Method for forming a titanium lined electrochemical cell

Assignee: Dow Chemical Co
•
Filing: 1987-02-12
•
Granted: 1988-08-23
•
Expires: 2007-02-12
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The invention is a method comprising: welding a titanium sheet having a thickness of less than about 2 millimeters to a ferrous material through a weldably compatible intermediate material and a titanium intermediate.

Inventors

  • 👤 Hiep D. Dang
  • 👤 Richard N. Beaver

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 23:41
CPC Classifications
B; B23; B23K; B23K35/00; B23K35/001; B23K35/005; B23K11/00; B23K11/16; B23K11/20

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 73 words
A method for welding a thin titanium sheet to a ferrous substrate comprising sequentially performing the following steps: (a) positioning a substantially homogenous vanadium intermediate adjacent to one surface of a ferrous substrate; (b) then welding a substantially homogenous titanium intermediate to the vanadium, intermediate, and welding said vanadium intermediate to said ferrous substrate; (c) then welding a titanium sheet having a thickness of less than about 2 millimeters to the titanium intermediate.
Claim 2
Independent Claim 73 words
A method for welding a thin titanium sheet to a ferrous substrate comprising sequentially performing the following steps: (a) positioning a substantially homogenous vanadium intermediate adjacent to one surface of a ferrous substrate; (b) then welding a substantially homogenous titanium intermediate to the vanadium, intermediate, and welding said vanadium intermediate to said ferrous substrate; (c) then welding a titanium sheet having a thickness of less than about 2 millimeters to the titanium intermediate.
Claim 3
Dependent Claim 16 words
The method of claim 1 wherein the titanium intermediate is less than about 2 millimeters thick.
Claim 4
Dependent Claim 15 words
The method of claim 1 wherein the vanadium is less than about 0.5 millimeter thick.
Claim 5
Dependent Claim 25 words
The method of claim 1 wherein the ferrous material is selected from the group consisting of iron, cast iron, ductile iron, steel, and stainless steel.
Claim 6
Independent Claim 78 words
A method for welding a thin titanium sheet to a ferrous substrate comprising sequentially performing the following steps: (a) positioning a plurality of spaced-apart substantially homogenous vanadium intermediates adjacent to one surface of a ferrous substrate; (b) then welding a homogenous titanium intermediate to each of the vanadium intermediates, and welding each said vanadium intermediate to said ferrous substrate; (c) then welding a titanium sheet having a thickness of less than about 2 millimeters to the titanium intermediates.
Claim 7
Independent Claim 78 words
A method for welding a thin titanium sheet to a ferrous substrate comprising sequentially performing the following steps: (a) positioning a plurality of spaced-apart substantially homogenous vanadium intermediates adjacent to one surface of a ferrous substrate; (b) then welding a homogenous titanium intermediate to each of the vanadium intermediates, and welding each said vanadium intermediate to said ferrous substrate; (c) then welding a titanium sheet having a thickness of less than about 2 millimeters to the titanium intermediates.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-08-23 1992-02-22 1992-08-23 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-08-23 1996-02-22 1996-08-23 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-08-23 2000-02-22 2000-08-23 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag