Method for producing thin film of oxide superconductor

Assignee: Sumitomo Electric Industries Ltd
•
Filing: 1988-03-30
•
Granted: 1991-05-21
•
Expires: 2008-03-30
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A thin film of an oxide superconductor having a homogeneous composition and less oxygen defects is produced by independently vaporizing onto a substrate at least one material selected from the group consisting of the elements of Ia, IIa and IIIa groups of the periodic table and their compounds and one material selected from the group consisting of Cu and its compounds and irradiating the substrate with oxygen ions and depositing the vaporized materials together with oxygen on the substrate to form the thin film of the oxide superconductor.

Inventors

  • 👤 Jun Shioya
  • 👤 Yoichi Yamaguchi
  • 👤 Akira Mizoguchi
  • 👤 Noriyuki Yoshida
  • 👤 Kenichi Takahashi
  • 👤 Kenji Miyazaki
  • 👤 Satoshi Takano
  • 👤 Noriki Hayashi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 18:59
CPC Classifications
C; C04; C04B; C04B41/00; C04B41/009; C04B35/00; C04B35/01; C04B35/45; C04B35/4504; C04B41/45; C04B41/50; C04B41/5072; C04B41/5074; C04B41/52; C04B41/80; C04B41/81; C04B41/85; C04B41/89; H; H10; H10N; H10N60/00; H10N60/01; H10N60/0268; H10N60/0296; H10N60/0324; H10N60/0381; H10N60/0548; H10N60/0801; Y; Y10; Y10S; Y10S505/00; Y10S505/70; Y10S505/704; Y10S505/725; Y10S505/73; Y10S505/732

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 93 words
A method for producing a thin film of an oxide superconductor comprising independently vaporizing at least one first material selected from the group consisting of Y, lanthanides and their compounds, at least one second material selected from the group consisting of Ca, Sr and Ba and their compounds, and one third material selected from the group consisting of Cu and its compounds, ionizing the vaporized materials and irradiating a substrate with oxygen ions to deposit the vaporized materials together with oxygen on the substrate to form the thin film of the oxide superconductor.
Claim 2
Independent Claim 93 words
A method for producing a thin film of an oxide superconductor comprising independently vaporizing at least one first material selected from the group consisting of Y, lanthanides and their compounds, at least one second material selected from the group consisting of Ca, Sr and Ba and their compounds, and one third material selected from the group consisting of Cu and its compounds, ionizing the vaporized materials and irradiating a substrate with oxygen ions to deposit the vaporized materials together with oxygen on the substrate to form the thin film of the oxide superconductor.
Claim 3
Dependent Claim 16 words
The method according to claim 1, wherein at least one of the materials is an oxide.
Claim 4
Dependent Claim 34 words
The method according to claim 2, wherein the first material is an oxide selected from the group consisting of La 2 O 3 , Y 2 O 3 and Sc 2 O 3 .
Claim 5
Dependent Claim 30 words
The method according to claim 1, wherein the second material is a carbonate selected from the group consisting of Ba 2 CO 3 , SrCO 3 and CaCO 3 .
Claim 6
Dependent Claim 12 words
The method according to claim 2, wherein the third material is CuO.
Claim 7
Dependent Claim 53 words
The method according to claim 1, wherein the oxide superconductor has a composition of the formula: M.sup.1.sub.x M.sup.2.sub.1-x M.sup.3 O.sub.3 (I) or M.sup.1.sub.y M.sup.2.sub.2-y M.sup.3 O.sub.4 (II) wherein M 1 and M 2 are elements independently selected from the group consisting of Y, lanthanides, Ca, Sr and Ba and M 3 is Cu.
Claim 8
Dependent Claim 17 words
The method according to claim 1, wherein the substrate is made of a flexible elongate ceramic body.
Claim 9
Dependent Claim 15 words
The method according to claim 7, wherein the flexible elongate ceramic body is a tape.
Claim 10
Dependent Claim 16 words
The method according to claim 7, wherein the flexible elongate ceramic body is a round wire.

References Cited (Backward Citations)

JPS5565358A Cited
FR2469005A1 Cited
US4430366A Cited
FR2602246A1 Cited
EP0282839A2 Cited
US4861750A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-05-20 1994-11-19 1995-05-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-05-20 1998-11-19 1999-05-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-05-20 2002-11-19 2003-05-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag