Photolithographic mask repair system
Assignee: JPMorgan Chase Bank NA
•
Filing: 1986-10-17
•
Granted: 1988-10-18
•
Expires: 2006-10-17
Abstract
Abstract A method and device are provided to accomplish laser driven pyrolytic, photolytic and photoactivativation process requiring controlled atmosphere without the use of gas tight cells. A method and device are provided to correct clear faults on a photo-lithographic mask by metallic deposition on the mask at standard temperature and pressure. The deposition is formed by the pyrolytic decomposition of an organometallic gas mixture which may include chromium and molybdenum hexacarbonyls, and a buffer gas. The decomposition is done utilizing a laser beam. The device may be incorporated into a system which has other members used to correct opaque faults in the same mask.
Inventors
- 👤 Zbigniew Drozdowicz
- 👤 Harvey Stone
- 👤 John Vogler
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-10-28 18:57
CPC Classifications
G; G03; G03F; G03F1/00; G03F1/68; G03F1/72; B; B23; B23K; B23K26/00; B23K26/14; B23K26/144; C; C23; C23C; C23C16/00; C23C16/04; C23C16/047; C23C16/44; C23C16/48; C23C16/483; H; H05; H05K; H05K3/00; H05K3/10; H05K3/14; H05K3/146; H05K3/22; H05K3/225; Y; Y10; Y10S; Y10S430/00; Y10S430/146
Claims Analysis
Total Claims: 22
Claim 1
Independent Claim
140 words
A method of preparing a surface for coating by creating a volume of controlled atmosphere, at substantially ambient temperature and pressure, without using a gas-tight cell, comprising: delivering a gas mixture including an effective amount of organometallic gas to the volume between a microscope objective and the surface, on which deposits are to be made or which is to be etched or otherwise modified, so that air, normally contained therein, is partially or fully displaced by said gas mixture; inducing a reaction in said gas mixture such that deposits are made therefrom onto the surface; and surrounding said objective by one or more shrouds, at least one of which is used to collect all the gaseous components produced in reactions occurring in said volume together with an unused portion of the said gas mixture and to safely vent them away.
Claim 2
Independent Claim
140 words
A method of preparing a surface for coating by creating a volume of controlled atmosphere, at substantially ambient temperature and pressure, without using a gas-tight cell, comprising: delivering a gas mixture including an effective amount of organometallic gas to the volume between a microscope objective and the surface, on which deposits are to be made or which is to be etched or otherwise modified, so that air, normally contained therein, is partially or fully displaced by said gas mixture; inducing a reaction in said gas mixture such that deposits are made therefrom onto the surface; and surrounding said objective by one or more shrouds, at least one of which is used to collect all the gaseous components produced in reactions occurring in said volume together with an unused portion of the said gas mixture and to safely vent them away.
Claim 3
Dependent Claim
21 words
The method of claim 1 wherein said objective is kept clear of said gas mixture by additional flow of buffer gas.
Claim 4
Dependent Claim
25 words
The method of claim 1 wherein said objective is used to deliver laser radiation to said surface to effect heating or photoactivation of said surface.
Claim 5
Dependent Claim
35 words
The method of claim 2 wherein said objective is used to deliver laser radiation to the vicinity of said surface to effect photolytic or combination photolytic/pyrolytic decomposition or activation of components of said gas mixture.
Claim 6
Independent Claim
62 words
A method of correcting clear faults on a photolithographic mask without a gas-tight cell comprising: providing a gas mixture at substantially ambient pressure and temperature in a region adjacent to said clear fault, said gas mixture including an effective amount of organometallic compound; and heating said mixture to decompose said organometallic compound into a metallic layer which deposits on said clear fault.
Claim 7
Independent Claim
62 words
A method of correcting clear faults on a photolithographic mask without a gas-tight cell comprising: providing a gas mixture at substantially ambient pressure and temperature in a region adjacent to said clear fault, said gas mixture including an effective amount of organometallic compound; and heating said mixture to decompose said organometallic compound into a metallic layer which deposits on said clear fault.
Claim 8
Dependent Claim
19 words
The method of claim 5 wherein said heating includes the step of applying a laser beam to said compound.
Claim 9
Dependent Claim
17 words
The method of claim 5 wherein said organometallic compound is selected from chromium hexacarbonyl, and molybdenum hexacarbonyl.
Claim 10
Dependent Claim
17 words
The method of claim 5 wherein said compound is a mixture of molybdenum hexacarbonyl and chromium hexacarbonyl.
Claim 11
Dependent Claim
22 words
The method of claim 5 when said mixture further includes a carrier gas selected from the group of argon, helium and nitrogen.
Claim 12
Independent Claim
148 words
A system for correcting opaque and clear defects on a photolithographic mask comprising: a first laser beam source; a second laser beam source; a laser beam delivery system for selective delivery of a laser beam from one of said first and second laser beam sources to said objective; and a source of an organometallic gas mixture coupled to the volume between said objective and mask; means for correcting opaque defects by directing the laser beam from the first source through said objective said laser beam removing excessive material from said mask; and means for correcting clear defects by directing the laser beam from the second source through said objective; and means for providing organometallic gas at substantially ambient pressure and temperature from said source to said volume, said laser beam from said second source decomposing said gas to deposit a layer of opaque material on said clear fault.
Claim 13
Independent Claim
148 words
A system for correcting opaque and clear defects on a photolithographic mask comprising: a first laser beam source; a second laser beam source; a laser beam delivery system for selective delivery of a laser beam from one of said first and second laser beam sources to said objective; and a source of an organometallic gas mixture coupled to the volume between said objective and mask; means for correcting opaque defects by directing the laser beam from the first source through said objective said laser beam removing excessive material from said mask; and means for correcting clear defects by directing the laser beam from the second source through said objective; and means for providing organometallic gas at substantially ambient pressure and temperature from said source to said volume, said laser beam from said second source decomposing said gas to deposit a layer of opaque material on said clear fault.
Claim 14
Dependent Claim
18 words
The system of claim 10 wherein said first laser source comprises an Nd:YAG laser and an SHG crystal.
Claim 15
Dependent Claim
13 words
The system of claim 10 wherein said second source includes an argon laser.
Claim 16
Dependent Claim
17 words
The system of claim 10 wherein said laser delivery system comprises several microscope objectives having different magnifications.
Claim 17
Dependent Claim
18 words
The system of claim 13 wherein one or more of said objectives is individually surrounded by said shroud.
Claim 18
Dependent Claim
22 words
The system of claim 14 wherein said shroud comprises a first pipe for coupling to said gas source, and an exhaust pipe.
Claim 19
Dependent Claim
22 words
The system of claim 15 wherein said shroud further comprises a cylindrical chamber disposed coaxially around said objective for concentrating said gas.
Claim 20
Dependent Claim
24 words
The system of claim 16 further comprising means for delivery a buffer gas to said objective to keep active gases away from said objective.
Claim 21
Dependent Claim
29 words
The system of claim 14 further comprising a vent chamber for exhausting gases from the shroud and coupling means for coupling said venting chamber to one of said shrouds.
Claim 22
Dependent Claim
33 words
The system of claim 10 wherein said laser delivery system comprises an objective with reflective mirrors and means for supplying a buffer gas to said objective to keep gases away from said mirrors.
References Cited (Backward Citations)
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1991-10-18 | 1992-04-18 | 1992-10-18 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1995-10-18 | 1996-04-18 | 1996-10-18 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1999-10-18 | 2000-04-18 | 2000-10-18 | $7700.00 | Window Closed / Lapsed |