Abstract Silicon carbide whisker-reinforced ceramic composites are fabricated in a highly reproducible manner by beneficating the surfaces of the silicon carbide whiskers prior to their usage in the ceramic composites. The silicon carbide whiskers which contain considerable concentrations of surface oxides and other impurities which interact with the ceramic composite material to form a chemical bond are significantly reduced so that only a relatively weak chemical bond is formed between the whisker and the ceramic material. Thus, when the whiskers interact with a crack propagating into the composite the crack is diverted or deflected along the whisker-matrix interface due to the weak chemical bonding so as to deter the crack propagation through the composite. The depletion of the oxygen-containing compounds and other impurities on the whisker surfaces and near surface region is effected by heat treating the whiskers in a suitable oxygen sparaging atmosphere at elevated temperatures. Additionally, a sedimentation technique may be utilized to remove whiskers which suffer structural and physical anomalies which render them undesirable for use in the composite. Also, a layer of carbon may be provided on the surface of the whiskers to further inhibit chemical bonding of the whiskers to the ceramic composite material.

Inventors

  • 👤 Terry N. Tiegs
  • 👤 Terrence B. Lindemer

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 17:20
CPC Classifications
C; C04; C04B; C04B35/00; C04B35/71; C04B35/78; C04B35/80; C04B35/01; C04B35/10; C04B35/111; C04B35/117; C04B35/119; C04B35/16; C04B35/18; C04B35/185; C04B35/48; C04B35/486; C04B35/488; C04B35/50; C04B35/505; C04B35/515; C04B35/56; C04B35/563; C04B35/58; C04B35/584; C04B35/597; C04B35/622; C04B35/626; C04B35/62605; C04B35/62645; C04B35/6265; C04B35/62675; C04B35/6268; C04B35/628; C04B35/62844; C04B35/62847; C04B35/62849; C04B35/62857; C04B35/62873; C04B35/62894; C04B35/62897; C04B2235/00; C04B2235/02; C04B2235/50; C04B2235/52; C04B2235/5208; C04B2235/5216; C04B2235/524; C04B2235/5244; C04B2235/5264; C04B2235/5276; C04B2235/5296; C04B2235/70; C04B2235/72; C04B2235/96; Y; Y10; Y10T; Y10T428/00; Y10T428/29; Y10T428/2913; Y10T428/2918; Y10T428/292; Y10T428/2933; Y10T428/2938

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 117 words
A ceramic composite comprising a ceramic matrix having elongated monocrystalline silicon carbide whiskers homogeneously dispersed therein with said whiskers being retained in said matrix with an insufficient bond at a matrix-whisker interface to promote debonding along said whisker-matrix interface when a crack propagating into said ceramic composite contacts said whiskers thereby providing bridging and deflection of said crack by said whiskers when said ceramic composite is subjected to sufficient stress to effect propagation of said crack therein, said whiskers having a surface characterized by a silicon dioxide-to-silicon carbide ratio of less than 0.1, a concentration of calcium oxide less than about 1.5 wt. %, and a coating of free carbon on said surface of about 1-100 angstroms.
Claim 2
Dependent Claim 117 words
A ceramic composite comprising a ceramic matrix having elongated monocrystalline silicon carbide whiskers homogeneously dispersed therein with said whiskers being retained in said matrix with an insufficient bond at a matrix-whisker interface to promote debonding along said whisker-matrix interface when a crack propagating into said ceramic composite contacts said whiskers thereby providing bridging and deflection of said crack by said whiskers when said ceramic composite is subjected to sufficient stress to effect propagation of said crack therein, said whiskers having a surface characterized by a silicon dioxide-to-silicon carbide ratio of less than 0.1, a concentration of calcium oxide less than about 1.5 wt. %, and a coating of free carbon on said surface of about 1-100 angstroms.
Claim 3
Dependent Claim 35 words
The ceramic composite claimed in claim 1, wherein said whiskers are in a size range having a diameter in the range of about 0.1 to 10 μm and a length-to-diameter ratio greater than about 10.
Claim 4
Dependent Claim 30 words
The ceramic composite as claimed in claim 1, wherein said ceramic matrix is selected from the group consisting of alumina, boron carbide, silicon nitride, sialons, mullite, zirconia, alumina-zirconia and yttria.
Claim 5
Dependent Claim 80 words
A ceramic composite comprising a ceramic matrix having elongated monocrystalline silicon carbide whiskers homogeneously dispersed therein, said whiskers having a diameter in the range of about 0.1 to 10 μm and a length to diameter ratio greater than about 10, said whiskers having a surface characterized by a silicon dioxide-to-silicon carbide ratio of less than 0.1, a concentration of calcium oxide less than about 1.5 wt. %, and a coating of free carbon on said surface of about 1-100 angstroms.
Claim 6
Dependent Claim 80 words
A ceramic composite comprising a ceramic matrix having elongated monocrystalline silicon carbide whiskers homogeneously dispersed therein, said whiskers having a diameter in the range of about 0.1 to 10 μm and a length to diameter ratio greater than about 10, said whiskers having a surface characterized by a silicon dioxide-to-silicon carbide ratio of less than 0.1, a concentration of calcium oxide less than about 1.5 wt. %, and a coating of free carbon on said surface of about 1-100 angstroms.

References Cited (Backward Citations)

US32843A Cited
US4194914A Cited
US4340636A Cited
US4543345A Cited
USRE32843E Cited
EP0172082A1 Cited
US4642271A Cited
US4652413A Cited
US4657877A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-04-09 1993-10-09 1994-04-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-04-09 1997-10-09 1998-04-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-04-09 2001-10-09 2002-04-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag