Fabricating a single level merged EEPROM cell having an ONO memory stack substantially spaced from the source region

Assignee: Texas Instruments Inc
•
Filing: 1989-08-29
•
Granted: 1992-06-09
•
Expires: 2009-08-29
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An electrically, programmable read-only memory cell is formed at a face (10) of a semiconductor layer (12). This cell comprises a doped drain region (36) and a doped source region (38) that are spaced from each other by a gate region (40). An ONO memory stack (28) is formed to extend over a portion of the gate region (40) that adjoins the drain region (36). The memory stack (28) is substantially spaced from the source region (38). A select gate insulator layer (30) is formed over the remainder of the gate region (40), and is preferably of the same thickness as the memory stack (28). A suitable gate conductor (32) is then deposited over insulator layers (26, 30). By being substantially spaced from source region (38), the memory stack (28) of the invention avoids the formation of ONO hole traps.

Inventors

  • 👤 Allan T. Mitchell
  • 👤 Bert R. Riemenschneider

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 05:50
CPC Classifications
H; H10; H10D; H10D30/00; H10D30/01; H10D30/021; H10D30/0411; H10D64/00; H10D64/01; H10D64/031; H10D64/035; H10B; H10B69/00

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 183 words
A method for manufacturing an electrically programmable read-only memory cell formed at a face of a semiconductor layer, comprising the steps: forming a first gate insulator layer over said semiconductor substrate; forming a dielectric floating gate electrode layer over said first gate insulator layer; forming a second gate insulator layer over said floating gate electrode layer; patterning and etching the first gate insulator layer, the floating gate electrode, and the second gate insulator layer to form a memory stack; forming a third insulator layer on said semiconductor layer adjoining said memory stack, said third insulator layer relatively thick with respect to said first and second insulator layer; forming gate conductor on the second and third insulator layers over a gate region in the semiconductor layer; forming a doped drain region in the semiconductor layer adjacent the gate region and the memory stack and self-aligned on at least one edge to said gate conductor; and forming a doped source region in the semiconductor layer adjacent the gate region, spaced from the memory stack, and self-aligned on at least one edge to said gate conductor.
Claim 2
Independent Claim 183 words
A method for manufacturing an electrically programmable read-only memory cell formed at a face of a semiconductor layer, comprising the steps: forming a first gate insulator layer over said semiconductor substrate; forming a dielectric floating gate electrode layer over said first gate insulator layer; forming a second gate insulator layer over said floating gate electrode layer; patterning and etching the first gate insulator layer, the floating gate electrode, and the second gate insulator layer to form a memory stack; forming a third insulator layer on said semiconductor layer adjoining said memory stack, said third insulator layer relatively thick with respect to said first and second insulator layer; forming gate conductor on the second and third insulator layers over a gate region in the semiconductor layer; forming a doped drain region in the semiconductor layer adjacent the gate region and the memory stack and self-aligned on at least one edge to said gate conductor; and forming a doped source region in the semiconductor layer adjacent the gate region, spaced from the memory stack, and self-aligned on at least one edge to said gate conductor.
Claim 3
Dependent Claim 34 words
The method of claim 1, and further including the step of: simultaneously etching the first gate insulator layer, the floating gate electrode layer and the third gate insulator layer in a single etch step.
Claim 4
Dependent Claim 38 words
The method of claim 1, and further including the step of forming the third insulator layer to be approximately as thick as the combined thicknesses of the first and second gate insulator layers and the gate electrode layer.
Claim 5
Dependent Claim 21 words
The method of claim 1, and further including the step of forming the first insulator layer by a thermal oxide step.
Claim 6
Dependent Claim 24 words
The method of claim 1, and further including the step of forming the second insulator layer by means of a thermal steam seal step.
Claim 7
Dependent Claim 20 words
The method of claim 1, and further including the step of forming the dielectric gate electrode layer from silicon nitride.
Claim 8
Dependent Claim 23 words
The method of claim 6, and further including the step of depositing the dielectric gate electrode layer by low pressure chemical vapor deposition.

References Cited (Backward Citations)

US3719866A Cited
US3877055A Cited
US4654828A Cited
US4611308A Cited
US4385308A Cited
US4795719A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-06-09 1995-12-09 1996-06-09 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-06-09 1999-12-09 2000-06-09 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-06-09 2003-12-09 2004-06-09 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag