Patent US4933131A successfully refreshed from Google Patents.
US4933131A
Expired / Lapsed
US
⏱️ 0.0 years remaining
Method of fabricating composite structures
Assignee: Sundstrand Corp
•
Filing: 1987-12-29
•
Granted: 1990-06-12
•
Expires: 2007-12-29
Abstract
Abstract A method of fabricating a composite structure having at least one skin molecularly bonded to a core. A skin is provided of reinforcing fibrous material and a thermoplastic matrix. The skin is thermoformed to the general exterior shape of the composite strucutre. The skin is placed in a mold, and a core material is injected into the mold against the skin under isostatic conditions. The core material includes a thermoplastic matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Inventors
- 👤 David W. Okey
- 👤 Hossein Saatchi
- 👤 John F. Scanlon
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-03 21:32
CPC Classifications
B; B29; B29D; B29D99/00; B29D99/001; B29D99/0021; B29C; B29C44/00; B29C44/02; B29C44/12; B29C44/14; B29C45/00; B29C45/14; B29C45/14778; B29C70/00; B29C70/04; B29C70/06; B29C70/08; B29C70/086; B32; B32B; B32B37/00; B29K; B29K2071/00; B29K2105/00; B29K2105/04; Y; Y10; Y10T; Y10T428/00; Y10T428/24; Y10T428/24149
Claims Analysis
Total Claims: 12
Claim 1
Independent Claim
86 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic polyetheretherketone matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under isostatic conditions, the core material including a thermoplastic matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 2
Independent Claim
86 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic polyetheretherketone matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under isostatic conditions, the core material including a thermoplastic matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 3
Independent Claim
86 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under isostatic conditions, the core material including a thermoplastic polyetheretherketone matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 4
Independent Claim
86 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under isostatic conditions, the core material including a thermoplastic polyetheretherketone matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 5
Independent Claim
87 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under isostatic conditions, the core material including a liquid crystal polymer matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 6
Independent Claim
87 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under isostatic conditions, the core material including a liquid crystal polymer matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 7
Independent Claim
86 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under isostatic conditions, the core material including a thermoplastic polyetherketone matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 8
Independent Claim
86 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under isostatic conditions, the core material including a thermoplastic polyetherketone matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 9
Independent Claim
86 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic polyetherketone matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under isostatic conditions, the core material including a thermoplastic matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 10
Independent Claim
86 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic polyetherketone matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under isostatic conditions, the core material including a thermoplastic matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 11
Independent Claim
90 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic polyetheretherketone matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under conditions of pressure and heat, the core material including a thermoplastic polyetheretherketone matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
Claim 12
Independent Claim
90 words
A method of fabricating a composite structure having at least one skin molecularly bonded to a core, comprising the steps of: providing a skin composed of reinforcing material and a thermoplastic polyetheretherketone matrix; thermoforming the skin to the general shape of the composite structure; and placing the skin in a mold and injecting a core material into the mold against the skin under conditions of pressure and heat, the core material including a thermoplastic polyetheretherketone matrix compatible to the thermoplastic matrix of the skin to form a molecular bond therewith.
References Cited (Backward Citations)
US2806509A
Cited
US4025686A
Cited
US4013810A
Cited
US4405543A
Cited
US4250136A
Cited
US4303728A
Cited
US4490317A
Cited
US4379103A
Cited
US4512836A
Cited
US4657717A
Cited
US4572856A
Cited
US4543289A
Cited
US4728698A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1993-06-11 | 1993-12-11 | 1994-06-12 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1997-06-11 | 1997-12-11 | 1998-06-12 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2001-06-11 | 2001-12-11 | 2002-06-12 | $7700.00 | Window Closed / Lapsed |