Abstract

Abstract A glass powder adhesive sheet used for a surface coating of inorganic structures comprising ceramics, metals, glasses, etc., a glazed ceramic substrate such as a substrate of electronic circuit, etc. or a heat-resistant label, etc., which comprises a glass powder molding comprising as main components, a glass powder and a resin binder, and an adhesive layer having a thermal decomposition initiation temperature higher than that of the resin binder, provided on the surface of the glass powder molding.

Inventors

  • 👤 Takashi Tominaga
  • 👤 Souji Nishiyama
  • 👤 Takahumi Sakuramoto
  • 👤 Makoto Honda

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-30 04:54
CPC Classifications
H; H05; H05K; H05K1/00; H05K1/02; H05K1/03; C; C04; C04B; C04B41/00; C04B41/009; C04B41/45; C04B41/4505; C04B41/4511; C04B41/4513; C04B41/80; C04B41/81; C09; C09J; C09J7/00; C09J7/20; C09J7/22; C03; C03C; C03C2218/00; C03C2218/30; C03C2218/355; H05K1/0306; H05K3/00; H05K3/22; H05K3/28; H05K3/281; Y; Y10; Y10T; Y10T428/00; Y10T428/28; Y10T428/31504; Y10T428/31551; Y10T428/31641; Y10T428/31645

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 72 words
A multilayer glass powder adhesive sheet comprising: a glass powder molding layer consisting essentially of glass powder and a resin binder; and an adhesive layer having a thermal decomposition initiation temperature higher than that of said resin binder, provided on the surface of the glass powder molding layer wherein the difference between the thermal decomposition initiation temperature of said adhesive layer and that of said resin binder is at least 10° C.
Claim 2
Dependent Claim 72 words
A multilayer glass powder adhesive sheet comprising: a glass powder molding layer consisting essentially of glass powder and a resin binder; and an adhesive layer having a thermal decomposition initiation temperature higher than that of said resin binder, provided on the surface of the glass powder molding layer wherein the difference between the thermal decomposition initiation temperature of said adhesive layer and that of said resin binder is at least 10° C.
Claim 3
Dependent Claim 23 words
A glass powder adhesive sheet as claimed in claim 1, wherein the glass powder has a softening point of 300° to 1400° C.
Claim 4
Dependent Claim 25 words
A glass powder adhesive sheet as claimed in claim 1, wherein the resin binder has a thermal decomposition initiation temperature of 100° to 350° C.
Claim 5
Dependent Claim 25 words
A glass powder adhesive sheet as claimed in claim 1, wherein the adhesive layer has a thermal decomposition initiation temperature of 100° to 350° C.
Claim 6
Dependent Claim 25 words
A glass powder adhesive sheet as claimed in claim 1, wherein the adhesive layer exhibits adhesive properties after activation by heat, water, solvent, or pressure.
Claim 7
Dependent Claim 28 words
A glass powder adhesive sheet as claimed in claim 1, wherein a release substrate having a self-supporting property is temporarily provided on the surface of the adhesive layer.
Claim 8
Dependent Claim 34 words
A glass powder adhesive sheet as claimed in claim 1, wherein the glass powder molding further comprises at least one powder selected from the group consisting of an inorganic powder and a metal powder.
Claim 9
Dependent Claim 23 words
A glass powder adhesive sheet as claimed in claim 7, wherein the glass powder has a softening point of 300° to 1400° C.
Claim 10
Dependent Claim 25 words
A glass powder adhesive sheet as claimed in claim 7, wherein the resin binder has a thermal decomposition initiation temperature of 100° to 350° C.
Claim 11
Dependent Claim 25 words
A glass powder adhesive sheet as claimed in claim 7, wherein the adhesive layer has a thermal decomposition initiation temperature of 100° to 350° C.
Claim 12
Dependent Claim 25 words
A glass powder adhesive sheet as claimed in claim 7, wherein the adhesive layer exhibits adhesive properties after activation by heat, water, solvent, or pressure.
Claim 13
Dependent Claim 28 words
A glass powder adhesive sheet as claimed in claim 7, wherein a release substrate having a self-supporting property is temporarily provided on the surface of the adhesive layer.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1994-04-15 1994-10-15 1995-04-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1998-04-15 1998-10-15 1999-04-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2002-04-15 2002-10-15 2003-04-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag