Abstract

Abstract The present invention discloses multi-layered resist structures and methods of producing them which can be used in electronic device lithography to produce micrometer and submicrometer geometries. The resist structure comprises two or more layers at least one of which is a metallic material and at least one of which is a radiation-sensitive material. The metallic layer exhibits both a high atomic number and a high density. The metallic material is positioned relative to the radiation-sensitive polymeric material so that it can be used to control reflection and backscatter of radiation used to create a latent image within the radiation-sensitive polymeric material. The thickness of the metallic layer is determined by the amount of reflection desired and the amount of backscatter permitted into the layer of radiation-sensitive polymeric material.

Inventors

  • 👤 Lawrence V. Gregor

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-06 00:56
CPC Classifications
G; G03; G03F; G03F7/00; G03F7/004; G03F7/09; G03F7/094; G03F7/091; Y; Y10; Y10S; Y10S430/00; Y10S430/143; Y10S438/00; Y10S438/942; Y10S438/948; Y10S438/95

Claims Analysis

Total Claims: 6
Claim 1
Independent Claim 128 words
A method of producing a multi-layer resist structure for use in fabrication of electronic devices, comprising the steps of: (a) Applying a thin layer of a metal or an alloy of said metal to the surface of a substrate, wherein the atomic number of said metallic layer ranges between about 60 and about 84 and the density of said metallic layer ranges between about 12 g/cm 2 and about 23 g/cm 2 , and wherein the thickness of said metallic layer ranges between about 400 Å and about 4,000 Å; (b) applying a layer of radiation-sensitive polymeric material over the surface of said metallic layer; and (c) exposing the surface of said radiation-sensitive polymeric material to patterned radiation to create a latent image within said radiation-sensitive polymeric material.
Claim 2
Independent Claim 128 words
A method of producing a multi-layer resist structure for use in fabrication of electronic devices, comprising the steps of: (a) Applying a thin layer of a metal or an alloy of said metal to the surface of a substrate, wherein the atomic number of said metallic layer ranges between about 60 and about 84 and the density of said metallic layer ranges between about 12 g/cm 2 and about 23 g/cm 2 , and wherein the thickness of said metallic layer ranges between about 400 Å and about 4,000 Å; (b) applying a layer of radiation-sensitive polymeric material over the surface of said metallic layer; and (c) exposing the surface of said radiation-sensitive polymeric material to patterned radiation to create a latent image within said radiation-sensitive polymeric material.
Claim 3
Dependent Claim 12 words
The method of claim 1 wherein said substrate is a polymeric material.
Claim 4
Dependent Claim 22 words
The method of claim 2 wherein said substrate polymeric material is selected from the group consisting of baked novolaks, polyimides, and polyarylsulfones.
Claim 5
Dependent Claim 32 words
The method of claim 1 wherein said metal is comprised of a metallic material selected from the group consisting of hafmum, tantalum, tungsten, rhenium, lead, and alloys of metals within said group.
Claim 6
Dependent Claim 27 words
The method of claim 1 wherein said radiation-sensitive polymeric material is comprised of a resist material selected from the group consisting of polysulfone-novolaks, diazoquinone-novolaks, polymethylmethacrylates, and polysiloxanes.

References Cited (Backward Citations)

US4165395A Cited
US4494004A Cited
US4362598A Cited
US4493855A Cited
US4612275A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1991-05-17 1991-11-16 1992-05-17 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1995-05-17 1995-11-16 1996-05-17 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1999-05-17 1999-11-16 2000-05-17 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag