Abstract Oxide cathode wires are produced by coating tungsten wires with emissive material by cataphoretic coating. It is important for the coating to have a substantially uniform thickness over the entire surface of the wire. This is achieved in a simple manner by reversing the polarity of the direction of current flow for a short time at the beginning of the coating process, so that the tungsten wire to be coated is connected as an anode. The remainder of the coating process is performed in a known manner with a tungsten wire connected as a cathode.

Inventors

  • 👤 Herbert Hemminger
  • 👤 Michael Schlipf

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-08 23:43
CPC Classifications
C; C25; C25D; C25D13/00; C25D13/12; C25D13/16; C25D13/02

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 78 words
A method of coating cathode wires by cataphorectically coating wires with an emissive material suspended in an electrolyte, comprising the steps of: suspending a wire in a suspension of emissive material in an electrolyte; connecting the wire as an anode for about a fraction of a second to about a few seconds; and thereafter connecting the wire as a cathode in the same suspension, whereby a uniform coating of the emissive material is cataphoretically coated on said wire.
Claim 2
Independent Claim 78 words
A method of coating cathode wires by cataphorectically coating wires with an emissive material suspended in an electrolyte, comprising the steps of: suspending a wire in a suspension of emissive material in an electrolyte; connecting the wire as an anode for about a fraction of a second to about a few seconds; and thereafter connecting the wire as a cathode in the same suspension, whereby a uniform coating of the emissive material is cataphoretically coated on said wire.
Claim 3
Dependent Claim 20 words
A method as described in claim 1, wherein the electrolyte contains diethyl carbonate, diethyl oxalate, ethyl alcohol, acetone and methanol.
Claim 4
Dependent Claim 15 words
A method as described in claim 2, wherein a counterelectrode of stainless steel is used.
Claim 5
Dependent Claim 24 words
A method as described in claim 3, wherein the wires to be coated are subjected to a pretreatment consisting of washing and reductive annealing.
Claim 6
Dependent Claim 24 words
A method as described in claim 2, wherein the wires to be coated are subjected to a pretreatment consisting of washing and reductive annealing.
Claim 7
Dependent Claim 15 words
A method as described in claim 1, wherein a counterelectrode of stainless steel is used.
Claim 8
Dependent Claim 24 words
A method as described in claim 6, wherein the wires to be coated are subjected to a pretreatment consisting of washing and reductive annealing.
Claim 9
Dependent Claim 27 words
A method as described in claim 1, wherein the emissive material is selected from a group consisting of barium carbonate, strontium carbonate, calcium carbonate and mixtures thereof.
Claim 10
Dependent Claim 15 words
A method as described in claim 8, wherein a counterelectrode of stainless steel is used.
Claim 11
Dependent Claim 24 words
A method as described in claim 9, wherein the wires to be coated are subjected to a pretreatment consisting of washing and reductive annealing.
Claim 12
Dependent Claim 24 words
A method as described in claim 8, wherein the wires to be coated are subjected to a pretreatment consisting of washing and reductive annealing.
Claim 13
Dependent Claim 24 words
A method as described in claim 1, wherein the wires to be coated are subjected to a pretreatment consisting of washing and reductive annealing.

References Cited (Backward Citations)

US4026780A Cited
US4100449A Cited
US4252630A Cited
US4302309A Cited
US4487673A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1992-02-21 1992-08-22 1993-02-21 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1996-02-21 1996-08-22 1997-02-21 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 2000-02-21 2000-08-22 2001-02-21 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag