Abstract The invention provides an electrode for piezoelectric composites having high acoustic attenuation. The electrode is composed of a first layer having high elasticity and lower conductivity and of a second layer lying thereabove that has higher conductivity. The invention also provides a method for the manufacture thereof. The first layer is an intrinsically conductive plastic directly deposited on the ceramic whose polymerization is initiated by chemical or anodic oxidation of the corresponding monomers. The second layer is fashioned of adequately conductive metal and is preferably first sputtered on or vapor-deposited in a thinner layer and is then subsequently electrolytically reinforced. Piezoelectric composites that exhibit high acoustic attenation and, thus, prevent an acoustic crosstalk between the individual transducer elements can be manufactured from piezoelectric ceramic lamina or foils provided with such electrodes. Such composites also withstand higher mechanical distortion (for example, due to thermal expansion), even if the ceramic is highly porous.

Inventors

  • 👤 Wolfram Wersing
  • 👤 Manfred Schnoeller
  • 👤 Karl Lubitz
  • 👤 Jutta Mohaupt

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 07:11
CPC Classifications
H; H03; H03H; H03H9/00; H03H9/02; H03H9/125; H03H9/13; H03H9/131; H10; H10N; H10N30/00; H10N30/01; H10N30/06; H10N30/80; H10N30/87; H10N30/877; H10N30/878; Y; Y10; Y10S; Y10S310/00; Y10S310/80

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 55 words
An electrode for piezoelectric composites having high acoustic attenuation comprising: a first layer composed of an intrinsically conductive plastic that is generated directly on a ceramic of a piezoelement by polymerization and having a higher elasticity than the ceramic; and a second layer composed of a metal having a higher conductivity than the plastic layer.
Claim 2
Dependent Claim 55 words
An electrode for piezoelectric composites having high acoustic attenuation comprising: a first layer composed of an intrinsically conductive plastic that is generated directly on a ceramic of a piezoelement by polymerization and having a higher elasticity than the ceramic; and a second layer composed of a metal having a higher conductivity than the plastic layer.
Claim 3
Dependent Claim 33 words
The electrode of claim 1 wherein: the thickness of the first layer is approximately 1 to about 15 um; and the thickness of the second layer is approximately 0.1 to about 20 um.
Claim 4
Dependent Claim 33 words
The electrode of claim 2 wherein: the thickness of the first layer is approximately 1 to about 15 um; and the thickness of the second layer is approximately 0.1 to about 20 um.
Claim 5
Dependent Claim 55 words
A piezoelectric composite for ultrasound transmission/reception equipment, including an electrode having high acoustic attenuation, the electrode comprising: a first layer, composed of an intrinsically conductive plastic deposited by polymerization on a ceramic, the layer having a high elasticity and a low conductivity in comparison to the ceramic; and a second layer composed of a metal.
Claim 6
Dependent Claim 55 words
A piezoelectric composite for ultrasound transmission/reception equipment, including an electrode having high acoustic attenuation, the electrode comprising: a first layer, composed of an intrinsically conductive plastic deposited by polymerization on a ceramic, the layer having a high elasticity and a low conductivity in comparison to the ceramic; and a second layer composed of a metal.
Claim 7
Dependent Claim 33 words
The electrode of claim 4 wherein: the thickness of the first layer is approximately 1 to about 15 um; and the thickness of the second layer is approximately 0.1 to about 20 um.

References Cited (Backward Citations)

US2077204A Cited
US2648785A Cited
US3803545A Cited
US3872332A Cited
US3912830A Cited
JPS513183A Cited
US4404489A Cited
US4695756A Cited
EP0154701A1 Cited
US4609845A Cited
US4701659A Cited
US4786837A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1993-02-12 1993-08-14 1994-02-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1997-02-12 1997-08-14 1998-02-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2001-02-12 2001-08-14 2002-02-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag