Claims Analysis
Total Claims: 24
Claim 1
Independent Claim
158 words
In a method of preparing pulp from a lignocellulosic material by subjecting said material to an alkaline pulping liquor at a select temperature, pressure and time period to attain a pulp having a select Kappa number range, the improvement comprising: (a) adding an amount up to about 10% by weight, based on a 100% weight basis of dry pulp being produced, of a digestive additive selected from the group consisting of alphasulfo alkyl esters, alkaryl sulfonates, alkanolamides, and mixtures thereof to said alkaline pulping liquor whereby a reduction of alkaline pulping liquor requirements, a reduction of H-factor, a reduction in material reject percentages, and a reduction in cooking time period is attained; (b) discharging said pulping liquors and the at least partially delignified lignocellulosic material to attain a pulp slurry; and (c) displacing said pulping liquor from said partially delignified lignocellulosic material with water or an aqueous liquor to attain a pulp having said select Kappa number range.
Claim 2
Dependent Claim
158 words
In a method of preparing pulp from a lignocellulosic material by subjecting said material to an alkaline pulping liquor at a select temperature, pressure and time period to attain a pulp having a select Kappa number range, the improvement comprising: (a) adding an amount up to about 10% by weight, based on a 100% weight basis of dry pulp being produced, of a digestive additive selected from the group consisting of alphasulfo alkyl esters, alkaryl sulfonates, alkanolamides, and mixtures thereof to said alkaline pulping liquor whereby a reduction of alkaline pulping liquor requirements, a reduction of H-factor, a reduction in material reject percentages, and a reduction in cooking time period is attained; (b) discharging said pulping liquors and the at least partially delignified lignocellulosic material to attain a pulp slurry; and (c) displacing said pulping liquor from said partially delignified lignocellulosic material with water or an aqueous liquor to attain a pulp having said select Kappa number range.
Claim 3
Dependent Claim
52 words
In a method as defined in claim 1 wherein said digestive additive is selected from the group consisting of alphasulfo alkyl esters, alkaryl sulfonates, and which are neutralized with a monovalent and/or divalent cation selected from the group consisting of an alkaline metal, alkaline earth metal, ammonium, substituted ammonium, and mixtures thereof.
Claim 4
Dependent Claim
44 words
In a method as defined claim 2 wherein the cation is selected from the group consisting of Na, K, Ca, Ba, Mg, NH 4 , (HOCH 2 CH 2 ) 3 NH, (HOCH 2 CH 2 ) 2 NH 2 , and mixtures thereof.
Claim 5
Dependent Claim
16 words
In a method as defined in 2 wherein said alphasulfo alkyl ester is an alkyl sulfosuccinate.
Claim 6
Dependent Claim
16 words
In a method as defined in 2 wherein said alphasulfo alkyl ester is an alkyl sulfosuccinate.
Claim 7
Dependent Claim
17 words
In a method as defined in claim 3 wherein said digestive additive is sodium alpha-sulfo methyl laurate.
Claim 8
Dependent Claim
16 words
In a method as defined in claim 3 wherein said digestive additive is sodium xylene sulfonate.
Claim 9
Dependent Claim
16 words
In a method as defined in claim 3 wherein said digestive additive is triethanolammonium lauryl sulfate.
Claim 10
Dependent Claim
16 words
In a method as defined in claim 3 wherein said digestive additive is disodium lauryl sulfosuccinate.
Claim 11
Dependent Claim
15 words
In a method as defined in claim 3 wherein said digestive additive is an alkanolamide.
Claim 12
Dependent Claim
13 words
In a method as defined in claim 9 wherein said alkanolamide is cocodiethanolamide.
Claim 13
Dependent Claim
22 words
In a method as defined in claim 3 wherein said digestive additive is a blend of sodium alpha-sulfo methyl laurate and cocodiethanolamide.
Claim 14
Dependent Claim
42 words
In a method as defined in claim 1 wherein the amount of said digestive additive added to said alkaline pulping liquor ranges from about 0.001% to about 5.0% by weight, based on a 100% total weight basis of dry pulp being produced.
Claim 15
Dependent Claim
181 words
In a method of preparing Kraft pulp from a lignocellulosic material by subjecting said materials to a Kraft pulping liquor at a selected temperature, pressure and time period to attain a pulp having a select Kappa number range, the improvement comprising: (a) adding an amount up to about 10% by weight, based on a 100% total weight basis of dry pulp being produced, of a digestive additive selected from the group consisting of alpha-sulfo alkyl esters, alkaryl sulfonates, alkyl sulfates, alkanolamides, and mixtures thereof to said Kraft pulping liquor whereby a reduction of pulping liquor requirements, a reduction of H-factor, a reduction in material reject percentages and a reduction in cooking time period is attained, relative to pulping liquor requirements, H-factor reject percentages and digestion time period experienced in similar Kraft pulping processes without said digestive additives; (b) discharging said pulping liquor and the at least partially lignocellulosic material to attain a pulp slurry; and (c) displacing said pulping liquor from said pulp slurry with water or an aqueous liquor to attain a Kraft pulp having a select Kappa number range.
Claim 16
Dependent Claim
181 words
In a method of preparing Kraft pulp from a lignocellulosic material by subjecting said materials to a Kraft pulping liquor at a selected temperature, pressure and time period to attain a pulp having a select Kappa number range, the improvement comprising: (a) adding an amount up to about 10% by weight, based on a 100% total weight basis of dry pulp being produced, of a digestive additive selected from the group consisting of alpha-sulfo alkyl esters, alkaryl sulfonates, alkyl sulfates, alkanolamides, and mixtures thereof to said Kraft pulping liquor whereby a reduction of pulping liquor requirements, a reduction of H-factor, a reduction in material reject percentages and a reduction in cooking time period is attained, relative to pulping liquor requirements, H-factor reject percentages and digestion time period experienced in similar Kraft pulping processes without said digestive additives; (b) discharging said pulping liquor and the at least partially lignocellulosic material to attain a pulp slurry; and (c) displacing said pulping liquor from said pulp slurry with water or an aqueous liquor to attain a Kraft pulp having a select Kappa number range.
Claim 17
Dependent Claim
44 words
In a method as defined in claim 13 wherein said alpha-sulfo alkyl esters, alkaryl sulfonates, and alkyl sulfonates are neutralized with a monovalent and/or divalent cation selected from the group consisting of an alkaline metal, alkaline earth metal, ammonium, substituted ammonium, and mixtures thereof.
Claim 18
Dependent Claim
16 words
In a method as defined in 13 wherein said alpha-sulfo alkyl ester is an alkyl sulfosuccinate.
Claim 19
Dependent Claim
16 words
In a method as defined in 13 wherein said alpha-sulfo alkyl ester is an alkyl sulfosuccinate.
Claim 20
Dependent Claim
44 words
In a method as defined claim 14 wherein the cation is selected from the group consisting of Na, K, Ca, Ba, Mg, NH 4 , (HOCH 2 CH 2 ) 3 NH, (HOCH 2 CH 2 ) 2 NH 2 , and mixtures thereof.
Claim 21
Dependent Claim
42 words
In a method as defined in claim 13 wherein the amount of said digestive additive added to said alkaline pulping liquor ranges from about 0.001% to about 5.0% by weight, based on a 100% total weight basis of dry pulp being produced.
Claim 22
Independent Claim
215 words
A method of producing a paperboard pulp having a Kappa number in the range of about 30 to about 110 from a lignocellulosic material comprising: (a) feeding an amount of said lignocellulosic material to a digester capable of yielding a given amount of paperboard pulp; (b) adding a sufficient amount of an alkaline pulping liquor to said digester to attain a select liquor-to lignocellulosic material ratio therein, said pulping liquor including therein an amount up to about 10%, based on a 100% total weight basis of dry paperboard pulp being produced, of a digestive additive selected from the consisting of sodium alpha-sulfo methyl laurate, sodium xylene sulfonate, triethanolammonium lauryl sulfate, disodium lauryl sulfosuccinate, cocodiethanolamide, and mixtures thereof, to attain an aqueous mixture of materials in said digester and subjecting said mixture to elevated temperatures and pressures over selected time periods so as to attain a reduction of pulping liquor requirements, a reduction of H-factor, a reduction of pulp material rejects and a reduction in digestion time, relative to pulping liquor requirements, H-factor, reject percentages and digestion time periods experienced in similar alkaline digestion processes without said digestive additive; and (c) displacing said aqueous mixture of materials from said digester in such a manner as to attain at least some paperboard pulp and spent pulping liquor.
Claim 23
Independent Claim
215 words
A method of producing a paperboard pulp having a Kappa number in the range of about 30 to about 110 from a lignocellulosic material comprising: (a) feeding an amount of said lignocellulosic material to a digester capable of yielding a given amount of paperboard pulp; (b) adding a sufficient amount of an alkaline pulping liquor to said digester to attain a select liquor-to lignocellulosic material ratio therein, said pulping liquor including therein an amount up to about 10%, based on a 100% total weight basis of dry paperboard pulp being produced, of a digestive additive selected from the consisting of sodium alpha-sulfo methyl laurate, sodium xylene sulfonate, triethanolammonium lauryl sulfate, disodium lauryl sulfosuccinate, cocodiethanolamide, and mixtures thereof, to attain an aqueous mixture of materials in said digester and subjecting said mixture to elevated temperatures and pressures over selected time periods so as to attain a reduction of pulping liquor requirements, a reduction of H-factor, a reduction of pulp material rejects and a reduction in digestion time, relative to pulping liquor requirements, H-factor, reject percentages and digestion time periods experienced in similar alkaline digestion processes without said digestive additive; and (c) displacing said aqueous mixture of materials from said digester in such a manner as to attain at least some paperboard pulp and spent pulping liquor.
Claim 24
Dependent Claim
42 words
In a method as defined in claim 18 wherein the amount of said digestive additive added to said alkaline pulping liquor ranges from about 0.001% to about 5.0% by weight, based on a 100% total weight basis of dry pulp being produced.