US5102691A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of pretreatment for the high-deposition-rate production of fluorine-doped tin-oxide coatings having reduced bulk resistivities and emissivities

Assignee: Arkema Inc
•
Filing: 1989-09-20
•
Granted: 1992-04-07
•
Expires: 2009-09-20
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for producing coatings on a heated substrate, preferably glass, comprises pretreating the substrate with a gaseous composition of water, air and a fluorine compound, and thereafter depositing a fluorine-doped tin-oxide coating on the substrate.

Inventors

  • 👤 David A. Russo
  • 👤 Ryan Dirkx
  • 👤 Jerome L. Buchanan

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 03:43
CPC Classifications
C; C03; C03C; C03C17/00; C03C17/22; C03C17/23; C23; C23C; C23C16/00; C23C16/02; C23C16/0209; C23C16/0218; C03C2217/00; C03C2217/20; C03C2217/21; C03C2217/211; C03C2217/24; C03C2217/241; C03C2218/00; C03C2218/10; C03C2218/15; C03C2218/152

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 55 words
The method of increasing the deposition rate of a fluorine-doped tin-oxide coating with reduced emissivity on a heated flat-glass substrate which comprises pretreating the substrate with a gaseous treating composition comprising at least 0.1 mol % water, a compound selected from the group consisting of fluorinated carboxylic acids and fluorinated carboxylic anhydrides, and a gas.
Claim 2
Independent Claim 55 words
The method of increasing the deposition rate of a fluorine-doped tin-oxide coating with reduced emissivity on a heated flat-glass substrate which comprises pretreating the substrate with a gaseous treating composition comprising at least 0.1 mol % water, a compound selected from the group consisting of fluorinated carboxylic acids and fluorinated carboxylic anhydrides, and a gas.
Claim 3
Dependent Claim 43 words
The method according to claim 1, wherein the gaseous treating composition comprises from about 0.1 to about 30 mol % water, from about 0.025 to about 5 mol % of the fluorine compound, and from about 65 to about 99.9 mol % air.
Claim 4
Dependent Claim 30 words
The method according to claim 1 wherein the gas is selected from the group consisting of air, oxygen, nitrogen, hydrogen, N 2 O, CO 2 , argon, and mixtures thereof.
Claim 5
Dependent Claim 41 words
The method according to claim 1 wherein the gaseous treating composition comprises from about 15 to about 25 mol % water, from about 0.1 to about 0.3 mol % trifluoroacetic acid, and from about 75 to about 85 mol % gas.
Claim 6
Dependent Claim 39 words
The method according to claim 1 wherein the composition comprises from about 0.6 to about 0.7 mol % water, from about 0.1 to about 0.2 mol % fluorine compound, and from about 99.1 to about 99.3 mol % gas.

References Cited (Backward Citations)

US3065103A Cited
US4293326A Cited
US4261722A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-04-07 1995-10-07 1996-04-07 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-04-07 1999-10-07 2000-04-07 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-04-07 2003-10-07 2004-04-07 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag