Abstract

Abstract A semiconductor device such as a Schottky-barrier rectifier diode is disclosed which has a barrier electrode formed on a semiconductor substrate of gallium arsenide or the like. Formed around the barrier electrode is an annular resistive layer, typically of titanium oxide, creating a Schottky barrier at its interface with the semiconductor substrate. The resistive layer has a sheet resistance of more than 10 kilohms per square. In order to prevent preliminary breakdowns from taking place at the peripheral part of the resistive layer before final breakdown of the device, the sheet resistance of the resistive layer is made higher as it extends away from the barrier electrode. For the ease of manufacture, the resistive layer can be divided into two or more annular regions of distinctly different sheet resistances.

Inventors

  • 👤 Koji Ohtsuka
  • 👤 Hirokazu Goto

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 02:33
CPC Classifications
H; H10; H10D; H10D8/00; H10D8/60; H10D30/00; H10D30/60; H10D30/67; H10D30/6729; H10D30/6737; H10D30/6738; H10D30/674; H10D30/675; H10D62/00; H10D62/80; H10D62/85; H10D64/00; H10D64/60; H10D64/62; H10D64/64; H10D8/01; H10D8/043; H10D8/051; Y; Y10; Y10S; Y10S148/00; Y10S148/139; Y10S148/14; Y10S438/00; Y10S438/934

Claims Analysis

Total Claims: 30
Claim 1
Independent Claim 149 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a first conductivity type; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky-barrier therebetween, the Schottky-barrier electrode comprising a first layer of unoxidized titanium formed in direct contact with the semiconductor region and a second layer of a metal other than titanium formed on the first layer; and (c) an annular resistive layer of titanium oxide formed around the Schottky-barrier electrode on the semiconductor region and forming a Schottky-barrier at its interface with the semiconductor region, the resistive layer being joined directly to the first layer of the Schottky-barrier electrode and having a sheet resistance which is higher than that of the first layer and which increases as the resistive layer extends away from the first layer, the minimum sheet resistance of the resistance layer being approximately 10 kilohms per square.
Claim 2
Dependent Claim 149 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a first conductivity type; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky-barrier therebetween, the Schottky-barrier electrode comprising a first layer of unoxidized titanium formed in direct contact with the semiconductor region and a second layer of a metal other than titanium formed on the first layer; and (c) an annular resistive layer of titanium oxide formed around the Schottky-barrier electrode on the semiconductor region and forming a Schottky-barrier at its interface with the semiconductor region, the resistive layer being joined directly to the first layer of the Schottky-barrier electrode and having a sheet resistance which is higher than that of the first layer and which increases as the resistive layer extends away from the first layer, the minimum sheet resistance of the resistance layer being approximately 10 kilohms per square.
Claim 3
Dependent Claim 40 words
The Schottky-barrier semiconductor device of claim 1 wherein the second layer of the Schottky-barrier electrode is less in size than the first layer and is so disposed thereon as to leave exposed an annular peripheral part to the first layer.
Claim 4
Dependent Claim 18 words
The Schottky-barrier semiconductor device of claim 1 wherein the second layer of the Schottky-barrier electrode is of aluminum.
Claim 5
Dependent Claim 126 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a first conductivity type; (b) a Schottky-barrier electrode comprising a metallic material formed on the semiconductor region for creating a Schottky-barrier therebetween; (c) an annular resistive layer comprising a metal-oxide material formed around the Schottky-barrier electrode on the semiconductor region and forming a Schottky-barrier at its interface with the semiconductor region, the resistive layer being electrically connected to the Schottky-barrier electrode and having a sheet resistance which is higher than that of the Schottky-barrier electrode and which increases as the resistive layer extends away from the Schottky-barrier electrode, the minimum sheet resistance of the resistive layer being approximately 10 kilohms per square; and (d) an insulating layer formed on the resistive layer.
Claim 6
Dependent Claim 126 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a first conductivity type; (b) a Schottky-barrier electrode comprising a metallic material formed on the semiconductor region for creating a Schottky-barrier therebetween; (c) an annular resistive layer comprising a metal-oxide material formed around the Schottky-barrier electrode on the semiconductor region and forming a Schottky-barrier at its interface with the semiconductor region, the resistive layer being electrically connected to the Schottky-barrier electrode and having a sheet resistance which is higher than that of the Schottky-barrier electrode and which increases as the resistive layer extends away from the Schottky-barrier electrode, the minimum sheet resistance of the resistive layer being approximately 10 kilohms per square; and (d) an insulating layer formed on the resistive layer.
Claim 7
Dependent Claim 15 words
The Schottky-barrier semiconductor device of claim 4 wherein the insulating layer is of silicon oxide.
Claim 8
Dependent Claim 24 words
The Schottky-barrier semiconductor device of claim 4 further comprising a field plate formed on the insulating layer and electrically connected to the Schottky-barrier electrode.
Claim 9
Dependent Claim 183 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a first conductivity type; (b) a Schottky-barrier electrode comprising a metallic material formed on the semiconductor region for creating a Schottky barrier therebetween; (c) a first annular resistive region comprising a metal-oxide material formed on the semiconductor region so as to surround the Schottky-barrier electrode and electrically connected to the Schottky-barrier electrode, the first resistive region having a sheet resistance of not less than 10 kilohms per square and creating a Schottky barrier at its interface with the semiconductor region; (d) a second annular resistive region comprising a metal-oxide material formed on the semiconductor region so as to surround the first resistive region and electrically connected to the first resistive region, the second resistive region having a higher sheet resistance than that of the first resistive region and creating a Schottky barrier at its interface with the semiconductor region; and (e) an annular equipotential metal region disposed between the first and second resistive regions, the equipotential region being less in sheet resistance than the first and second resistive regions.
Claim 10
Dependent Claim 183 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a first conductivity type; (b) a Schottky-barrier electrode comprising a metallic material formed on the semiconductor region for creating a Schottky barrier therebetween; (c) a first annular resistive region comprising a metal-oxide material formed on the semiconductor region so as to surround the Schottky-barrier electrode and electrically connected to the Schottky-barrier electrode, the first resistive region having a sheet resistance of not less than 10 kilohms per square and creating a Schottky barrier at its interface with the semiconductor region; (d) a second annular resistive region comprising a metal-oxide material formed on the semiconductor region so as to surround the first resistive region and electrically connected to the first resistive region, the second resistive region having a higher sheet resistance than that of the first resistive region and creating a Schottky barrier at its interface with the semiconductor region; and (e) an annular equipotential metal region disposed between the first and second resistive regions, the equipotential region being less in sheet resistance than the first and second resistive regions.
Claim 11
Dependent Claim 160 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor region; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky barrier therebetween, the Schottky-barrier electrode comprising a first layer of titanium formed on the semiconductor region, a second layer of titanium formed on the first layer, and a third layer of a metal other than titanium formed on the second layer; (c) a first annular titanium oxide region formed on the semiconductor region so as to surround the first layer of the Schottky-barrier electrode and electrically connected to the first layer, the first titanium oxide region creating a Schottky barrier at its interface with the semiconductor region; and (d) a second annular titanium oxide region formed on part of the first titanium oxide region so as to surround the second layer of the Schottky-barrier electrode and electrically connected to the second layer, the second titanium oxide region being less in sheet resistance than the first titanium oxide region.
Claim 12
Dependent Claim 160 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor region; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky barrier therebetween, the Schottky-barrier electrode comprising a first layer of titanium formed on the semiconductor region, a second layer of titanium formed on the first layer, and a third layer of a metal other than titanium formed on the second layer; (c) a first annular titanium oxide region formed on the semiconductor region so as to surround the first layer of the Schottky-barrier electrode and electrically connected to the first layer, the first titanium oxide region creating a Schottky barrier at its interface with the semiconductor region; and (d) a second annular titanium oxide region formed on part of the first titanium oxide region so as to surround the second layer of the Schottky-barrier electrode and electrically connected to the second layer, the second titanium oxide region being less in sheet resistance than the first titanium oxide region.
Claim 13
Dependent Claim 18 words
The Schottky-barrier semiconductor device of claim 8 wherein the third layer of the Schottky-barrier electrode is of anluminum.
Claim 14
Dependent Claim 190 words
A p-n junction semiconductor device comprising: (a) a first semiconductor region of a first conductivity type; (b) a second semiconductor region having a second conductivity type opposite to the first conductivity type and being less in resistivity than the first semiconductor region, the first and second semiconductor regions being disposed contiguous to each other to create a p-n junction therebetween; (c) an ohmic electrode formed on the second semiconductor region; (d) an annular resistive layer formed on the first semiconductor region so as to surround the ohmic electrode and creating a Schottky barrier at its interface with the first semiconductor region, the resistive layer being electrically connected to the ohmic electrode and having a sheet resistance which is higher than that of the ohmic electrode and which increases as the resistive layer extends away from the ohmic electrode, the minimum sheet resistance of the resistive layer being approximately 10 kilohms per square; and (e) an annular resistance region formed on the second semiconductor region and interposed between the annular resistive layer and the ohmic electrode, the resistive region being electrically connected to both the resistive layer and the ohmic electrode.
Claim 15
Dependent Claim 190 words
A p-n junction semiconductor device comprising: (a) a first semiconductor region of a first conductivity type; (b) a second semiconductor region having a second conductivity type opposite to the first conductivity type and being less in resistivity than the first semiconductor region, the first and second semiconductor regions being disposed contiguous to each other to create a p-n junction therebetween; (c) an ohmic electrode formed on the second semiconductor region; (d) an annular resistive layer formed on the first semiconductor region so as to surround the ohmic electrode and creating a Schottky barrier at its interface with the first semiconductor region, the resistive layer being electrically connected to the ohmic electrode and having a sheet resistance which is higher than that of the ohmic electrode and which increases as the resistive layer extends away from the ohmic electrode, the minimum sheet resistance of the resistive layer being approximately 10 kilohms per square; and (e) an annular resistance region formed on the second semiconductor region and interposed between the annular resistive layer and the ohmic electrode, the resistive region being electrically connected to both the resistive layer and the ohmic electrode.
Claim 16
Dependent Claim 24 words
The p-n junction semiconductor device of claim 10 wherein the resistive layer is of titanium oxide, and the resistive region is of unoxidized titanium.
Claim 17
Dependent Claim 165 words
A schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a conductivity type; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky-barrier therebetween; (c) a first resistive region formed on the semiconductor region so as to surround the Schottky-barrier electrode and electrically connected to the Schottky-barrier electrode, the first resistive region having a sheet resistance of not less than 10 kilohms per square and creating a Schottky-barrier at its interface with the semiconductor region; (d) a second resistive region formed on the semiconductor region so as to surround the first resistive region and electrically connected to the first resistive region, the second resitive region having a higher sheet resistance than that of the first resistive region and creating a Schottky-barrier at its interface with the semiconductor region; and (e) an annular equipotential metal region disposed between the first and second resistive regions, the equipotential region being less in sheet resistance than the first and second resistive regions.
Claim 18
Dependent Claim 165 words
A schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a conductivity type; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky-barrier therebetween; (c) a first resistive region formed on the semiconductor region so as to surround the Schottky-barrier electrode and electrically connected to the Schottky-barrier electrode, the first resistive region having a sheet resistance of not less than 10 kilohms per square and creating a Schottky-barrier at its interface with the semiconductor region; (d) a second resistive region formed on the semiconductor region so as to surround the first resistive region and electrically connected to the first resistive region, the second resitive region having a higher sheet resistance than that of the first resistive region and creating a Schottky-barrier at its interface with the semiconductor region; and (e) an annular equipotential metal region disposed between the first and second resistive regions, the equipotential region being less in sheet resistance than the first and second resistive regions.
Claim 19
Dependent Claim 180 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a conductivity type; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky-barrier therebetween, the Schottky-barrier electrode comprising a first layer of unoxidized titanium formed in direct contact with the semiconductor region and a second layer of a metal other than titanium formed on the unoxidized titanium layer; (c) a first resistive region of titanium oxide formed on the semiconductor region so as to surround the Schottky-barrier electrode and directly joined to the first layer of the Schottky-barrier electrode, the first resistive region having a sheet resistance of not less than 10 kilohms per square and creating a Schottky-barrier at its interface with the semiconductor region; and (d) a second resistive region of titanium oxide formed on the semiconductor region so as to surround the first resistive region and electrically connected to the first resistive region, the second resistive region having a higher sheet resistance than that of the first resistive region and creating a Schottky-barrier at its interface with the semiconductor region.
Claim 20
Dependent Claim 180 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a conductivity type; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky-barrier therebetween, the Schottky-barrier electrode comprising a first layer of unoxidized titanium formed in direct contact with the semiconductor region and a second layer of a metal other than titanium formed on the unoxidized titanium layer; (c) a first resistive region of titanium oxide formed on the semiconductor region so as to surround the Schottky-barrier electrode and directly joined to the first layer of the Schottky-barrier electrode, the first resistive region having a sheet resistance of not less than 10 kilohms per square and creating a Schottky-barrier at its interface with the semiconductor region; and (d) a second resistive region of titanium oxide formed on the semiconductor region so as to surround the first resistive region and electrically connected to the first resistive region, the second resistive region having a higher sheet resistance than that of the first resistive region and creating a Schottky-barrier at its interface with the semiconductor region.
Claim 21
Dependent Claim 40 words
The Schottky-barrier semiconductor device of claim 13 wherein the second layer of the Schottky-barrier electrode is less in size than the first layer and is so disposed thereon as to leave exposed an annular peripheral part of the first layer.
Claim 22
Dependent Claim 18 words
The Schottky-barrier semiconductor device of claim 13 wherein the second layer of the Schottky-barrier electrode is of aluminum.
Claim 23
Dependent Claim 148 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a conductivity type; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky-barrier therebetween; (c) a first resistive region formed on the semiconductor region so as to surround the Schottky-barrier electrode and electrically connected to the Schottky-barrier electrode, the first resistive region having a sheet resistance of not less than 10 kilohms per square and creating a Schottky-barrier at its interface with the semiconductor region; (d) a second resistive region formed on the semiconductor region so as to surround the first resistive region and electrically connected to the first resistive region, the second resistive region having a higher sheet resistance than that of the first resistive region and creating a Schottky-barrier at its interface with the semiconductor region; and (e) an insulating layer formed on the first and second resistive regions.
Claim 24
Dependent Claim 148 words
A Schottky-barrier semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a conductivity type; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky-barrier therebetween; (c) a first resistive region formed on the semiconductor region so as to surround the Schottky-barrier electrode and electrically connected to the Schottky-barrier electrode, the first resistive region having a sheet resistance of not less than 10 kilohms per square and creating a Schottky-barrier at its interface with the semiconductor region; (d) a second resistive region formed on the semiconductor region so as to surround the first resistive region and electrically connected to the first resistive region, the second resistive region having a higher sheet resistance than that of the first resistive region and creating a Schottky-barrier at its interface with the semiconductor region; and (e) an insulating layer formed on the first and second resistive regions.
Claim 25
Dependent Claim 15 words
The Schottky-barrier semiconductor device of claim 16 wherein the insulating layer is of silicon oxide.
Claim 26
Dependent Claim 24 words
The Schottky-barrier semiconductor device of claim 16 further comprising a field plate formed on the insulating layer and electrically connected to the Schottky-barrier electrode.
Claim 27
Dependent Claim 215 words
A p-n junction semiconductor device comprising: (a) a semiconductor substrate, the semiconductor substrate having a first semiconductor region of a first conductivity type, and a second semiconductor region having a second conductivity type opposite to the first conductivity type and being less in resistivity than the first semiconductor region, the first and second semiconductor regions being disposed contiguous to each other to create a p-n junction therebetween; (b) an ohmic electrode formed on the second semiconductor region; (c) a first resistive region formed on the first semiconductor region so as to surround the ohmic electrode and electrically connected to the ohmic electrode, the first resistive region having a sheet resistance of not less than 10 kilohms per square and creating a Schottky-barrier at its interface with the first semiconductor region; (d) a second resistive region formed on the first semiconductor region so as to surround the first resistive region and electrically connected to the first resistive region, the second resistive region having a higher sheet resistance than that of the first resistive region and creating a Schottky-barrier at its interface with the first semiconductor region; and (e) an annular equipotential metal region disposed between the first and second resistive regions, the equipotential region being less in sheet resistance than the first and second resistive layers.
Claim 28
Dependent Claim 215 words
A p-n junction semiconductor device comprising: (a) a semiconductor substrate, the semiconductor substrate having a first semiconductor region of a first conductivity type, and a second semiconductor region having a second conductivity type opposite to the first conductivity type and being less in resistivity than the first semiconductor region, the first and second semiconductor regions being disposed contiguous to each other to create a p-n junction therebetween; (b) an ohmic electrode formed on the second semiconductor region; (c) a first resistive region formed on the first semiconductor region so as to surround the ohmic electrode and electrically connected to the ohmic electrode, the first resistive region having a sheet resistance of not less than 10 kilohms per square and creating a Schottky-barrier at its interface with the first semiconductor region; (d) a second resistive region formed on the first semiconductor region so as to surround the first resistive region and electrically connected to the first resistive region, the second resistive region having a higher sheet resistance than that of the first resistive region and creating a Schottky-barrier at its interface with the first semiconductor region; and (e) an annular equipotential metal region disposed between the first and second resistive regions, the equipotential region being less in sheet resistance than the first and second resistive layers.
Claim 29
Dependent Claim 171 words
A p-n junction semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a conductivity type; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky-barrier therebetween, the Schottky-barrrier electrode comprising a first layer of titanium formed on the semiconductor region, and a second layer of titanium formed on the first layer, and a third layer of a metal other than titanium formed on the second layer; (c) a first titanium oxide region formed on the semiconductor region so as to surround the first layer of the Schottky-barrier electrode and electrically connected to the first layer, the first titanium oxide region creating a Schottky-barrier at its interface with the semiconductor region; and (d) a second titanium oxide region formed on part of the first titanium oxide layer so as to surround the second layer of the Schottky-barrier electrode and electrically connected to the second layer, the sheet resistance of the second titanium oxide region being less than the sheet resistance than the first titanium oxide region.
Claim 30
Dependent Claim 171 words
A p-n junction semiconductor device comprising: (a) a semiconductor substrate having a semiconductor region of a conductivity type; (b) a Schottky-barrier electrode formed on the semiconductor region for creating a Schottky-barrier therebetween, the Schottky-barrrier electrode comprising a first layer of titanium formed on the semiconductor region, and a second layer of titanium formed on the first layer, and a third layer of a metal other than titanium formed on the second layer; (c) a first titanium oxide region formed on the semiconductor region so as to surround the first layer of the Schottky-barrier electrode and electrically connected to the first layer, the first titanium oxide region creating a Schottky-barrier at its interface with the semiconductor region; and (d) a second titanium oxide region formed on part of the first titanium oxide layer so as to surround the second layer of the Schottky-barrier electrode and electrically connected to the second layer, the sheet resistance of the second titanium oxide region being less than the sheet resistance than the first titanium oxide region.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1995-01-13 1995-07-15 1996-01-14 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1999-01-13 1999-07-15 2000-01-14 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2003-01-13 2003-07-15 2004-01-14 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag