US4988541A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Process for making retroreflector sheet
Assignee: 3M Innovative Properties Co
•
Filing: 1990-01-02
•
Granted: 1991-01-29
•
Expires: 2010-01-02
Abstract
Abstract Process for making retroreflector sheet having protrusions which are retroreflective on selected side surfaces of the protrusions. Continuous web of polymeric base sheet having a front surface with a plurality, of protrusions, each protrusion having a top surface and at least one side surface, is provided. The web is conveyed through a nip in contact with a liquid film of bonding polymer at sufficient pressure to displace the film from the protrusion top surfaces and onto selected side surfaces, depending upon the relative speeds of the web and bonding polymer film. Retroreflective beads are applied to the liquid film which is then solidified (e.g., by temperature change) to hold the beads in place.
Inventors
- 👤 Thomas P. Hedblom
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-23 22:57
CPC Classifications
B; B29; B29D; B29D11/00; B29D11/00605; B29D11/00615; B05; B05C; B05C1/00; B05C1/04; B05C1/08; B05C1/12; B05D; B05D1/00; B05D1/28; E; E01; E01F; E01F9/00; E01F9/50; E01F9/506; E01F9/512; E01F9/576; E01F9/578; G; G02; G02B; G02B5/00; G02B5/12; G02B5/126; G02B5/128
Claims Analysis
Total Claims: 8
Claim 1
Independent Claim
165 words
A process for producing a retroreflective sheet comprising the steps of: (A) providing a resilient polymeric continuous web base sheet having a back surface and a plurality of protrusions projecting from a front surface of the sheet opposite said back surface, each of the protrusions having a top surface and at least one side surface; (B) applying a discontinuous layer of a liquid bead bond material to selected portions of the side surfaces of the protrusions by conveying the web over a roller where the protrusions are pressed against a film of bead bond material, the pressure over the area of web in contact with the bead bond film being sufficient to keep the bead bond material off the top surfaces of the protrusions and force the bead bond material onto selected portions of the side surfaces; (C) partially embedding a plurality of retroreflecting beads in the liquid layer of bead bond material; and (D) solidifying the bead bond layer to form a retroreflector sheet.
Claim 2
Dependent Claim
165 words
A process for producing a retroreflective sheet comprising the steps of: (A) providing a resilient polymeric continuous web base sheet having a back surface and a plurality of protrusions projecting from a front surface of the sheet opposite said back surface, each of the protrusions having a top surface and at least one side surface; (B) applying a discontinuous layer of a liquid bead bond material to selected portions of the side surfaces of the protrusions by conveying the web over a roller where the protrusions are pressed against a film of bead bond material, the pressure over the area of web in contact with the bead bond film being sufficient to keep the bead bond material off the top surfaces of the protrusions and force the bead bond material onto selected portions of the side surfaces; (C) partially embedding a plurality of retroreflecting beads in the liquid layer of bead bond material; and (D) solidifying the bead bond layer to form a retroreflector sheet.
Claim 3
Dependent Claim
33 words
The process of claim 1 wherein the pressure is provided by a backing roller pressing against the back surface of the base sheet, forcing the protrusions into contact with the bead bond film.
Claim 4
Dependent Claim
16 words
The process of claim 2 wherein the rollers have a hardness greater than 75 Shore A.
Claim 5
Dependent Claim
33 words
The process of claim 1 wherein the bead bond includes polyurethane and pigment and the solidifying step is carried out by exposing the embedded retroreflecting sheet to a temperature of about 177° C.
Claim 6
Dependent Claim
23 words
The process of claim 1 wherein the liquid bead bond material has a viscosity at 24° C. of about 1800 to 10,000 centipoise.
Claim 7
Dependent Claim
144 words
A process for producing a retroreflector sheet, the process comprising the steps of: providing a resilient polymeric base sheet having a back surface and a plurality of protrusions projecting from a front surface of the sheet opposite said back surface, each of the protrusions having a top surface and at least one side surface; applying a discontinuous layer of a liquid bead bond material to selected portions of the side surfaces of the protrusions by pressing a film of said bead bond against the protrusions with sufficient pressure to displace the liquid bead bond from the protrusion top surfaces and onto at least one side surface; partially embedding a plurality of retroreflecting beads in the liquid layer of bead bond material; and solidifying the bead bond layer to form a retroreflector sheet with partially embedded retroreflecting beads on selected portions of the front surface.
Claim 8
Dependent Claim
144 words
A process for producing a retroreflector sheet, the process comprising the steps of: providing a resilient polymeric base sheet having a back surface and a plurality of protrusions projecting from a front surface of the sheet opposite said back surface, each of the protrusions having a top surface and at least one side surface; applying a discontinuous layer of a liquid bead bond material to selected portions of the side surfaces of the protrusions by pressing a film of said bead bond against the protrusions with sufficient pressure to displace the liquid bead bond from the protrusion top surfaces and onto at least one side surface; partially embedding a plurality of retroreflecting beads in the liquid layer of bead bond material; and solidifying the bead bond layer to form a retroreflector sheet with partially embedded retroreflecting beads on selected portions of the front surface.
References Cited (Backward Citations)
US2108645A
Cited
US2143946A
Cited
US3436359A
Cited
US3418896A
Cited
US3580887A
Cited
US4020211A
Cited
US3935365A
Cited
US4040760A
Cited
US4069281A
Cited
US4117192A
Cited
US4248932A
Cited
US4381388A
Cited
US4530859A
Cited
US4681401A
Cited
US4388359A
Cited
EP0162229A1
Cited
US4573763A
Cited
US4758469A
Cited
EP0237315A2
Cited
US4701019A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1994-01-28 | 1994-07-30 | 1995-01-29 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1998-01-28 | 1998-07-30 | 1999-01-29 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2002-01-28 | 2002-07-30 | 2003-01-29 | $7700.00 | Window Closed / Lapsed |