Abstract
Abstract There is disclosed methods for producing self-supporting ceramic matrix and ceramic matrix composite bodies by batch, semi-continuous, and continuous processes utilzing the directed oxidation of a molten parent metal with an oxidant to form an oxidation reaction product which may embed filler material.
Inventors
- 👤 Harold D. Lesher
- 👤 Ratnesh K. Dwivedi
- 👤 Perry B. Goldberg
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-01 22:13
CPC Classifications
C; C04; C04B; C04B35/00; C04B35/71; C04B35/74; C04B41/00; C04B41/009; C04B35/622; C04B35/64; C04B35/65; C04B35/652; C04B41/45; C04B41/50; C04B41/5025; C04B41/5053; C04B41/80; C04B41/81; C04B41/85; C04B41/87
Claims Analysis
Total Claims: 28
Claim 1
Independent Claim
357 words
A method for producing at least one self-supporting ceramic matrix composite body which comprises: (a) providing a molten pool of parent metal within a container: (b) contacting at least one mass of filler material or at least one preform with the surface of said molten pool of parent metal so that said at least one mass of filler material or said at least one preform does not receive any substantial support from said container thereby causing said at least one mass of filler material or said at least one preform to float on the surface of said molten pool of parent metal; (c) reacting molten parent metal from said molten pool of parent metal with an oxidant to form an oxidant reaction product which grows into and embeds at least a portion of said at least one mass of filler material or said at least one preform; (d) maintaining said parent metal at a temperature higher than the melting temperature of said parent metal, but lower than the melting temperature of said oxidation reaction product, to form said oxidation reaction product, which product is in contact with, and extends between, said body of molten parent metal and said oxidant; (e) continuing said reaction at said temperature so that said molten parent metal is progressively drawn through said oxidation reaction product towards said oxidant and into said at least one mass of filler material or said at least one preform so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker body of said oxidation reaction product, and thereby embedding with oxidation reaction product at least a portion of said at least one mass of filler material or said at least one preform, which is floating on the surface of said molten pool of parent metal, thereby forming said at least one ceramic matrix composite body; and (f) removing said at least one ceramic matrix composite body from the surface of said molten pool of parent metal before said at least one ceramic matrix composite body receives any substantial support from said container.
Claim 2
Independent Claim
357 words
A method for producing at least one self-supporting ceramic matrix composite body which comprises: (a) providing a molten pool of parent metal within a container: (b) contacting at least one mass of filler material or at least one preform with the surface of said molten pool of parent metal so that said at least one mass of filler material or said at least one preform does not receive any substantial support from said container thereby causing said at least one mass of filler material or said at least one preform to float on the surface of said molten pool of parent metal; (c) reacting molten parent metal from said molten pool of parent metal with an oxidant to form an oxidant reaction product which grows into and embeds at least a portion of said at least one mass of filler material or said at least one preform; (d) maintaining said parent metal at a temperature higher than the melting temperature of said parent metal, but lower than the melting temperature of said oxidation reaction product, to form said oxidation reaction product, which product is in contact with, and extends between, said body of molten parent metal and said oxidant; (e) continuing said reaction at said temperature so that said molten parent metal is progressively drawn through said oxidation reaction product towards said oxidant and into said at least one mass of filler material or said at least one preform so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker body of said oxidation reaction product, and thereby embedding with oxidation reaction product at least a portion of said at least one mass of filler material or said at least one preform, which is floating on the surface of said molten pool of parent metal, thereby forming said at least one ceramic matrix composite body; and (f) removing said at least one ceramic matrix composite body from the surface of said molten pool of parent metal before said at least one ceramic matrix composite body receives any substantial support from said container.
Claim 3
Independent Claim
356 words
A method for producing at least one self-supporting ceramic matrix composite body which comprises: (a) providing a molten pool of parent metal within a container; (b) contacting at least one mass of filler material or at least one preform with the surface of said molten pool of parent metal so that said at least one mass of filler material or said at least one preform does not receive any substantial support from said container thereby causing said at least one mass of filler material or said at least one preform to float on the surface of said molten pool of parent metal; (c) reacting molten parent metal from said molten pool of parent metal with an oxidant to form an oxidation reaction product which grows into and embeds at least a portion of said at least one mass of filler material or said at least one preform; (d) maintaining said parent metal at a temperature higher than the melting temperature of said parent metal, but lower than the melting temperature of said oxidation reaction product, to form said oxidation reaction product, which product is in contact with, and extends between, said body of molten parent metal and said oxidant; (e) continuing said reaction at said temperature so that said molten parent metal is progressively drawn through said oxidation reaction product towards said oxidant and into said at least one mass of filler material or said at least one preform so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product thereby forming a progressively thicker body of said oxidation reaction product, and thereby embedding with oxidation reaction product at least a portion of said at least one mass of filler material or said at least one preform, which is floating on the surface of said molten pool of parent metal, thereby forming said at least one ceramic matrix composite body; and (f) removing said at least one ceramic matrix composite body from said molten pool of parent metal after said ceramic matrix composite body has sunk below the surface of said molten pool of parent metal.
Claim 4
Independent Claim
356 words
A method for producing at least one self-supporting ceramic matrix composite body which comprises: (a) providing a molten pool of parent metal within a container; (b) contacting at least one mass of filler material or at least one preform with the surface of said molten pool of parent metal so that said at least one mass of filler material or said at least one preform does not receive any substantial support from said container thereby causing said at least one mass of filler material or said at least one preform to float on the surface of said molten pool of parent metal; (c) reacting molten parent metal from said molten pool of parent metal with an oxidant to form an oxidation reaction product which grows into and embeds at least a portion of said at least one mass of filler material or said at least one preform; (d) maintaining said parent metal at a temperature higher than the melting temperature of said parent metal, but lower than the melting temperature of said oxidation reaction product, to form said oxidation reaction product, which product is in contact with, and extends between, said body of molten parent metal and said oxidant; (e) continuing said reaction at said temperature so that said molten parent metal is progressively drawn through said oxidation reaction product towards said oxidant and into said at least one mass of filler material or said at least one preform so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product thereby forming a progressively thicker body of said oxidation reaction product, and thereby embedding with oxidation reaction product at least a portion of said at least one mass of filler material or said at least one preform, which is floating on the surface of said molten pool of parent metal, thereby forming said at least one ceramic matrix composite body; and (f) removing said at least one ceramic matrix composite body from said molten pool of parent metal after said ceramic matrix composite body has sunk below the surface of said molten pool of parent metal.
Claim 5
Independent Claim
328 words
A method for producing self-supporting ceramic matrix composite bodies which comprises: (a) providing a molten pool of parent metal within a container; (b) contacting at least one mass of filler material or at least one preform with the surface of said molten pool of parent metal at a first point; (c) moving said at least one mass of filler material or said at least one preform across the surface of said molten pool of parent metal from said first point towards a second point; (d) reacting molten parent metal from said molten pool of parent metal with an oxidant to form an oxidation reaction product which grows into and embeds at least a portion of said at least one mass of filler material or at least one preform as said at least one mass of filler material or said at least one preform moves towards said second point; (e) maintaining said parent metal at a temperature higher than the melting temperature of said parent metal, but lower than the melting temperature of said oxidation reaction product, to form said oxidation reaction product, which product is in contact with, and extends between, said body of molten parent metal and said oxidant; (f) continuing said reaction at said temperature so that said molten parent metal is progressively drawn through said oxidation reaction product towards said oxidant and into said at least one mass of filler material or said at least one preform so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product thereby forming a progressively thicker body of said oxidation reaction product, and thereby embedding with oxidation reaction product at least a portion of said at least one mass of filler material or said at least one preform, thereby forming said at least one ceramic matrix composite body; (g) removing said at least one ceramic matrix composite body from the surface of said molten pool of parent metal.
Claim 6
Independent Claim
328 words
A method for producing self-supporting ceramic matrix composite bodies which comprises: (a) providing a molten pool of parent metal within a container; (b) contacting at least one mass of filler material or at least one preform with the surface of said molten pool of parent metal at a first point; (c) moving said at least one mass of filler material or said at least one preform across the surface of said molten pool of parent metal from said first point towards a second point; (d) reacting molten parent metal from said molten pool of parent metal with an oxidant to form an oxidation reaction product which grows into and embeds at least a portion of said at least one mass of filler material or at least one preform as said at least one mass of filler material or said at least one preform moves towards said second point; (e) maintaining said parent metal at a temperature higher than the melting temperature of said parent metal, but lower than the melting temperature of said oxidation reaction product, to form said oxidation reaction product, which product is in contact with, and extends between, said body of molten parent metal and said oxidant; (f) continuing said reaction at said temperature so that said molten parent metal is progressively drawn through said oxidation reaction product towards said oxidant and into said at least one mass of filler material or said at least one preform so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product thereby forming a progressively thicker body of said oxidation reaction product, and thereby embedding with oxidation reaction product at least a portion of said at least one mass of filler material or said at least one preform, thereby forming said at least one ceramic matrix composite body; (g) removing said at least one ceramic matrix composite body from the surface of said molten pool of parent metal.
Claim 7
Dependent Claim
29 words
The method of claim 1, wherein said at least one mass of filler material or said at least one preform is at least partially coated with a barrier material.
Claim 8
Dependent Claim
26 words
The method of claim 1, wherein said at least one mass of filler material or said at least one preform is attached to a flotation collar.
Claim 9
Dependent Claim
58 words
The method of claim 3, wherein an external or overhead support means is attached to or in contact with said at least one mass of filler material or said at least one preform while said at least one mass of filler material or said at least one preform is in contact with said molten pool of parent metal.
Claim 10
Independent Claim
287 words
A method of forming at least one ceramic matrix composite body which comprises: (a) forming at least one structure which comprises at least one internal cavity, and at least one wall which is permeable to a vapor-phase oxidant, wherein at least a portion of said cavity is defined by at least a portion of said at least one permeable wall; (b) providing a vapor-phase oxidant within at least a portion of said cavity; (c) immersing said at least one structure within a molten body of parent metal; (d) allowing said vapor-phase oxidant to contact said molten parent metal through said at least one permeable wall; (e) reacting said molten parent metal with said vapor-phase oxidant to form an oxidation reaction product which grows into and embeds at least a portion of said at least one permeable wall; (f) maintaining said molten body of parent metal at a temperature which is above the melting temperature of said parent metal but below the melting temperature of said oxidation reaction product and continuing said reaction so that said molten parent metal is progressively drawn through said oxidation reaction product towards said vapor-phase oxidant and into said at least one permeable wall so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker body of said oxidation reaction product and thereby embedding at least a portion of said at least one permeable wall within said oxidation reaction product to form said ceramic matrix composite body; (g) withdrawing said at least one structure from said molten body of parent metal; and (h) recovering said at least one ceramic matrix composite body from said at least one structure.
Claim 11
Independent Claim
287 words
A method of forming at least one ceramic matrix composite body which comprises: (a) forming at least one structure which comprises at least one internal cavity, and at least one wall which is permeable to a vapor-phase oxidant, wherein at least a portion of said cavity is defined by at least a portion of said at least one permeable wall; (b) providing a vapor-phase oxidant within at least a portion of said cavity; (c) immersing said at least one structure within a molten body of parent metal; (d) allowing said vapor-phase oxidant to contact said molten parent metal through said at least one permeable wall; (e) reacting said molten parent metal with said vapor-phase oxidant to form an oxidation reaction product which grows into and embeds at least a portion of said at least one permeable wall; (f) maintaining said molten body of parent metal at a temperature which is above the melting temperature of said parent metal but below the melting temperature of said oxidation reaction product and continuing said reaction so that said molten parent metal is progressively drawn through said oxidation reaction product towards said vapor-phase oxidant and into said at least one permeable wall so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker body of said oxidation reaction product and thereby embedding at least a portion of said at least one permeable wall within said oxidation reaction product to form said ceramic matrix composite body; (g) withdrawing said at least one structure from said molten body of parent metal; and (h) recovering said at least one ceramic matrix composite body from said at least one structure.
Claim 12
Independent Claim
260 words
A method of forming at least one ceramic matrix composite body which comprises: (a) placing at least one mass of filler material or at least one preform comprising an oxidant within a support means; (b) immersing said at least one mass of filler material or said at least one preform in a molten body of parent metal; (c) reacting said molten parent metal with said oxidant to form an oxidation reaction product which grows into and embeds at least a portion of said at least one mass of filler material or said at least one preform; (d) maintaining said molten body of parent metal at a temperature which is above the melting temperature of said parent metal but below the melting temperature of said oxidation reaction product and continuing said reaction so that said molten parent metal is progressively drawn through said oxidation reaction product towards said oxidant and into said at least one mass of filler material or said at least one preform so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker body of said oxidation reaction product and thereby embedding at lest a portion of said at least one mass of filler material or said at least one preform within said oxidation reaction product to form said at least one ceramic matrix composition body; (e) withdrawing said support means from said molten body of parent metal; and (f) removing said at least one ceramic matrix composite body from said support means.
Claim 13
Independent Claim
260 words
A method of forming at least one ceramic matrix composite body which comprises: (a) placing at least one mass of filler material or at least one preform comprising an oxidant within a support means; (b) immersing said at least one mass of filler material or said at least one preform in a molten body of parent metal; (c) reacting said molten parent metal with said oxidant to form an oxidation reaction product which grows into and embeds at least a portion of said at least one mass of filler material or said at least one preform; (d) maintaining said molten body of parent metal at a temperature which is above the melting temperature of said parent metal but below the melting temperature of said oxidation reaction product and continuing said reaction so that said molten parent metal is progressively drawn through said oxidation reaction product towards said oxidant and into said at least one mass of filler material or said at least one preform so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker body of said oxidation reaction product and thereby embedding at lest a portion of said at least one mass of filler material or said at least one preform within said oxidation reaction product to form said at least one ceramic matrix composition body; (e) withdrawing said support means from said molten body of parent metal; and (f) removing said at least one ceramic matrix composite body from said support means.
Claim 14
Dependent Claim
19 words
The method of claim 7, wherein said cavity is continuously provided with a vapor-phase oxidant through an internal means.
Claim 15
Dependent Claim
19 words
The method of claim 7, wherein said cavity is continuously provided with a vapor-phase oxidant through an external means.
Claim 16
Dependent Claim
24 words
The method of claim 10, wherein said external means comprises a means for directing the flow of the vapor-phase oxidant towards said permeable wall.
Claim 17
Dependent Claim
14 words
The method of claim 11, wherein said means comprises a piece of reticulated ceramic.
Claim 18
Dependent Claim
26 words
The method of claim 1, wherein at least a portion of said surface of said molten pool of parent metal is covered with a barrier metal.
Claim 19
Independent Claim
383 words
A method for producing at least one self-supporting ceramic matrix composite body which comprises: (a) providing a molten pool of parent metal within a container: (b) contacting at least one mass of filler material or at least one preform with the surface of said molten pool of parent metal so that said at least one mass of filler material or said at least one preform does not receive any substantial support from said container thereby causing said at least one mass of filler material or said at least one preform to float on the surface of said molten pool of parent metal; (c) reacting molten parent metal from said molten pool of parent metal with an oxidant to form an oxidant reaction product which grows into and embeds at least a portion of said at least one mass of filler material or said at least one preform; (d) maintaining said parent metal at a temperature higher than the melting temperature of said parent metal, but lower than the melting temperature of said oxidation reaction product, to form said oxidation reaction product, which product is in contact with, and extends between, said body of molten parent metal and said oxidant; (e) continuing said reaction at said temperature so that said molten parent metal is progressively drawn through said oxidation reaction product towards said oxidant and into said at least one mass of filler material or said at least one preform so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker body of said oxidation reaction product, and thereby embedding with oxidation reaction product at least a portion of said at least one mass of filler material or said at least one preform, which is floating on the surface of said molten pool of parent metal, thereby forming said at least one ceramic matrix composite body; and (f) removing said at least one ceramic matrix composite body from said molten pool of parent metal after said ceramic matrix composite body has partially sunk below the surface of said molten pool of parent metal and contacted at least one support means which prevents said ceramic matrix composite body from sinking below the surface of said molten pool of parent metal.
Claim 20
Independent Claim
383 words
A method for producing at least one self-supporting ceramic matrix composite body which comprises: (a) providing a molten pool of parent metal within a container: (b) contacting at least one mass of filler material or at least one preform with the surface of said molten pool of parent metal so that said at least one mass of filler material or said at least one preform does not receive any substantial support from said container thereby causing said at least one mass of filler material or said at least one preform to float on the surface of said molten pool of parent metal; (c) reacting molten parent metal from said molten pool of parent metal with an oxidant to form an oxidant reaction product which grows into and embeds at least a portion of said at least one mass of filler material or said at least one preform; (d) maintaining said parent metal at a temperature higher than the melting temperature of said parent metal, but lower than the melting temperature of said oxidation reaction product, to form said oxidation reaction product, which product is in contact with, and extends between, said body of molten parent metal and said oxidant; (e) continuing said reaction at said temperature so that said molten parent metal is progressively drawn through said oxidation reaction product towards said oxidant and into said at least one mass of filler material or said at least one preform so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker body of said oxidation reaction product, and thereby embedding with oxidation reaction product at least a portion of said at least one mass of filler material or said at least one preform, which is floating on the surface of said molten pool of parent metal, thereby forming said at least one ceramic matrix composite body; and (f) removing said at least one ceramic matrix composite body from said molten pool of parent metal after said ceramic matrix composite body has partially sunk below the surface of said molten pool of parent metal and contacted at least one support means which prevents said ceramic matrix composite body from sinking below the surface of said molten pool of parent metal.
Claim 21
Dependent Claim
29 words
The method of claim 2, wherein said at least one mass of filler material or said at least one preform is at least partially coated with a barrier material.
Claim 22
Dependent Claim
29 words
The method of claim 3, wherein said at least one mass of filler material or said at least one preform is at least partially coated with a barrier material.
Claim 23
Dependent Claim
26 words
The method of claim 3, wherein said at least one mass of filler material or said at least one preform is attached to a floatation collar.
Claim 24
Dependent Claim
26 words
The method of claim 2, wherein at least a portion of said surface of said molten pool of parent metal is covered with a barrier material.
Claim 25
Dependent Claim
27 words
The method of claim 3, wherein said at least a portion of said surface of said molten pool of parent metal is covered with a barrier material.
Claim 26
Dependent Claim
91 words
The method of claim 1, wherein said molten pool of parent metal is continuously contacted with at least one new mass of filler material or at least one new preform as said at least one ceramic matrix composite body is removed from the surface of said molten pool parent metal, said at least one new mass of filler material or said at least one new preform replacing the at least one mass of filler material or the at least one preform which produced said at least one ceramic matrix composite body.
Claim 27
Independent Claim
306 words
A method of continuously forming ceramic matrix composite bodies which comprises: (a) forming more than one structure which comprises at least one internal cavity, and at least one wall which is permeable to a vapor-phase oxidant, wherein at least a portion of said cavity is defined by at least a portion of said at lest one permeable wall; (b) providing a vapor-phase oxidant in at least a portion of said at least one internal cavity of each of said structures; (c) immersing said structure within a molten body of parent metal (d) allowing said vapor-phase oxidant to contact said molten parent metal through said at least one permeable wall; (e) reacting said molten parent metal with said vapor-phase oxidant to form an oxidation reaction product which grows into and embeds at least a portion of said at least one permeable wall; (f) maintaining said molten body of parent metal at a temperature which is above the melting temperature of said parent metal but below the melting temperature of said oxidation reaction product and continuing said reaction so that said molten parent metal is progressively drawn through said oxidation reaction product towards said vapor-phase oxidant and into said at least one permeable wall so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker body of said oxidation reaction product and thereby embedding at least a portion of said at least one permeable wall within said oxidation reaction portion to form at least one ceramic matrix composite body; (g) withdrawing said structures from said molten body of parent metal; (h) recovering said at least one ceramic matrix composite body from each of said structures; and (i) continuously repeating steps (b) through (h) with said structures to continuously produce ceramic matrix composite bodies.
Claim 28
Independent Claim
306 words
A method of continuously forming ceramic matrix composite bodies which comprises: (a) forming more than one structure which comprises at least one internal cavity, and at least one wall which is permeable to a vapor-phase oxidant, wherein at least a portion of said cavity is defined by at least a portion of said at lest one permeable wall; (b) providing a vapor-phase oxidant in at least a portion of said at least one internal cavity of each of said structures; (c) immersing said structure within a molten body of parent metal (d) allowing said vapor-phase oxidant to contact said molten parent metal through said at least one permeable wall; (e) reacting said molten parent metal with said vapor-phase oxidant to form an oxidation reaction product which grows into and embeds at least a portion of said at least one permeable wall; (f) maintaining said molten body of parent metal at a temperature which is above the melting temperature of said parent metal but below the melting temperature of said oxidation reaction product and continuing said reaction so that said molten parent metal is progressively drawn through said oxidation reaction product towards said vapor-phase oxidant and into said at least one permeable wall so that fresh oxidation reaction product continues to form at the interface between said oxidant and previously formed oxidation reaction product, thereby forming a progressively thicker body of said oxidation reaction product and thereby embedding at least a portion of said at least one permeable wall within said oxidation reaction portion to form at least one ceramic matrix composite body; (g) withdrawing said structures from said molten body of parent metal; (h) recovering said at least one ceramic matrix composite body from each of said structures; and (i) continuously repeating steps (b) through (h) with said structures to continuously produce ceramic matrix composite bodies.
References Cited (Backward Citations)
US3824113A
Cited
US4713360A
Cited
US4853352A
Cited
US4916113A
Cited
US4851375A
Cited
US4828785A
Cited
US4923832A
Cited
US4859640A
Cited
US4900699A
Cited
US4918034A
Cited
US4818734A
Cited
US4830799A
Cited
US4957779A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1995-06-09 | 1995-12-09 | 1996-06-09 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1999-06-09 | 1999-12-09 | 2000-06-09 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2003-06-09 | 2003-12-09 | 2004-06-09 | $7700.00 | Window Closed / Lapsed |