Patent US5145749A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5145749A Expired / Lapsed US ⏱️ 0.0 years remaining

Coating composition and coated paper

Assignee: Image Products Group LLC
•
Filing: 1989-06-07
•
Granted: 1992-09-08
•
Expires: 2009-06-07
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Erasable coatings for xerography paper comprise a pigment such as calcium carbonate in a binder such as an aqueous emulsion of an acrylic polymer. The erasability of the coating is improved by replacing at least 15 wt % of the binder with a polyalkane or (preferably) polyalkene wax, such as an aqueous emulsion of a polyolefin.

Inventors

  • 👤 Michael K. Matthew

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 14:37
CPC Classifications
D; D21; D21H; D21H19/00; D21H19/36; D21H19/44; D21H19/56; D21H19/58; G; G03; G03G; G03G7/00; G03G7/0006; G03G7/002; G03G7/0026; G03G7/004; Y; Y10; Y10S; Y10S428/00; Y10S428/916; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31801; Y10T428/31804; Y10T428/31808; Y10T428/31855; Y10T428/3188; Y10T428/31895

Claims Analysis

Total Claims: 15
Claim 1
Independent Claim 118 words
Electrophotographic paper comprising a coating composition adhered to a substrate, said coating composition being erasable by local breakage of adhesion of said coating composition to said substrate, said coating composition comprising a synthetic polymeric elastomeric binder and a wax, said synthetic polymeric elastomeric binder being selected from the group consisting of an aqueous emulsion of an acrylic polymer and polymethylmethacrylate and wherein said wax is selected from the group consisting of polyalkane and polyalkene waxes and is present in an amount of at least 15 wt % of the elastomeric binder, said coating composition being adapted to receive an image at the top free surface thereof and resist penetration through the coating, of substances which define said images.
Claim 2
Dependent Claim 118 words
Electrophotographic paper comprising a coating composition adhered to a substrate, said coating composition being erasable by local breakage of adhesion of said coating composition to said substrate, said coating composition comprising a synthetic polymeric elastomeric binder and a wax, said synthetic polymeric elastomeric binder being selected from the group consisting of an aqueous emulsion of an acrylic polymer and polymethylmethacrylate and wherein said wax is selected from the group consisting of polyalkane and polyalkene waxes and is present in an amount of at least 15 wt % of the elastomeric binder, said coating composition being adapted to receive an image at the top free surface thereof and resist penetration through the coating, of substances which define said images.
Claim 3
Dependent Claim 14 words
The paper as claimed in claim 1, wherein the wax is a polyolefin wax.
Claim 4
Dependent Claim 15 words
The paper as claimed in claim 1, wherein the wax is an aqueous polyolefin emulsion.
Claim 5
Dependent Claim 32 words
The paper as claimed in claim 1, wherein the wax is a polyolefin emulsion which is present in the composition in an amount of at least 10 wt % of the composition.
Claim 6
Dependent Claim 21 words
The paper as claimed in claim 4, wherein the amount of polyolefin emulsion is about 15 wt % of the composition.
Claim 7
Dependent Claim 28 words
The paper as claimed in claim 4, wherein the particulate constituent is present in an amount of from about 46 to about 50 wt % of the composition.
Claim 8
Dependent Claim 42 words
The paper as claimed in claim 1, wherein the coating composition contains a particulate constituent selected from the group consisting of calcium carbonate powder and particulate silica, with a particle size in a range from about 4.5 μm to about 5 μm.
Claim 9
Dependent Claim 20 words
The paper as claimed in claim 7, wherein the particulate constituent is present in an amount of 10-50 wt %.
Claim 10
Dependent Claim 19 words
The paper as claimed in claim 1, wherein the binder is present in an amount of 25-90 wt %.
Claim 11
Dependent Claim 126 words
Electrophotographic paper, which comprises: a paper support, and a coating adhered to said paper support, said coating being erasable by local breakage of adhesion of said coating to said paper support, said coating comprising about 25-90 wt % of a synthetic polymeric elastomeric binder and a wax, said synthetic polymeric elastomeric binder being selected from the group consisting of an aqueous emulsion of an acrylic polymer and polymethylmethacrylate, and wherein said wax is selected from the group consisting of polyalkane and polyalkene waxes which is present to an extent of at least 15 wt % of the elastomeric binder, said coating composition being adapted to receive an image at the top free surface thereof and resist penetration through the coating, of substances which define said images.
Claim 12
Dependent Claim 126 words
Electrophotographic paper, which comprises: a paper support, and a coating adhered to said paper support, said coating being erasable by local breakage of adhesion of said coating to said paper support, said coating comprising about 25-90 wt % of a synthetic polymeric elastomeric binder and a wax, said synthetic polymeric elastomeric binder being selected from the group consisting of an aqueous emulsion of an acrylic polymer and polymethylmethacrylate, and wherein said wax is selected from the group consisting of polyalkane and polyalkene waxes which is present to an extent of at least 15 wt % of the elastomeric binder, said coating composition being adapted to receive an image at the top free surface thereof and resist penetration through the coating, of substances which define said images.
Claim 13
Dependent Claim 17 words
The paper as claimed in claim 10, further comprising about 10-50 wt % of a particulate constituent.
Claim 14
Dependent Claim 92 words
In xerography paper comprising a support and a coating containing a synthetic polymeric elastomeric binder thereon, said coating being adapted to receive an image at the top free surface thereof and resist penetration through the coating of substances which define said image, the improvement comprising incorporating into said coating a polyalkane or polyalkene wax in an amount at least 15 wt % of said elastomeric binder material, said coating incorporating said wax being adhered to said support, said coating being erasable by local breakage of adhesion of said coating to said support.
Claim 15
Dependent Claim 92 words
In xerography paper comprising a support and a coating containing a synthetic polymeric elastomeric binder thereon, said coating being adapted to receive an image at the top free surface thereof and resist penetration through the coating of substances which define said image, the improvement comprising incorporating into said coating a polyalkane or polyalkene wax in an amount at least 15 wt % of said elastomeric binder material, said coating incorporating said wax being adhered to said support, said coating being erasable by local breakage of adhesion of said coating to said support.

References Cited (Backward Citations)

JPS4911850A Cited
US4092449A Cited
SU598921A1 Cited
US4267092A Cited
JPS5854096A Cited
US4551499A Cited
US4517228A Cited
US4636258A Cited
US4792515A Cited
US4849316A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-09-08 1996-03-09 1996-09-08 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-09-08 2000-03-09 2000-09-08 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-09-08 2004-03-09 2004-09-08 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag