Since only a very thin layer remains, the slow speed or isotropic nature of the second etching process does not take an unacceptable amount of time or cause other problems, such as loss of critical dimension.

Inventors

  • 👤 Steven A. Henck

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 03:37
CPC Classifications
G; G01; G01B; G01B11/00; G01B11/02; G01B11/06; G01B11/0616; G01B11/0641; G01B11/065

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 90 words
A method for processing a layer of material used in the fabrication of semiconductor devices comprising the steps of: placing a semiconductor device in a processing chamber, said semiconductor device having a first layer of a material covering portions of the surface of a second layer of said material; etching said first layer; monitoring in situ the thickness of said first layer during said etching and substantially in real-time using an ellipsometer; stopping said etching of said first layer so as to leave a residual layer having a selected thickness.
Claim 2
Independent Claim 90 words
A method for processing a layer of material used in the fabrication of semiconductor devices comprising the steps of: placing a semiconductor device in a processing chamber, said semiconductor device having a first layer of a material covering portions of the surface of a second layer of said material; etching said first layer; monitoring in situ the thickness of said first layer during said etching and substantially in real-time using an ellipsometer; stopping said etching of said first layer so as to leave a residual layer having a selected thickness.
Claim 3
Dependent Claim 36 words
The method of claim 1 wherein said steps of monitoring includes obtaining a plurality of thickness measurements during said etching and further including the step of determining an etching rate from said plurality of thickness measurements.
Claim 4
Dependent Claim 26 words
The method of claim 2 wherein said etching is stopped after a period of time as determined by said etching rate to obtain said selected thickness.
Claim 5
Dependent Claim 18 words
The method of claim 1 wherein said step of etching comprises the step of anisotropic reactive ion etching.
Claim 6
Independent Claim 143 words
A method for etching a layer of material used in the fabrication of semiconductor devices comprising the steps of: placing a semiconductor device in a processing chamber, said semiconductor device having a first layer of a material covering portions of the surface of a second layer of said material, said second layer covering said substrate; etching said first layer with a first etching process in said chamber; monitoring in situ and in real-time with an ellipsometer the thickness of said first layer during said etching with said first process; stopping said etching of said first layer with said first etching process so as to leave a residual layer of said first layer; and etching said residual layer with a second etching process to remove said first layer and expose said second layer said second etching process being different than said first etching process.
Claim 7
Independent Claim 143 words
A method for etching a layer of material used in the fabrication of semiconductor devices comprising the steps of: placing a semiconductor device in a processing chamber, said semiconductor device having a first layer of a material covering portions of the surface of a second layer of said material, said second layer covering said substrate; etching said first layer with a first etching process in said chamber; monitoring in situ and in real-time with an ellipsometer the thickness of said first layer during said etching with said first process; stopping said etching of said first layer with said first etching process so as to leave a residual layer of said first layer; and etching said residual layer with a second etching process to remove said first layer and expose said second layer said second etching process being different than said first etching process.
Claim 8
Dependent Claim 21 words
The method of claim 5 wherein said step of etching with a second etching process comprises the step of isotropic etching.
Claim 9
Dependent Claim 25 words
The method of claim 5 wherein said step of etching with a second etching process occurs at a slower rate than said first etching process.
Claim 10
Dependent Claim 18 words
The method of claim 5 wherein said step of etching comprises the step of anisotropic reactive ion etching.
Claim 11
Independent Claim 81 words
A method for processing a layer of material used in the fabrication of semiconductor devices comprising the steps of: placing a semiconductor device in a processing chamber, said semiconductor device having a first layer of a material covering portions of the surface of a second layer of said material; etching said first layer; monitoring in situ the thickness of said first layer during said etching and in real-time using an ellipsometer; stopping said etching once said first layer has been removed.
Claim 12
Independent Claim 81 words
A method for processing a layer of material used in the fabrication of semiconductor devices comprising the steps of: placing a semiconductor device in a processing chamber, said semiconductor device having a first layer of a material covering portions of the surface of a second layer of said material; etching said first layer; monitoring in situ the thickness of said first layer during said etching and in real-time using an ellipsometer; stopping said etching once said first layer has been removed.
Claim 13
Dependent Claim 18 words
The method of claim 9 wherein said step of etching comprises the step of anisotropic reactive ion etching.

References Cited (Backward Citations)

US4105338A Cited
US4218924A Cited
US4332833A Cited
US4434025A Cited
JPS593925A Cited
US4838694A Cited
JPS63254733A Cited
US4927485A Cited
JPH0382120A Cited
US5002631A Cited
US5131752A Cited
JPH0482217A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1998-06-19 1998-12-19 1999-06-20 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2002-06-19 2002-12-19 2003-06-20 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2006-06-19 2006-12-19 2007-06-20 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag