Abstract

Abstract Accurate metered amounts of Pnictide 4 species are delivered via an argon carrier gas into an evacuated sputtering deposition chamber. The pnictide is maintained at a high temperature in a tall column by means of a constant temperature oil bath. An inert gas, such as argon, is passed through the column of Pnictide and the Pnictide 4 enriched carrier gas delivered to the vacuum chamber. Films of pnictide, polypnictide, and other pnictide compounds may be deposited for semiconductor, thin film transistors, and other applications including insulation and passivation, particularly on III-V semiconductors. The local order of the deposited films may be controlled by varying the amount of energy delivered to the surface of the substrate, which is a function of its temperature, the RF power used, and the amount of excess P 4 supplied. The pnictides used in the invention may include phosphorus, arsenic and antimony. Phosphorous and KP 15 , and KP x wherein x ranges from 15 to infinity are discussed. Deposition onto III-V semiconductors (InP, GaP, and GaAs) are disclosed.

Inventors

  • 👤 Rozalie Schachter
  • 👤 Marcello Viscogliosi

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-04 18:55
CPC Classifications
H; H10; H10P; H10P14/00; H10P14/60; H10P14/63; H10P14/6326; H10P14/6328; H10P14/6329; C; C23; C23C; C23C14/00; C23C14/22; C23C14/34; H10D; H10D64/00; H10D64/60; H10D64/66; H10D64/68; H10P14/40; H10P14/412; H10P14/68; H10K; H10K10/00; H10K10/40; H10K10/46; H10K10/462

Claims Analysis

Total Claims: 20
Claim 1
Independent Claim 78 words
The method of vacuum deposition of an elemental pnictide comprising the steps of: passing a gas inert to elemental pnictide through a heated condensed phase elemental pnictide material to provide an elemental pnictide vapor, generating a plasma in a vacuum chamber by electrically energizing inert gas therein, passing said elemental pnictide vapor through said electrically generated inert gas plasma in said vacuum chamber, and depositing elemental pnictide from said vapor on a stationary substrate in said vacuum chamber.
Claim 2
Independent Claim 78 words
The method of vacuum deposition of an elemental pnictide comprising the steps of: passing a gas inert to elemental pnictide through a heated condensed phase elemental pnictide material to provide an elemental pnictide vapor, generating a plasma in a vacuum chamber by electrically energizing inert gas therein, passing said elemental pnictide vapor through said electrically generated inert gas plasma in said vacuum chamber, and depositing elemental pnictide from said vapor on a stationary substrate in said vacuum chamber.
Claim 3
Dependent Claim 18 words
The method of claim 1 wherein said vacuum chamber is maintained at a pressure above 10 -4 Torr.
Claim 4
Independent Claim 94 words
A method of vacuum deposition of an elemental pnictide or pnictide containing film on a substrate comprising the steps of: passing a gas inert to elemental pnictide through a source of heated condensed phase elemental pnictide for carrying pnictide vapor therefrom, supplying said inert gas and said pnictide to a vacuum chamber housing a substrate for providing pnictide vapor in said vacuum chamber, and sputtering a pnictide containing target within said vacuum chamber in said environment of elemental pnictide vapor and inert gas to form a pnictide or pnictide containing film on said substrate.
Claim 5
Independent Claim 94 words
A method of vacuum deposition of an elemental pnictide or pnictide containing film on a substrate comprising the steps of: passing a gas inert to elemental pnictide through a source of heated condensed phase elemental pnictide for carrying pnictide vapor therefrom, supplying said inert gas and said pnictide to a vacuum chamber housing a substrate for providing pnictide vapor in said vacuum chamber, and sputtering a pnictide containing target within said vacuum chamber in said environment of elemental pnictide vapor and inert gas to form a pnictide or pnictide containing film on said substrate.
Claim 6
Dependent Claim 15 words
The method of claim 3 including the step of: providing KP 15 as said target.
Claim 7
Dependent Claim 24 words
The method of claim 4 further including the step of maintaining the pressure within said vacuum chamber at a level above 10 -4 Torr.
Claim 8
Dependent Claim 23 words
The method of claim 4 wherein said heated pnictide is introduced into said vacuum chamber in the form of a pnictide 4 species.
Claim 9
Dependent Claim 29 words
The method of claim 4 further including the step of controlling the local order of the pnictide film deposited on said substrate by controlling the temperature of said substrate.
Claim 10
Dependent Claim 31 words
The method of claim 4 further including the step of controlling the local order of said pnictide film deposited on said substrate by controlling the energy emitted during said sputtering apparatus.
Claim 11
Dependent Claim 42 words
The method of claim 4 further including the step of controlling the local order of the deposition of said pnictide film deposited on said substrate by controlling the rate of supply of said pnictide to said vacuum chamber from said pnictide source.
Claim 12
Dependent Claim 15 words
The method of claim 4 wherein said sputtering step is done by an RF sputterer.
Claim 13
Dependent Claim 54 words
The method of claim 4 further including the step of controlling the local order of said pnictide film deposited on said substrate by: controlling the temperature of said substrate, controlling the energy emitted during said sputtering step, and controlling the rate of supply of said pnictide to said vacuum chamber from said pnictide source.
Claim 14
Dependent Claim 17 words
The method of claim 3 wherein said inert gas in said vacuum chamber is in a plasma.
Claim 15
Dependent Claim 41 words
The method of claim 12 further including the step of: supplying said inert gas for carrying said pnictide to said vacuum chamber and supplying said inert gas as a plasma in said vacuum chamber from a common source of inert gas.
Claim 16
Dependent Claim 31 words
The method of claim 12 including the step of simultaneously supplying said inert carrier gas to said pnictide source and to said vacuum chamber from said common source of inert gas.
Claim 17
Independent Claim 14 words
The method of claims 12, 13 or 14 wherein said inert gas is argon.
Claim 18
Dependent Claim 11 words
The method of claim 3 wherein said pnictide source is phorphorus.
Claim 19
Dependent Claim 11 words
The method of claim 3 wherein said pnictide source is arsenic.
Claim 20
Independent Claim 15 words
The method of claims 1, 2, 3 or 4 wherein said pnictide source is antimony.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-08-02 1992-02-01 1992-08-02 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-08-02 1996-02-01 1996-08-02 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-08-02 2000-02-01 2000-08-02 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag