Patent US5045499A successfully refreshed from Google Patents.
US5045499A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method of manufacturing a distributed brass reflector type semiconductor laser
Assignee: Japan Science and Technology Agency
•
Filing: 1989-09-26
•
Granted: 1991-09-03
•
Expires: 2009-09-26
Abstract
Abstract Disclosed are a distributed Bragg reflector type semiconductor laser and a method of manufacturing such a laser a high yields, in which the upper surface of an active waveguide is covered by an external waveguide, the external waveguide at side portions thereof, the external waveguide is coupled with the edge surfaces of the active waveguide without any gap remaining, and the coupling ratio of the active waveguide and external waveguide is high.
Inventors
- 👤 Hideaki Nishizawa
- 👤 Mitsuo Takahashi
- 👤 Yasuharu Suematsu
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-27 17:19
CPC Classifications
H; H01; H01S; H01S5/00; H01S5/10; H01S5/12; H01S5/125; Y; Y10; Y10S; Y10S148/00; Y10S148/095; Y10S148/119
Claims Analysis
Total Claims: 7
Claim 1
Independent Claim
333 words
A method of manufacturing a distributed Bragg reflector type semiconductor laser comprising the steps of: forming a buffer layer (2) on a p- or n-type semiconductor monocrystalline substrate (1) by an epitaxial growth method, said buffer layer (2) having the same electrical polarity as said substrate (1); forming by epitaxial growth a non-doped active waveguide layer (3) on said buffer layer (2), or on said substrate (1) in the case where no buffer layer is interposed; forming by epitaxial growth a depression layer (4) having an electrical polarity opposite to that of said substrate (1) on said non-doped active waveguide layer (3); forming a stripe-shaped film (5) in a central portion of an upper surface of said depression layer (4); etching both the depression layer (4) and the active waveguide layer (3) while retaining the central portion covered by said film (5); forming a distributed Bragg reflector (6) serving as a diffraction grating on upper surfaces of the remaining depression layer (4) and the buffer layer (2) which is exposed on both sides of said active waveguide layer (3) or on the upper surface of the substrate (1) by use of an interference exposing method; etching edge surfaces of the active waveguide layer (3) in the horizontal direction by using the depression layer (4) as a mask, thereby allowing edge surfaces (W) of the active waveguide layer (3) to be set back by a distance of 0.2 μm to 1.0 μm behind edge surfaces (U) of the depression layer (4); forming by epitaxial growth on the buffer layer (2) or the substrate (1) with said distributed Bragg reflector (6) formed thereon and on the depression layer (4) an external waveguide layer (7) having an electrical polarity opposite to that of the substrate (1); forming by epitaxial growth on said external waveguide layer (7) a clad layer (8) having an electrical polarity opposite to that of the substrate (1); and forming electrodes (9) and (10) on the substrate (1) and said clad layer (8).
Claim 2
Independent Claim
333 words
A method of manufacturing a distributed Bragg reflector type semiconductor laser comprising the steps of: forming a buffer layer (2) on a p- or n-type semiconductor monocrystalline substrate (1) by an epitaxial growth method, said buffer layer (2) having the same electrical polarity as said substrate (1); forming by epitaxial growth a non-doped active waveguide layer (3) on said buffer layer (2), or on said substrate (1) in the case where no buffer layer is interposed; forming by epitaxial growth a depression layer (4) having an electrical polarity opposite to that of said substrate (1) on said non-doped active waveguide layer (3); forming a stripe-shaped film (5) in a central portion of an upper surface of said depression layer (4); etching both the depression layer (4) and the active waveguide layer (3) while retaining the central portion covered by said film (5); forming a distributed Bragg reflector (6) serving as a diffraction grating on upper surfaces of the remaining depression layer (4) and the buffer layer (2) which is exposed on both sides of said active waveguide layer (3) or on the upper surface of the substrate (1) by use of an interference exposing method; etching edge surfaces of the active waveguide layer (3) in the horizontal direction by using the depression layer (4) as a mask, thereby allowing edge surfaces (W) of the active waveguide layer (3) to be set back by a distance of 0.2 μm to 1.0 μm behind edge surfaces (U) of the depression layer (4); forming by epitaxial growth on the buffer layer (2) or the substrate (1) with said distributed Bragg reflector (6) formed thereon and on the depression layer (4) an external waveguide layer (7) having an electrical polarity opposite to that of the substrate (1); forming by epitaxial growth on said external waveguide layer (7) a clad layer (8) having an electrical polarity opposite to that of the substrate (1); and forming electrodes (9) and (10) on the substrate (1) and said clad layer (8).
Claim 3
Dependent Claim
18 words
A method according to claim 1, wherein said epitaxial growth method is a liquid phase epitaxial growth method.
Claim 4
Dependent Claim
18 words
A method according to claim 1, wherein said epitaxial growth method is a vapor phase epitaxial growth method.
Claim 5
Dependent Claim
66 words
A method according to claim 2 or 3, wherein said substrate (1) is a p-type InP monocrystal, said buffer layer (2) is a p-type InP monocrystal, said active waveguide layer (3) is a non-doped InGaAsP mixed crystal, said depression layer (4) is an n-type InP monocrystal, said external waveguide layer (7) is an n-type InGaAsP mixed crystal, and said clad layer is an n-type InP monocrystal.
Claim 6
Dependent Claim
37 words
A method according to claim 4, wherein said depression layer (4) is selectively etched by an HCl-based etching liquid and said active waveguide layer (3) is selectively etched by an H 2 SO 4 -based etching liquid.
Claim 7
Dependent Claim
37 words
A method according to claim 5, wherein when the edge surfaces (W) of said active waveguide layer (3) are etched in a lateral direction, the etching speed falls within a range from 0.02 μm/minute to 0.2 μm/minute.
References Cited (Backward Citations)
JPS56111284A
Cited
JPS5743428A
Cited
JPS59227177A
Cited
US4575919A
Cited
US4662988A
Cited
JPS61166087A
Cited
JPS61171190A
Cited
US4815087A
Cited
US4830986A
Cited
US4835117A
Cited
JPS63114190A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1994-09-02 | 1995-03-04 | 1995-09-03 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1998-09-02 | 1999-03-04 | 1999-09-03 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2002-09-02 | 2003-03-04 | 2003-09-03 | $7700.00 | Window Closed / Lapsed |