Claims Analysis
Total Claims: 10
Claim 1
Independent Claim
129 words
A negative silver halide photographic light-sensitive material having a silver halide emulsion layer, which layer comprises monodispersed cubic or tetradecahedral silver haloiodide grains prepared in the presence of an iridium salt in an amount of 1×10 -8 to 1×10 -5 mole per one mole of silver, wherein the silver iodide content in the surface part of said grain is larger than the average silver iodide content in said grain, and additionally containing in said emulsion layer or in some other hydrophilic colloid layer, a compound of formula (I): R.sub.1 --NHNH--CHO (I) wherein R 1 represents an aliphatic group or an aromatic group, wherein the silver iodide content in the surface part of the silver halide grains is larger than the average silver iodide content thereof by 50% or more.
Claim 2
Dependent Claim
129 words
A negative silver halide photographic light-sensitive material having a silver halide emulsion layer, which layer comprises monodispersed cubic or tetradecahedral silver haloiodide grains prepared in the presence of an iridium salt in an amount of 1×10 -8 to 1×10 -5 mole per one mole of silver, wherein the silver iodide content in the surface part of said grain is larger than the average silver iodide content in said grain, and additionally containing in said emulsion layer or in some other hydrophilic colloid layer, a compound of formula (I): R.sub.1 --NHNH--CHO (I) wherein R 1 represents an aliphatic group or an aromatic group, wherein the silver iodide content in the surface part of the silver halide grains is larger than the average silver iodide content thereof by 50% or more.
Claim 3
Dependent Claim
25 words
The negative silver halide photographic light-sensitive material as claimed in claim 1, wherein said iridium salt is selected from water-soluble iridium salts and iridium complexes.
Claim 4
Dependent Claim
28 words
The negative silver halide photographic light-sensitive material as claimed in claim 2, wherein said iridium salt is iridium trichloride, iridium tetra-chloride, potassium hexachloro-iridate(III), potassium hexachloro-iridate(IV), or ammonium hexachloro-iridate(III).
Claim 5
Independent Claim
166 words
A method for formation of negative images of ultra-high contrast, characterized in that a negative silver halide photographic light-sensitive material having a silver halide emulsion layer, which layer comprises monodispersed cubic or tetradecahedral silver haloiodide grains prepared in the presence of an iridium salt in an amount of 1×10 -8 to 1×10 -5 mole per one mole of silver, wherein the silver iodide content in the surface part of said grain is larger than the average silver iodide content in said grain, and additionally containing in said emulsion layer or in some other hydrophilic colloid layer, a compound of a formula (I): R.sub.1 --NHNH--CHO (I) wherein R 1 represents an aliphatic group or an aromatic group, is exposed image-wise and then treated with a developer containing 0.15 mole/l or more sulfite ion and having a pH value of 9.5-12.3, wherein the silver iodide content in the surface part of the silver halide grains is larger than the average silver iodide content thereof by 50% or more.
Claim 6
Independent Claim
166 words
A method for formation of negative images of ultra-high contrast, characterized in that a negative silver halide photographic light-sensitive material having a silver halide emulsion layer, which layer comprises monodispersed cubic or tetradecahedral silver haloiodide grains prepared in the presence of an iridium salt in an amount of 1×10 -8 to 1×10 -5 mole per one mole of silver, wherein the silver iodide content in the surface part of said grain is larger than the average silver iodide content in said grain, and additionally containing in said emulsion layer or in some other hydrophilic colloid layer, a compound of a formula (I): R.sub.1 --NHNH--CHO (I) wherein R 1 represents an aliphatic group or an aromatic group, is exposed image-wise and then treated with a developer containing 0.15 mole/l or more sulfite ion and having a pH value of 9.5-12.3, wherein the silver iodide content in the surface part of the silver halide grains is larger than the average silver iodide content thereof by 50% or more.
Claim 7
Dependent Claim
26 words
The negative silver halide photographic light-sensitive material as claimed in claim 1, wherein said silver haloiodide grains have an average grain size of 0.7μ or less.
Claim 8
Dependent Claim
26 words
The negative silver halide photographic light-sensitive material as claimed in claim 1, wherein said silver haloiodide grains have an average grain size of 0.5μ or less.
Claim 9
Dependent Claim
21 words
A method as claimed in claim 4, wherein said silver haloiodide grains have an average grain size of 0.7μ or less.
Claim 10
Dependent Claim
21 words
A method as claimed in claim 4, wherein said silver haloiodide grains have an average grain size of 0.5μ or less.