Low methionine gelatino-peptizer tabular grain silver bromide and bromoiodide emulsions and processes for their preparation

Assignee: Eastman Kodak Co
•
Filing: 1987-02-17
•
Granted: 1987-12-15
•
Expires: 2007-02-17
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract The present invention is directed to a process of precipitating for use in photography a thin, tabular grain silver bromide or bromoiodide emulsion employing a gelatino-peptizer comprised of less than 30 micromoles of methionine per gram and to an emulsion produced by this process. A variety of advantages can be realized, including a wider range of permissible bromide ion concentrations during precipitation, thinner and/or larger diameter tabular grains, a reduced rod population, and novel tabular grain forms.

Inventors

  • 👤 Joe E. Maskasky

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-02 13:43
CPC Classifications
G; G03; G03C; G03C1/00; G03C1/005; G03C1/035; G03C1/0051; G03C1/04; G03C1/047

Claims Analysis

Total Claims: 20
Claim 1
Independent Claim 59 words
A process for the precipitation of a thin tabular grain emulsion comprising concurrently introducing into a reaction vessel silver, bromide, and, optionally, iodide ions to form tabular grains of less than 0.2 μm in thickness and maintaining the tabular grains in suspension with a gelatino-peptizer, characterized in that the gelatino-peptizer contains less than 30 micromoles of methionine per gram.
Claim 2
Dependent Claim 59 words
A process for the precipitation of a thin tabular grain emulsion comprising concurrently introducing into a reaction vessel silver, bromide, and, optionally, iodide ions to form tabular grains of less than 0.2 μm in thickness and maintaining the tabular grains in suspension with a gelatino-peptizer, characterized in that the gelatino-peptizer contains less than 30 micromoles of methionine per gram.
Claim 3
Dependent Claim 21 words
A process according to claim 1 further characterized in that the gelatino-peptizer contains less than 12 micromoles of methionine per gram.
Claim 4
Dependent Claim 21 words
A process according to claim 2 further characterized in that the gelatino-peptizer contains less than 5 micromoles of methionine per gram.
Claim 5
Dependent Claim 35 words
A process according to claim 1 further characterized in that the pBr within the reaction vessel is maintained in the range of from 1.6 to 2.4 at the time that tabular grains are being formed.
Claim 6
Dependent Claim 35 words
A process according to claim 4 further characterized in that the pBr within the reaction vessel is maintained in the range of from 1.6 to 2.2 at the time the tabular grains are being formed.
Claim 7
Dependent Claim 36 words
A process according to claim 1 further characterized in that the gelatino-peptizer is treated with an oxidizing agent to lower its methionine content prior to concurrent introduction into the reaction vessel of silver and bromide ions.
Claim 8
Dependent Claim 22 words
A process according to claim 6 further characterized in that the gelatino-peptizer is treated with hydrogen peroxide to lower its methionine content.
Claim 9
Dependent Claim 80 words
A process according to claim 1 further characterized in that a thin tabular grain silver bromide emulsion in which tabular silver bromide grains having a thickness of less than 0.2 μm and an aspect ratio of greater than 5:1 account for greater than 50 percent of the total grain projected area is prepared by concurrently introducing silver and bromide ions into the reaction vessel while maintaining the pBr within the reaction vessel in the range of from 1.1 to 2.0.
Claim 10
Dependent Claim 81 words
A process according to claim 1 further characterized in that a thin tabular grain silver bromoiodide emulsion in which tabular silver bromoiodide grains having a thickness of less than 0.2 μm and an aspect ratio of greater than 5:1 account for greater than 50 percent of the total grain projected area is prepared by concurrently introducing silver, bromide, and iodide ions into the reaction vessel while maintaining the pBr within the reaction vessel in the range of from 1.1 to 2.0.
Claim 11
Dependent Claim 55 words
A thin tabular grain emulsion comprising tabular silver bromide or bromoiodide grains having a thickness of less than 0.2 μm and an aspect ratio of greater than 5:1 accounting for greater than 50 percent of the total grain projected area of said emulsion and a gelatino-peptizer containing less than 30 micromoles of methionine per gram.
Claim 12
Dependent Claim 55 words
A thin tabular grain emulsion comprising tabular silver bromide or bromoiodide grains having a thickness of less than 0.2 μm and an aspect ratio of greater than 5:1 accounting for greater than 50 percent of the total grain projected area of said emulsion and a gelatino-peptizer containing less than 30 micromoles of methionine per gram.
Claim 13
Dependent Claim 22 words
A thin tabular grain emulsion according to claim 10 in which the gelatino-peptizer contains less than 12 micromoles of methionine per gram.
Claim 14
Dependent Claim 22 words
A thin tabular grain emulsion according to claim 10 in which the gelatino-peptizer contains less than 5 micromoles of methionine per gram.
Claim 15
Dependent Claim 29 words
A thin tabular grain emulsion according to claim 10 in which at least 2 percent of the total grain projected area is accounted for by thin tabular trapezoidal grains.
Claim 16
Dependent Claim 29 words
A thin tabular grain emulsion according to claim 13 in which at least 50 percent of the total grain projected area is accounted for by thin tabular trapezoidal grains.
Claim 17
Dependent Claim 43 words
A thin tabular grain emulsion according to claim 10 in which tabular silver bromide grains having a thickness of less than 0.2 μm and an aspect ratio of greater than 8:1 account for greater than 70 percent of the total grain projected area.
Claim 18
Dependent Claim 50 words
A thin tabular grain emulsion according to claim 10 in which said gelatino-peptizer consists essentially of gelatin and tabular silver bromide grains having a thickness of less than 0.2 μm and an aspect ratio of greater than 20:1 account for greater than 90 percent of the total grain projected area.
Claim 19
Dependent Claim 43 words
A thin tabular grain emulsion according to claim 10 in which tabular silver bromoiodide grains having a thickness of less than 0.2 μm and an aspect ratio of greater than 8:1 account for greater than 70 percent of the total grain projected area.
Claim 20
Dependent Claim 50 words
A thin tabular grain emulsion according to claim 10 in which said gelatino-peptizer consists essentially of gelatin and tabular silver bromoiodide grains having a thickness of less than 0.2 μm and an aspect ratio of greater than 20:1 account for greater than 90 percent of the total grain projected area.

References Cited (Backward Citations)

GB245456A Cited
US2890215A Cited
JPS5870221A Cited
US4434226A Cited
JPS59195232A Cited
US4520098A Cited
EP1449902A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-12-14 1991-06-15 1991-12-15 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-12-14 1995-06-15 1995-12-15 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-12-14 1999-06-15 1999-12-15 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag