Ion conducting polymers
Assignee: Magna Donnelly Corp
•
Filing: 1992-08-31
•
Granted: 1994-04-05
•
Expires: 2012-08-31
Abstract
Abstract An ion conducting polymer composition is described which exhibits electrical conductivities of at least 10 -6 S/cm and has good optical properties and is easily processable. The composition comprises a PEO-based block copolymer and a dissociable lithium salt. The invention also includes a laminate formed from the ion conducting polymer composition, and related methods of forming.
Inventors
- 👤 Anoop Agrawal
- 👤 Frederick R. Grimes
- 👤 Pierre-Marc Allemand
- 👤 Michael Trosky, Jr.
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-26 11:49
CPC Classifications
H; H01; H01M; H01M10/00; H01M10/05; H01M10/056; H01M10/0564; H01M10/0565; C; C08; C08L; C08L71/00; C08L71/02; G; G02; G02F; G02F1/00; G02F1/01; G02F1/15; G02F1/1514; G02F1/1523; G02F1/1525; H01M10/052; Y; Y02; Y02E; Y02E60/00; Y02E60/10
Claims Analysis
Total Claims: 28
Claim 1
Independent Claim
56 words
An ion conducting polymer composition comprising: a block copolymer of the formula R'--(CH 2 CH 2 O) n --R", wherein the molecular weight of said block copolymer is less than about 5000, n is from about 5 to about 34, and R' and R" are flexible units; and an effective amount of a dissociable lithium salt.
Claim 2
Dependent Claim
56 words
An ion conducting polymer composition comprising: a block copolymer of the formula R'--(CH 2 CH 2 O) n --R", wherein the molecular weight of said block copolymer is less than about 5000, n is from about 5 to about 34, and R' and R" are flexible units; and an effective amount of a dissociable lithium salt.
Claim 3
Dependent Claim
74 words
An ion conducting polymer composition in accordance with claim 1 wherein said dissociable lithium salt is selected from the group comprising LiPF 6 , LiBF 4 , LiBr, LiN(SO 2 CF 3 ) 2 , LiI, LiNO 3 , LiSCN, LiB(C 6 H 5 ) 4 , LiAsF 6 , LiCF 3 COO, LiClO 4 , LiCF 3 SO 3 , LiSO 3 (CF 2 ) 3 SO 3 Li, and Li 2 S.
Claim 4
Dependent Claim
19 words
An ion polymer composition in accordance with claim 2 wherein said R' and said R" are both polypropylene oxide.
Claim 5
Dependent Claim
31 words
An ion conducting polymer composition in accordance with claim 3 wherein the molar ratio of ethylene oxide in said block copolymer to lithium cation is from about 6:1 to about 80:1.
Claim 6
Dependent Claim
15 words
An ion conducting polymer composition in accordance with claim 1 further comprising: a compatible plasticizer.
Claim 7
Dependent Claim
33 words
An ion conducting polymer composition in accordance with claim 5, wherein said plasticizer is selected from the group comprising propylene carbonate, ethylene glycol, glycerol, tetraethylene glycol, polyethylene glycol, propylene triol and propylene/ethylene triol.
Claim 8
Dependent Claim
16 words
An ion conducting polymer composition in accordance with claim 1 further comprising: a silane coupling agent.
Claim 9
Dependent Claim
63 words
An ion conducting polymer composition in accordance with claim 7 wherein said silane coupling agent is of the formula X'--(CH 2 ) m ---Si(OR'") 3 ; m is from about 2 to about 6; X' is selected from the group comprising glycidoxy, amino, mercapto, hydroxyl and acrylate; and R'" is selected from the group comprising --CH 3 and --CH 2 CH 3 .
Claim 10
Dependent Claim
29 words
An ion conducting polymer composition in accordance with claim 1 wherein said end groups R' and R" are selected from the group comprising polypropylene oxide, polyethyleneimine, polyphosphazine, and polysiloxane.
Claim 11
Dependent Claim
45 words
An ion conducting polymer composition in accordance with claim 1 wherein the ratio of the number of moles of ethylene oxide in said block copolymer to the number of moles of lithium cations in said dissociable lithium salt is from about 6:1 to about 80:1.
Claim 12
Dependent Claim
31 words
An ion conducting polymer composition in accordance with claim 10 wherein the molar ratio of ethylene oxide in said block copolymer to lithium cation is from about 6:1 to about 20:1.
Claim 13
Dependent Claim
22 words
An ion conducting polymer composition in accordance with claim 1 wherein said block copolymer has a molecular weight less than about 2500.
Claim 14
Dependent Claim
76 words
An ion conducting polymer composition in accordance with claim 1 further comprising: dangling branches primarily attached to at least one of said R' and R" groups, said dangling branches of the formula CH 3 (CH 2 CH 2 X) p Z; wherein p is from about 0 to about 10; X is selected from the group comprising oxygen, nitrogen, and sulfur; and Z is selected from the group comprising epoxy, glycidoxy, amino, mercapto, hydroxyl, and acrylate.
Claim 15
Independent Claim
136 words
A method of forming an ion conducting polymeric laminate between a first and a second substrate, each said substrate having two faces, said method comprising: preparing an ion conducting polymer composition comprising a block copolymer and an effective amount of a dissociable lithium salt, said block copolymer being of the formula R'--(CH 2 CH 2 O) n --R", wherein the molecular weight of said block copolymer is less than about 5000, n is from about 5 to about 34, and R' and R" are flexible units; depositing said composition onto one of said faces of said first substrate; contacting one of said faces of said second substrate with said composition deposited upon said first substrate such that a thin film of said composition is formed between said first and said second substrates; and curing said composition.
Claim 16
Independent Claim
136 words
A method of forming an ion conducting polymeric laminate between a first and a second substrate, each said substrate having two faces, said method comprising: preparing an ion conducting polymer composition comprising a block copolymer and an effective amount of a dissociable lithium salt, said block copolymer being of the formula R'--(CH 2 CH 2 O) n --R", wherein the molecular weight of said block copolymer is less than about 5000, n is from about 5 to about 34, and R' and R" are flexible units; depositing said composition onto one of said faces of said first substrate; contacting one of said faces of said second substrate with said composition deposited upon said first substrate such that a thin film of said composition is formed between said first and said second substrates; and curing said composition.
Claim 17
Dependent Claim
32 words
A method of forming an ion conducting polymeric laminate in accordance with claim 14 wherein said R' and said R" are selected from the group comprising polypropylene oxide, polyethyleneimine, polyphosphazine, and polysiloxane.
Claim 18
Dependent Claim
24 words
A method of forming an ion conducting polymeric laminate in accordance with claim 15 wherein said R' and said R" are both polypropylene oxide.
Claim 19
Dependent Claim
49 words
A method of forming an ion conducting polymeric laminate in accordance with claim 14 wherein the ratio of the number of moles of ethylene oxide in said block copolymer to the number of moles of lithium cations in said dissociable lithium salt is from about 6:1 to about 80:1.
Claim 20
Dependent Claim
49 words
A method of forming an ion conducting polymeric laminate in accordance with claim 17 wherein the ratio of the number of moles of ethylene oxide in said block copolymer to the number of moles of lithium cations in said dissociable lithium salt is from about 6:1 to about 20:1.
Claim 21
Dependent Claim
78 words
A method of forming an ion conducting polymeric laminate in accordance with claim 14 wherein said dissociable lithium salt is selected from the group comprising LiPF 6 , LiBF 4 , LiBr, LiN(SO 2 CF 3 ) 2 , LiI, LiNO 3 , LiSCN, LiB(C 6 H 5 ) 4 , LiAsF 6 , LiCF 3 COO, LiClO 4 , LiCF 3 SO 3 , LiSO 3 (CF 2 ) 3 SO 3 Li, and Li 2 S.
Claim 22
Dependent Claim
23 words
A method of forming an ion conducting polymeric laminate in accordance with claim 14 wherein said dissociable lithium salt is LiClO 4 .
Claim 23
Dependent Claim
25 words
A method of forming an ion conducting polymeric laminate in accordance with claim 14 wherein said dissociable lithium salt is LiCF 3 SO 3 .
Claim 24
Dependent Claim
26 words
A method of forming an ion conducting polymeric laminate in accordance with claim 14 wherein said block copolymer has a molecular weight less than about 2500.
Claim 25
Dependent Claim
93 words
An ion conducting polymeric laminate comprising: at least one substrate having at least one face; and a layer of ion conducting polymer composition comprising an ion conducting polymer and an effective amount of a dissociable lithium salt, said polymer composition contacting said one face of said substrate, wherein said ion conducting polymer comprises a block copolymer of the formula R'--(CH 2 CH 2 O) n --R", the molecular weight of said block copolymer is less than about 5000, n is from about 5 to about 34, and R' and R" are flexible units.
Claim 26
Dependent Claim
93 words
An ion conducting polymeric laminate comprising: at least one substrate having at least one face; and a layer of ion conducting polymer composition comprising an ion conducting polymer and an effective amount of a dissociable lithium salt, said polymer composition contacting said one face of said substrate, wherein said ion conducting polymer comprises a block copolymer of the formula R'--(CH 2 CH 2 O) n --R", the molecular weight of said block copolymer is less than about 5000, n is from about 5 to about 34, and R' and R" are flexible units.
Claim 27
Dependent Claim
80 words
An ion conducting polymer composition comprising: an ethylene oxide block copolymer having end groups R' and R", said end groups being flexible units, said copolymer having a molecular weight less than about 5000; and an effective amount of a dissociable lithium salt, wherein said composition before curing exhibits a viscosity of less than about 100 Poise and after curing, said composition exhibits a conductivity of at least about 10 -6 S/cm, and a luminous transmittance of at least about 70%.
Claim 28
Dependent Claim
80 words
An ion conducting polymer composition comprising: an ethylene oxide block copolymer having end groups R' and R", said end groups being flexible units, said copolymer having a molecular weight less than about 5000; and an effective amount of a dissociable lithium salt, wherein said composition before curing exhibits a viscosity of less than about 100 Poise and after curing, said composition exhibits a conductivity of at least about 10 -6 S/cm, and a luminous transmittance of at least about 70%.
References Cited (Backward Citations)
US4357401A
Cited
US4758483A
Cited
US5051211A
Cited
US4840856A
Cited
US4792504A
Cited
JPH0234660A
Cited
US5061581A
Cited
US5194490A
Cited
US5173205A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1997-04-04 | 1997-10-04 | 1998-04-05 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 2001-04-04 | 2001-10-04 | 2002-04-05 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2005-04-04 | 2005-10-04 | 2006-04-05 | $7700.00 | Window Closed / Lapsed |