Patent US5091053A successfully refreshed from Google Patents.
← Back to Patent Explorer
US5091053A Expired / Lapsed US ⏱️ 0.0 years remaining

Matte finishes on optical fibers and other glass articles

Assignee: Nokia Bell Labs
•
Filing: 1990-02-28
•
Granted: 1992-02-25
•
Expires: 2010-02-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A mixture of buffered hydrofluoric acid (e.g., HF and NH 4 F) and a treating agent (e.g., acetic acid, phosphoric acid, hydrochloric acid, sulfuric acid or formic acid) is used to produce a matte finish on the pure silica cladding of an optical fiber, on a borosilicate glass tube and on a sodium lime glass plate. The matte finish may be used to increase the adhesion of other materials to the glass (e.g., of metal coatings to silica fibers) or to reduce glare.

Inventors

  • 👤 Greg E. Blonder
  • 👤 Bertrand H. Johnson

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-03 23:00
CPC Classifications
G; G02; G02B; G02B6/00; G02B6/24; G02B6/245; C; C03; C03C; C03C15/00; C03C25/00; C03C25/10; C03C25/104; C03C25/106; C03C25/1061; C03C25/1063; C03C25/66; C03C25/68; G02B6/42; G02B6/4201; G02B6/4248

Claims Analysis

Total Claims: 5
Claim 1
Independent Claim 68 words
A method of forming a textured or matte finish on at least a portion of a silica cladding of an optical fiber by subjecting said cladding portion to a mixture comprising a fluorine-based etchant and a treating agent, said agent comprising an acid which, by itself, does not significantly etch said portion and which is selected from the group consisting of acetic acid, hydrochloric acid and sulfuric acid.
Claim 2
Independent Claim 68 words
A method of forming a textured or matte finish on at least a portion of a silica cladding of an optical fiber by subjecting said cladding portion to a mixture comprising a fluorine-based etchant and a treating agent, said agent comprising an acid which, by itself, does not significantly etch said portion and which is selected from the group consisting of acetic acid, hydrochloric acid and sulfuric acid.
Claim 3
Dependent Claim 22 words
The method of claim 1 wherein said mixture comprises by volume about 25% of 3:1 BOE and 75% of said treating agent.
Claim 4
Dependent Claim 20 words
The method of claim 1 further including depositing a metal layer on said portion having a textured or matte finish.
Claim 5
Dependent Claim 13 words
The method of claim 3 wherein said metal layer is deposited by electroplating.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-02-24 1995-08-26 1996-02-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-02-24 1999-08-26 2000-02-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-02-24 2003-08-26 2004-02-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag