Patent US5185240A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5185240A Expired / Lapsed US ⏱️ 0.0 years remaining

Silver halide photographic material

Assignee: Fujifilm Holdings Corp
•
Filing: 1990-08-10
•
Granted: 1993-02-09
•
Expires: 2010-08-10
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Disclosed is an autopositive silver halide photographic material which comprises at least one silver halide emulsion layer, characterized in that said emulsion layer or at least one other hydrophilic colloid layers contains at least one compound selected from the group consisting of compounds represented by the following general formulas (1), (2) and (3): ##STR1## wherein R 1 represents hydrogen atom or an alkyl group; and R 2 , R 3 and R 4 each represents hydrogen atom, a halogen atom, an alkyl group or an alkoxy group; ##STR2## wherein R 5 represents hydrogen atom or an alkyl group; and R 6 and R 7 each represents hydrogen atom, an alkyl group, a halogen atom or an aryl group; ##STR3## wherein R 8 represents a lower alkylene group; X represents a halogen atom, nitro group, hydroxy group, a cyano group, a lower alkyl group, a lower alkoxy group, ##STR4## or --SO 3 M; R 12 represents hydrogen atom, --OM, a lower alkyl group, a lower alkoxy group or ##STR5## R 13 and R 14 may be the same or different groups and each represents hydrogen atom, a lower alkyl group, --COR 17 or --SO 2 R 17 ; R 15 and R 16 may be the same or different groups and each represents hydrogen atom or a lower alkyl group; R 17 represents a lower alkyl group; M represents hydrogen atom, an alkali metal or an atomic group required for forming a monovalent cation; and n represents 0 or an integer of 1 to 5.

Inventors

  • 👤 Junji Miyata
  • 👤 Satoshi Kanetake
  • 👤 Yasufumi Morimoto
  • 👤 Kenji Hanayama

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 10:08
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/005; G03C1/06; G03C1/34; G03C1/485; G03C1/48515; Y; Y10; Y10S; Y10S430/00; Y10S430/141

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 254 words
An autopositive silver halide photographic material which comprises at least one silver halide emulsion layer wherein said emulsion layer or at least one other hydrophilic colloid layer contains at least one member selected from the group consisting of the compounds represented by the following general formulas (1), (2) and (3): ##STR17## wherein R 1 represents hydrogen atom or an alkyl group; and R 2 , R 3 and R 4 each represents hydrogen atom, a halogen atom, an alkyl group or an alkoxy group; ##STR18## wherein R 5 represents hydrogen atom or an alkyl group; and R 6 and R 7 each represents hydrogen atom, an alkyl group, a halogen atom or an aryl group; ##STR19## wherein R 8 represents a lower alkylene group; X represents a halogen atom, nitro group, hydroxy group, a cyano group, a lower alkyl group, a lower alkoxy group, --COR 12 , ##STR20## or --SO 3 M; R 12 represents hydrogen atom, --OM, a lower alkyl group, a lower alkoxy group or ##STR21## R 13 and R 14 may be the same or different groups and each represents hydrogen atom, a lower alkyl group, --COR 17 or --SO 2 R 17 ; R 15 and R 16 may be the same or different groups and each represents hydrogen atom or a lower alkyl group; R 17 represents a lower alkyl group; M represents hydrogen atom, an alkali metal or an atomic group required for forming a monovalent cation; and n represents 0 or an integer of 1 to 5.
Claim 2
Dependent Claim 254 words
An autopositive silver halide photographic material which comprises at least one silver halide emulsion layer wherein said emulsion layer or at least one other hydrophilic colloid layer contains at least one member selected from the group consisting of the compounds represented by the following general formulas (1), (2) and (3): ##STR17## wherein R 1 represents hydrogen atom or an alkyl group; and R 2 , R 3 and R 4 each represents hydrogen atom, a halogen atom, an alkyl group or an alkoxy group; ##STR18## wherein R 5 represents hydrogen atom or an alkyl group; and R 6 and R 7 each represents hydrogen atom, an alkyl group, a halogen atom or an aryl group; ##STR19## wherein R 8 represents a lower alkylene group; X represents a halogen atom, nitro group, hydroxy group, a cyano group, a lower alkyl group, a lower alkoxy group, --COR 12 , ##STR20## or --SO 3 M; R 12 represents hydrogen atom, --OM, a lower alkyl group, a lower alkoxy group or ##STR21## R 13 and R 14 may be the same or different groups and each represents hydrogen atom, a lower alkyl group, --COR 17 or --SO 2 R 17 ; R 15 and R 16 may be the same or different groups and each represents hydrogen atom or a lower alkyl group; R 17 represents a lower alkyl group; M represents hydrogen atom, an alkali metal or an atomic group required for forming a monovalent cation; and n represents 0 or an integer of 1 to 5.
Claim 3
Dependent Claim 156 words
An autopositive silver halide photographic material as in claim 1, wherein said silver halide emulsion has (1) a density of at least 2.0 when a sample is prepared by coating the emulsion in such an amount as to give a coating weight of 3.0 g/m 2 in terms of silver and the sample in an unexposed state is developed under the following conditions and (2) a density of not higher than 1.8 when the sample is exposed to tungsten light source (color temperature 2864K.) for (357) lux (100) seconds and then developed under the following conditions: (a) composition of developing solution: ______________________________________ Phenidone 0.8 g Hydroquinone 25 g Potassium bromide 3.3 g Sodium carbonate 10.8 g Potassium sulfite 67 g 5-Methylbenztriazole 0.2 g Ethylenediaminetetraacetic acid 2.8 g Sodium 2-mercaptobenzimidazole- 0.3 g 5-sulfonate Add KOH and H.sub.2 O to make 1 liter; and pH 10.7 ______________________________________ (b) development temperature, 38° C.; and (c) development time, 20 seconds.
Claim 4
Dependent Claim 36 words
An autopositive silver halide photographic material of claim 1, wherein the compounds represented by the general formula (1) or (2) are used in an amount of 5×10 -6 to 5×10 -3 mol per mol of silver.
Claim 5
Dependent Claim 35 words
An autopositive silver halide photographic material of claim 1, wherein the compounds represented by the general formula (3) are used in an amount of 2×10 -6 to 2×10 -1 mol per mol of silver halide.
Claim 6
Dependent Claim 16 words
An autopositive silver halide photographic material of claim 1, wherein said silver halide emulsion is monodisperse.
Claim 7
Dependent Claim 29 words
An autopositive silver halide photographic material of claim 1, wherein said emulsion layer or at least one other hydrophilic colloid layer contains a compound represented by general formula (1).
Claim 8
Dependent Claim 29 words
An autopositive silver halide photographic material of claim 1, wherein said emulsion layer or at least one other hydrophilic colloid layer contains a compound represented by general formula (2).
Claim 9
Dependent Claim 29 words
An autopositive silver halide photographic material of claim 1, wherein said emulsion layer or at least one other hydrophilic colloid layer contains a compound represented by general formula (3).

References Cited (Backward Citations)

US2870015A Cited
US3526507A Cited
US3501307A Cited
US3650759A Cited
US4059450A Cited
US4997752A Cited
US4923790A Cited
US5059516A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1996-02-09 1996-08-10 1997-02-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 2000-02-09 2000-08-10 2001-02-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2004-02-09 2004-08-10 2005-02-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag