Process for producing a filament-containing composite in a ceramic matrix
Assignee: General Electric Co
•
Filing: 1987-12-14
•
Granted: 1989-12-12
•
Expires: 2007-12-14
Abstract
Abstract A composite is produced by admixing a matrix-forming material with organic binding material, forming the resulting mixture into a tape, disposing a layer of spaced filaments between at least two of the tapes to form a layered structure, laminating the layered structure, heating the layered structure to remove organic binding material and hot pressing the resulting porous structure to form a composite containing spaced filaments.
Inventors
- 👤 Raj N. Singh
- 👤 Achuta R. Gaddipati
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-04 18:28
CPC Classifications
C; C04; C04B; C04B35/00; C04B35/622; C04B35/626; C04B35/63; C04B35/632; C04B35/634; C04B35/63404; C04B35/63416; C04B35/6342; C04B35/63424; C04B35/63432; C04B35/63448; C04B35/63468; C04B35/64; C04B35/645; Y; Y10; Y10T; Y10T428/00; Y10T428/12; Y10T428/12014; Y10T428/12028; Y10T428/12049; Y10T428/12056; Y10T428/30
Claims Analysis
Total Claims: 9
Claim 1
Independent Claim
231 words
A process for producing a composite containing a layer of filaments embedded in a ceramic matrix which comprises the following steps: (a) providing matrix-forming ceramic material; (b) admixing said matrix-forming material with an organic binding material; (c) forming the resulting mixture into a tape; (d) providing a filament having a diameter of at least about 50 microns and a length at least about 10 times its diameter; (e) forming a plurality of said filaments into a layer wherein said filaments are spaced from each other and at least substantially parallel to each other; (f) disposing said layer of filaments intermediate the faces of two of said tapes forming a layered structure; (g) laminating the layered structure to form a laminated structure; (h) heating said laminate structure to remove said organic binding material leaving no significant deleterious residue; and (i) hot pressing the resulting porous structure at a sufficient temperature under a sufficient pressure for a sufficient period of time to consolidate said structure to produce said composite having a porosity of less than about 5% by volume, said composite containing no significant reaction product of said filaments and said matrix, said matrix having a thermal expansion coefficient which ranges from lower than that of said filaments to less than about 15% higher than that of said filaments, at least about 10% by volume of said composite being comprised of spaced filaments.
Claim 2
Dependent Claim
231 words
A process for producing a composite containing a layer of filaments embedded in a ceramic matrix which comprises the following steps: (a) providing matrix-forming ceramic material; (b) admixing said matrix-forming material with an organic binding material; (c) forming the resulting mixture into a tape; (d) providing a filament having a diameter of at least about 50 microns and a length at least about 10 times its diameter; (e) forming a plurality of said filaments into a layer wherein said filaments are spaced from each other and at least substantially parallel to each other; (f) disposing said layer of filaments intermediate the faces of two of said tapes forming a layered structure; (g) laminating the layered structure to form a laminated structure; (h) heating said laminate structure to remove said organic binding material leaving no significant deleterious residue; and (i) hot pressing the resulting porous structure at a sufficient temperature under a sufficient pressure for a sufficient period of time to consolidate said structure to produce said composite having a porosity of less than about 5% by volume, said composite containing no significant reaction product of said filaments and said matrix, said matrix having a thermal expansion coefficient which ranges from lower than that of said filaments to less than about 15% higher than that of said filaments, at least about 10% by volume of said composite being comprised of spaced filaments.
Claim 3
Dependent Claim
51 words
The process according to claim 1 wherein said filaments are selected from the group consisting of elemental carbon, a silicon carbide-containing material containing at least about 50% by weight of silicon and at least about 25% by weight of carbon based on the weight of said material, and a combination thereof.
Claim 4
Dependent Claim
16 words
The process according to claim 1 wherein said matrix-forming material is comprised of polycrystalline ceramic particulates.
Claim 5
Dependent Claim
23 words
The process according to claim 1 wherein said matrix-forming material is comprised of particulates selected from the group consisting of mullite and zircon.
Claim 6
Dependent Claim
32 words
The process according to claim 1 wherein said matrix-forming material is comprised of polycrystalline ceramic particulates and whiskers wherein said whiskers range up to about 30% by volume of said matrix-forming material.
Claim 7
Dependent Claim
52 words
The process according to claim 1 wherein before said layered structure is assembled, an organic solution of organic binder is sprayed on the faces of the tapes to be contacted with the filaments and dried to leave a sticky film of organic binder in amount sufficient to at least significantly enhance adhesion.
Claim 8
Dependent Claim
31 words
The process according to claim 1 wherein said matrix has a thermal expansion coefficient ranging from lower than that of said filaments to about the same as that of said filaments.
Claim 9
Dependent Claim
37 words
The process according to claim 1 wherein a plurality of said layers of filaments is used in forming the layered structure and wherein all of said layers of filaments are separated from each other by said tape.
References Cited (Backward Citations)
US3565683A
Cited
US3788893A
Cited
US4142008A
Cited
US4141948A
Cited
US4120731A
Cited
US4220455A
Cited
US4247304A
Cited
US4377564A
Cited
US4663230A
Cited
US4642271A
Cited
US4628002A
Cited
US4764427A
Cited
US4737476A
Cited
US4759950A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1992-12-11 | 1993-06-12 | 1993-12-12 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1996-12-11 | 1997-06-12 | 1997-12-12 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 2000-12-11 | 2001-06-12 | 2001-12-12 | $7700.00 | Window Closed / Lapsed |