Abstract

Abstract In a method for continuous casting of an aluminum-lithium alloy through an open-ended mold for forming an ingot, wherein gas under pressure is brought into contact with a molten surface part of said ingot directly before solidification, the gas used consists of from 1 to 15 volume % of oxygen and balance of inert gas. The casting is stabilized and cast skin is improved by the use of said gas.

Inventors

  • 👤 Shigeru Yanagimoto
  • 👤 Ryoichi Kondo

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-10 02:24
CPC Classifications
B; B22; B22D; B22D11/00; B22D11/04; B22D11/045; B22D11/0401; B22D11/10; B22D11/11

Claims Analysis

Total Claims: 8
Claim 1
Independent Claim 51 words
A method for continuous casting of an aluminum-lithium alloy through an open-ended mold for forming an ingot, comprising, contacting a pressurized gas with a molten surface part directly before solidication, characterized in that said pressurized gas consists of from 1 to 15 volume % of oxygen and balance of inert gas.
Claim 2
Independent Claim 51 words
A method for continuous casting of an aluminum-lithium alloy through an open-ended mold for forming an ingot, comprising, contacting a pressurized gas with a molten surface part directly before solidication, characterized in that said pressurized gas consists of from 1 to 15 volume % of oxygen and balance of inert gas.
Claim 3
Dependent Claim 35 words
A method according to claim 1, wherein lubricating agent is fed to an inner circumferential surface of the open-ended mold, and pressure is applied to a circumferential part of the ingot, directly before the solidification.
Claim 4
Dependent Claim 27 words
A method according to claim 1, wherein said inert gas is at least one gas selected from the group consisting of nitrogen, argon, carbon dioxide, and helium.
Claim 5
Dependent Claim 15 words
A method according to claim 3, wherein the continuous casting method is a vertical casting.
Claim 6
Dependent Claim 15 words
A method according to claim 3, wherein the continuous casting method is a horizontal casting.
Claim 7
Dependent Claim 23 words
A method according to claim 1, 2, 3, 4, or 5, wherein said aluminum-lithium alloy contains 0.5% by weight or more of lithium.
Claim 8
Dependent Claim 19 words
A method according to claim 6, wherein said aluminum-lithium alloy contains from 0.5 to 5% by weight of lithium.

References Cited (Backward Citations)

US4200138A Cited
US4157728A Cited
US4157728B1 Cited
US4610295A Cited
US4651804A Cited
JPS60250860A Cited
US4567936A Cited
JPS62220248A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-06-04 1993-12-04 1994-06-05 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-06-04 1997-12-04 1998-06-05 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-06-04 2001-12-04 2002-06-05 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag