Plasma doping process and apparatus therefor

Assignee: Panasonic Holdings Corp
•
Filing: 1988-08-04
•
Granted: 1990-06-26
•
Expires: 2008-08-04
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In a plasma doping process utilizing a radio frequency discharging in a vacuum by for doping an impurity into a semiconductor substrate, the radio frequency discharging is made intermittently and under controlling of average current of the discharging, thereby the impurity concentration is desirably controlled; and especially by selecting the vacuum in a range between 1×10 -4 -5×10 -2 torr, undesirable deposition of the impurity on the substrate surface is evadable.

Inventors

  • 👤 Ichiro Nakayama
  • 👤 Bunji Mizuno
  • 👤 Masabumi Kubota
  • 👤 Masuo Tanno

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 13:33
CPC Classifications
H; H10; H10P; H10P32/00; H10P32/10; H10P32/12; H10P32/1204

Claims Analysis

Total Claims: 20
Claim 1
Independent Claim 103 words
Method for plasma-doping of impurity on a semiconductor substrate comprising the steps of: placing an object semiconductor substrate on a first electrode in a vacuum chamber, introducing a gas of a controlled reduced pressure containing at least one impurity, into said vacuum chamber, impressing a radio frequency current of a high voltage in intermittence across said first electrode and a second electrode in said chamber thereby causing radio frequency discharging in said chamber, to generate plasma doping, and controlling a duty ratio of said intermittence in accordance with a program to control the amount of impurity doped on a surface of said substrate.
Claim 2
Dependent Claim 103 words
Method for plasma-doping of impurity on a semiconductor substrate comprising the steps of: placing an object semiconductor substrate on a first electrode in a vacuum chamber, introducing a gas of a controlled reduced pressure containing at least one impurity, into said vacuum chamber, impressing a radio frequency current of a high voltage in intermittence across said first electrode and a second electrode in said chamber thereby causing radio frequency discharging in said chamber, to generate plasma doping, and controlling a duty ratio of said intermittence in accordance with a program to control the amount of impurity doped on a surface of said substrate.
Claim 3
Dependent Claim 90 words
Method for plasma-doping of impurity on a semiconductor substrate comprising the step of: placing an object semiconductor substrate on a first electrode in a vacuum chamber, introducing a gas of a controlled reduced pressure containing at least one impurity into said vacuum chamber, and impressing a radio frequency current of a high voltage in intermittence across said first electrode and said second electrode in said chamber, the frequency of said intermittence being 0.1 Hz to 50 Hz, thereby causing radio frequency discharging in said chamber to generate a plasma doping.
Claim 4
Dependent Claim 90 words
Method for plasma-doping of impurity on a semiconductor substrate comprising the step of: placing an object semiconductor substrate on a first electrode in a vacuum chamber, introducing a gas of a controlled reduced pressure containing at least one impurity into said vacuum chamber, and impressing a radio frequency current of a high voltage in intermittence across said first electrode and said second electrode in said chamber, the frequency of said intermittence being 0.1 Hz to 50 Hz, thereby causing radio frequency discharging in said chamber to generate a plasma doping.
Claim 5
Dependent Claim 19 words
Method in accordance with claim 1, wherein said object substrate is on single-crystalline silicon, polycrystalline silicon or amorphous silicon.
Claim 6
Dependent Claim 15 words
Method in accordance with claim 1, wherein said impurity is boron, phosphorus or arsenide. PG,26
Claim 7
Dependent Claim 111 words
Method for plasma-doping of impurity on a semiconductor substrate comprising the steps of: placing an object semiconductor substrate on a first electrode in a vacuum chamber, introducing a gas of a controlled reduced pressure containing at least one impurity, into said vacuum chamber, impressing a radio frequency current of a high voltage across said first electrode and a second electrode in said chamber through means for measuring said radio frequency current, thereby causing radio frequency discharging in said chamber to generate a plasma, and controlling said radio frequency current based on a measurement thereof in accordance with a program, to control amount of impurity doped on the surface of said substrate.
Claim 8
Dependent Claim 111 words
Method for plasma-doping of impurity on a semiconductor substrate comprising the steps of: placing an object semiconductor substrate on a first electrode in a vacuum chamber, introducing a gas of a controlled reduced pressure containing at least one impurity, into said vacuum chamber, impressing a radio frequency current of a high voltage across said first electrode and a second electrode in said chamber through means for measuring said radio frequency current, thereby causing radio frequency discharging in said chamber to generate a plasma, and controlling said radio frequency current based on a measurement thereof in accordance with a program, to control amount of impurity doped on the surface of said substrate.
Claim 9
Dependent Claim 19 words
Method in accordance with claim 5, wherein said object substrate is on single-crystalline silicon, polycrystalline silicon or amorphous silicon.
Claim 10
Dependent Claim 14 words
Method in accordance with claim 5, wherein said impurity is boron, phosphorus or arsenide.
Claim 11
Dependent Claim 93 words
Method for plasma doping of impurity of a semiconductor substrate comprising the steps of: placing an object semiconductor substrate on a first electrode in a vacuum chamber, introducing a gas of a pressure of from 1×10 -3 torr to 5×10 -2 torr containing at least one impurity, into said vacuum chamber, intermittently impressing a radio frequency current of a high voltage across said first electrode and a second electrode in said chamber, and controlling the impressed period of said current to contol the amount of impurity doped on a surface of said substrate.
Claim 12
Dependent Claim 93 words
Method for plasma doping of impurity of a semiconductor substrate comprising the steps of: placing an object semiconductor substrate on a first electrode in a vacuum chamber, introducing a gas of a pressure of from 1×10 -3 torr to 5×10 -2 torr containing at least one impurity, into said vacuum chamber, intermittently impressing a radio frequency current of a high voltage across said first electrode and a second electrode in said chamber, and controlling the impressed period of said current to contol the amount of impurity doped on a surface of said substrate.
Claim 13
Dependent Claim 27 words
Method in accordance with claim 8, wherein the surface of the objective substrate is of single-crystalline silicon and have trenches as electrodes of capacitor or isolation region.
Claim 14
Dependent Claim 114 words
Method for plasma-doping of impurity on a semiconductor substrate comprising the steps of: placing an object semiconductor substrate on a first electrode in a vacuum chamber, introducing a gas of a pressure of from 1×10 -4 torr to 5×10 -2 torr containing at least one impurity, into said vacuum chamber, intermittently impressing a radio frequency current of a high voltage across said first electrode and a second electrode in said chamber and microwave into said chamber thereby causing radio frequency discharging and electronic cyclotron resonance discharge in said chamber, to generate plasma doping, and controlling the impressed period of said current to control the amount of impurity doped on a surface of said substrate.
Claim 15
Dependent Claim 114 words
Method for plasma-doping of impurity on a semiconductor substrate comprising the steps of: placing an object semiconductor substrate on a first electrode in a vacuum chamber, introducing a gas of a pressure of from 1×10 -4 torr to 5×10 -2 torr containing at least one impurity, into said vacuum chamber, intermittently impressing a radio frequency current of a high voltage across said first electrode and a second electrode in said chamber and microwave into said chamber thereby causing radio frequency discharging and electronic cyclotron resonance discharge in said chamber, to generate plasma doping, and controlling the impressed period of said current to control the amount of impurity doped on a surface of said substrate.
Claim 16
Dependent Claim 20 words
Method in accordance with claim 10, wherein said object semiconductor substrate is of single-crystalline silicon, polycrystalline silicon or amorphous silicon.
Claim 17
Dependent Claim 14 words
Method in accordance with claim 10, wherein said impurity is boron, phosphorus or arsenide.
Claim 18
Dependent Claim 27 words
Method in accordance with claim 10, wherein the surface of the objective substrate is of single-crystalline silicon and have trenches as electrodes of capacitor or isolation region.
Claim 19
Dependent Claim 93 words
Method for plasma-doping of impurity on a semiconductor substrate comprising the steps of: placing an object semiconductor substrate on a first electrode in a vacuum chamber. introducing a gas of a controlled reduced pressure containing at least one impurity, into said vacuum chamber, and impressing a radio frequency current of a high voltage in intermittence across said first electrode and a second electrode in said chamber thereby causing radio the frequency discharging in said chamber, frequency of said intermittence being changed to make plasma doping with depthwise modulated concentration in said semiconductor substrate.
Claim 20
Dependent Claim 93 words
Method for plasma-doping of impurity on a semiconductor substrate comprising the steps of: placing an object semiconductor substrate on a first electrode in a vacuum chamber. introducing a gas of a controlled reduced pressure containing at least one impurity, into said vacuum chamber, and impressing a radio frequency current of a high voltage in intermittence across said first electrode and a second electrode in said chamber thereby causing radio the frequency discharging in said chamber, frequency of said intermittence being changed to make plasma doping with depthwise modulated concentration in said semiconductor substrate.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-06-25 1993-12-25 1994-06-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-06-25 1997-12-25 1998-06-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-06-25 2001-12-25 2002-06-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag