PIN junction photovoltaic element containing Zn, Se, Te, H in an amount of 1 to 4 atomic %

Assignee: Canon Inc
•
Filing: 1988-11-18
•
Granted: 1991-04-16
•
Expires: 2008-11-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An improved pin junction photovoltaic element which causes photoelectromotive force by the junction of a p-type semiconductor layer, an i-type semiconductor layer and an n-type semiconductor layer, characterized in that at least one of said p-type semiconductor layer and said n-type semiconductor layer comprises a p-typed or n-typed ZSnSe 1-x Te x :H:M film, where M is a dopant of p-type or n-type: the quantitative ratio of the Se to the Te is in the range of from 1:9 to 3:7 in terms of atomic ratio: the amount of the H is in the range of from 1 to 4 atomic %: and said film contains crystal grain domains in a proportion of 65 to 85 vol % per unit volume; and said i-type semiconductor layer comprises a non-single crystal Si(H,F) film or a non-single crystal Si(C,Ge)(H,F) film.

Inventors

  • 👤 Katsumi Nakagawa
  • 👤 Shunichi Ishihara
  • 👤 Masahiro Kanai
  • 👤 Tsutomu Murakami
  • 👤 Kozo Arao
  • 👤 Yasushi Fujioka
  • 👤 Akira Sakai

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 08:54
CPC Classifications
H; H10; H10F; H10F10/00; H10F10/10; H10F10/17; H10F10/172; H10F71/00; H10F71/125; H10F71/1253; H10F77/00; H10F77/10; H10F77/12; H10F77/123; H10F77/1233; H10F77/1237; H10F77/16; H10F77/169; H10F77/1696; Y; Y02; Y02E; Y02E10/00; Y02E10/50; Y02E10/548

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 156 words
An improved pin junction photovoltaic element which comprises a p-type semiconductor layer, an i-type semiconductor layer and an n-type semiconductor layer being stacked, characterized in that at least one of said p-type semiconductor layer and said n-type semiconductor layer comprises a p-type or n-type film comprised of zinc atoms, selenium atoms, tellurium atoms and hydrogen atoms; the quantitative ratio of said selenium atoms to said tellurium atoms is in the range of from 1:9 to 3:7 in terms of atomic ratio in said film: the amount of said hydrogen atoms in said film is in the range of from 1 to 4 atomic %; said film contains crystal grain domains in a proportion of 65 to 85 vol % per unit volume: and said film contains a dopant of p-type or n-type; and said i-type semiconductor layer comprises a non-single crystal film containing silicon atoms and at least one kind of hydrogen atoms and fluorine atoms.
Claim 2
Dependent Claim 156 words
An improved pin junction photovoltaic element which comprises a p-type semiconductor layer, an i-type semiconductor layer and an n-type semiconductor layer being stacked, characterized in that at least one of said p-type semiconductor layer and said n-type semiconductor layer comprises a p-type or n-type film comprised of zinc atoms, selenium atoms, tellurium atoms and hydrogen atoms; the quantitative ratio of said selenium atoms to said tellurium atoms is in the range of from 1:9 to 3:7 in terms of atomic ratio in said film: the amount of said hydrogen atoms in said film is in the range of from 1 to 4 atomic %; said film contains crystal grain domains in a proportion of 65 to 85 vol % per unit volume: and said film contains a dopant of p-type or n-type; and said i-type semiconductor layer comprises a non-single crystal film containing silicon atoms and at least one kind of hydrogen atoms and fluorine atoms.
Claim 3
Dependent Claim 46 words
The pin junction photovoltaic element according to claim 1, wherein said p-type dopant to be contained in said deposited film to constitute the p-type semiconductor layer is a member selected from the group consisting of Group IA elements and Group VA elements of the Periodic Table.
Claim 4
Dependent Claim 14 words
The pin junction photovoltaic element according to claim 2, wherein said member is lithium.
Claim 5
Dependent Claim 46 words
The pin junction photovoltaic element according to claim 1, wherein said n-type dopant to be contained in said deposited film to constitute the n-type semiconductor layer is a member selected from the group consisting of Group IIIA elements and Group IVA elements of the Periodic Table.
Claim 6
Dependent Claim 16 words
The pin junction photovoltaic element according to claim 4, wherein said element is aluminum or gallium.
Claim 7
Dependent Claim 32 words
The pin junction photovoltaic element according to claim 1, wherein said non-single crystal film to constitute the i-type semiconductor layer further contains at least one kind of carbon atoms and germanium atoms.
Claim 8
Dependent Claim 308 words
An improved pin junction photovoltaic element which comprises a p-type semiconductor layer, an i-type semiconductor layer and an n-type semiconductor layer being stacked, characterized in that said p-type semiconductor layer comprises a p-type film comprised of zinc atoms, selenium atoms, tellurium atoms and hydrogen atoms; the quantitative ratio of said selenium atoms to said tellurium atoms is in the range of from 1:9 to 3:7 in terms of atomic ratio in said film; the amount of said hydrogen atoms in said film is in the range of from 1 to 4 atomic %; said film contains crystal grain domains in a proportion of 65 to 85 vol % per unit volume: and said film contains a p-type dopant selected from the group consisting of Group IA elements and Group VA elements of the Periodic Table; said i-type semiconductor layer comprises a non-single crystal film selected from the group consisting of non-single crystal films containing silicon atoms as the matrix and at least one kind of hydrogen atoms and fluorine atoms and non-single crystal films containing silicon atoms, at least one kind of carbon atoms and germanium atoms and at least one kind of hydrogen atoms and germanium atoms; and said n-type semiconductor layer comprises an n-type film comprised of zinc atoms, selenium atoms, tellurium atoms and hydrogen atoms; the quantitative ratio of said selenium atoms to said tellurium atoms is in the range of from 1:9 to 3:7 in terms of atomic ratio in said film; the amount of said hydrogen atoms in said film is in the range of from 1 to 4 atomic %; said film contains crystal grain domains in a proportion of 65 to 85 vol % per unit volume and said film contains an n-type dopant selected from the group consisting of Group IIIA elements and Group IVA elements of the Periodic Table.
Claim 9
Dependent Claim 308 words
An improved pin junction photovoltaic element which comprises a p-type semiconductor layer, an i-type semiconductor layer and an n-type semiconductor layer being stacked, characterized in that said p-type semiconductor layer comprises a p-type film comprised of zinc atoms, selenium atoms, tellurium atoms and hydrogen atoms; the quantitative ratio of said selenium atoms to said tellurium atoms is in the range of from 1:9 to 3:7 in terms of atomic ratio in said film; the amount of said hydrogen atoms in said film is in the range of from 1 to 4 atomic %; said film contains crystal grain domains in a proportion of 65 to 85 vol % per unit volume: and said film contains a p-type dopant selected from the group consisting of Group IA elements and Group VA elements of the Periodic Table; said i-type semiconductor layer comprises a non-single crystal film selected from the group consisting of non-single crystal films containing silicon atoms as the matrix and at least one kind of hydrogen atoms and fluorine atoms and non-single crystal films containing silicon atoms, at least one kind of carbon atoms and germanium atoms and at least one kind of hydrogen atoms and germanium atoms; and said n-type semiconductor layer comprises an n-type film comprised of zinc atoms, selenium atoms, tellurium atoms and hydrogen atoms; the quantitative ratio of said selenium atoms to said tellurium atoms is in the range of from 1:9 to 3:7 in terms of atomic ratio in said film; the amount of said hydrogen atoms in said film is in the range of from 1 to 4 atomic %; said film contains crystal grain domains in a proportion of 65 to 85 vol % per unit volume and said film contains an n-type dopant selected from the group consisting of Group IIIA elements and Group IVA elements of the Periodic Table.
Claim 10
Dependent Claim 23 words
The pin junction photovoltaic element according to claim 7, wherein said p-type dopant is lithium and said n-type dopant is aluminum or gallium.

References Cited (Backward Citations)

JPS5224483A Cited
US4105472A Cited
US4105477A Cited
US4105478A Cited
US4217374A Cited
US4345107A Cited
US4465527A Cited
US4525687A Cited
JPS61120480A Cited
US4851302A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-04-15 1994-10-15 1995-04-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-04-15 1998-10-15 1999-04-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-04-15 2002-10-15 2003-04-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag