Claims Analysis
Total Claims: 23
Claim 1
Independent Claim
223 words
A paintable olefinic composition comprising, in weight percent based upon the total weight of the composition: A. about 30 to about 70 percent graft-modified polypropylene or a blend of polypropylene and graft-modified polypropylene; B. a nongrafted substantially linear ethylene polymer or a graft-modified substantially linear polymer or a blend of nongrafted substantially linear ethylene polymer and graft-modified substantially linear polymer, present in an amount from greater than 0 to about 40 percent; and C. an interpolymer of ethylene and an α,β-unsaturated carbonyl comonomer or an interpolymer of ethylene and carbon monoxide comonomer, the interpolymer present in an amount from greater than 0 up to about 50 percent; with provisos that: (i) the sum of components B and C is between about 30 and about 70 wt. % of the composition; and (ii) the substantially linear ethylene polymer is characterized as having (a) a melt flow ratio defined by the equation: I.sub.10 /I.sub.2 ≧5.63 (b) a molecular weight distribution defined by the equation: M.sub.w /M.sub.n ≦(I.sub.10 /I.sub.2)-4.63 (c) a density greater than about 0.850 g/cm 3 ; and (d) a critical shear rate at onset of surface melt fracture of at least 50 percent greater than the critical shear rate at the onset of surface melt fracture of a linear olefin polymer having about the same I 2 and M w /M n .
Claim 2
Dependent Claim
223 words
A paintable olefinic composition comprising, in weight percent based upon the total weight of the composition: A. about 30 to about 70 percent graft-modified polypropylene or a blend of polypropylene and graft-modified polypropylene; B. a nongrafted substantially linear ethylene polymer or a graft-modified substantially linear polymer or a blend of nongrafted substantially linear ethylene polymer and graft-modified substantially linear polymer, present in an amount from greater than 0 to about 40 percent; and C. an interpolymer of ethylene and an α,β-unsaturated carbonyl comonomer or an interpolymer of ethylene and carbon monoxide comonomer, the interpolymer present in an amount from greater than 0 up to about 50 percent; with provisos that: (i) the sum of components B and C is between about 30 and about 70 wt. % of the composition; and (ii) the substantially linear ethylene polymer is characterized as having (a) a melt flow ratio defined by the equation: I.sub.10 /I.sub.2 ≧5.63 (b) a molecular weight distribution defined by the equation: M.sub.w /M.sub.n ≦(I.sub.10 /I.sub.2)-4.63 (c) a density greater than about 0.850 g/cm 3 ; and (d) a critical shear rate at onset of surface melt fracture of at least 50 percent greater than the critical shear rate at the onset of surface melt fracture of a linear olefin polymer having about the same I 2 and M w /M n .
Claim 3
Dependent Claim
17 words
The composition of claim 1 in which component (A) is a blend of polypropylene and graft-modified polypropylene.
Claim 4
Dependent Claim
19 words
The composition of claim 2 in which component (A) comprises at least about 50 wt % of graft-modified polypropylene.
Claim 5
Dependent Claim
20 words
The composition of claim 3 in which component (B) is between about 10 and 30 wt % of the composition.
Claim 6
Dependent Claim
23 words
The composition of claim 4 in which component (B) comprises at least about 50 wt % of the nongrafted substantially linear ethylene polymer.
Claim 7
Dependent Claim
26 words
The composition of claim 5 in which the density of the nongrafted substantially linear ethylene polymer is between about 0.850 to about 0.920 g/cm 3 .
Claim 8
Dependent Claim
20 words
The composition of claim 6 in which component (C) comprises between about 10 and 40 wt % of the composition.
Claim 9
Dependent Claim
38 words
The composition of claim 7 in which component (C) is selected from the group consisting of ethylene/acrylic acid copolymer, ethylene/methacrylic acid copolymer, ethylene/vinyl acetate copolymer, ethylene/carbon monoxide copolymer, ethylene/propylene/carbon monoxide terpolymer, ethylene/carbon monoxide/acrylic acid terpolymer, and mixtures thereof.
Claim 10
Dependent Claim
29 words
The composition of claim 1 in which the graft-modified polypropylene is graft-modified with at least about 0.01 wt %, based on the weight of the polypropylene, of maleic anhydride.
Claim 11
Dependent Claim
32 words
The composition of claim 1 in which the graft-modified substantially linear ethylene polymer is graft-modified with at least about 0.01 wt %, based on the weight of the polymer, of maleic anhydride.
Claim 12
Dependent Claim
14 words
The composition of claim 8 in which component (C) is an ethylene/acrylic acid copolymer.
Claim 13
Dependent Claim
30 words
The composition of claim 11 in which the ethylene/acrylic acid copolymer contains about 3 to about 20 wt %, based on the weight of the copolymer, acrylic acid monomer units.
Claim 14
Dependent Claim
23 words
The composition of claim 1 in which component (C) is at least one of an ethylene/carbon monoxide copolymer and an ethylene/propylene/carbon monoxide terpolymer.
Claim 15
Dependent Claim
10 words
A fabricated article made from the composition of claim 1.
Claim 16
Dependent Claim
9 words
The fabricated article of claim 14 made by extrusion.
Claim 17
Dependent Claim
10 words
The fabricated article of claim 14 made by injection molding.
Claim 18
Dependent Claim
10 words
The fabricated article of claim 14 made by compression molding.
Claim 19
Dependent Claim
11 words
A painted fabricated article made from the composition of claim 1.
Claim 20
Dependent Claim
10 words
The painted article of claim 18 made by injection molding.
Claim 21
Dependent Claim
10 words
The painted article of claim 18 made by compression molding.
Claim 22
Dependent Claim
163 words
A paintable olefinic composition consisting essentially of, in weight percent based upon the total weight of the composition about: A. 40 to about 60 percent graft-modified polypropylene; B. 10 to about 30 percent nongrafted substantially linear ethylene polymer; and C. 10 to about 40 percent ethylene/acrylic acid copolymer; with the provisos that: (i) the sum of components B and C is between about 40 and 60 wt % of the composition; and (ii) the substantially linear ethylene polymer is characterized as having: (a) a melt flow ratio defined by the equation: I.sub.10 /I.sub.2 ≧5.63; (b) a molecular weight distribution defined by the equation: M.sub.w /M.sub.n ≦(I.sub.10 /I.sub.2)-4.63; (c) a density greater than about 0.850 g/cm 3; and (d) a critical shear rate at onset of surface melt fracture of at least 50 percent greater than the critical shear rate at the onset of surface melt fracture of a linear olefin polymer having about the same I 2 and M w /M n .
Claim 23
Dependent Claim
163 words
A paintable olefinic composition consisting essentially of, in weight percent based upon the total weight of the composition about: A. 40 to about 60 percent graft-modified polypropylene; B. 10 to about 30 percent nongrafted substantially linear ethylene polymer; and C. 10 to about 40 percent ethylene/acrylic acid copolymer; with the provisos that: (i) the sum of components B and C is between about 40 and 60 wt % of the composition; and (ii) the substantially linear ethylene polymer is characterized as having: (a) a melt flow ratio defined by the equation: I.sub.10 /I.sub.2 ≧5.63; (b) a molecular weight distribution defined by the equation: M.sub.w /M.sub.n ≦(I.sub.10 /I.sub.2)-4.63; (c) a density greater than about 0.850 g/cm 3; and (d) a critical shear rate at onset of surface melt fracture of at least 50 percent greater than the critical shear rate at the onset of surface melt fracture of a linear olefin polymer having about the same I 2 and M w /M n .