Abstract

Abstract A reflecting mirror for use as a rearview mirror in an automobile, the mirror having a plurality of thin layers arranged on a glass plate. One of the layers is made of a transparent dielectric material having a refractive index which is not less than a refractive index of WO 2 and the other is made of a metal material having a reflecting factor ranging between 50-70%. The light introduced into the mirror is reflected at different borders formed in the mirror between the layers so as to provide lights of different phases. Therefore, there is an interference, and, consequently, the mirror provides a certain selected tone in accordance with the value of the optical thickness of the transparent dielectric layer, resulting in an anti-glare effect and a deep color.

Inventors

  • 👤 Takasi Taguchi
  • 👤 Yoshiki Ueno
  • 👤 Tadashi Hattori

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-28 15:14
CPC Classifications
G; G02; G02B; G02B5/00; G02B5/08; G02B5/0816; G02B5/085; G02B5/0858; B; B60; B60R; B60R1/00; B60R1/02; B60R1/08; B60R1/083; G02B5/0883

Claims Analysis

Total Claims: 9
Claim 1
Independent Claim 158 words
A reflecting colored mirror for an automobile having anti-glare effects comprising: an opaque thin metal layer having a reflecting factor ranging from 50% to 70%, said metal layer defining a first light reflecting surface; and a thin layer made of a transparent dielectric material, said dielectric layer being formed on said surface of said thin metal layer, said dielectric layer forming a second light-reflecting surface on a surface of said dielectric layer opposite said first light-reflecting surface of said thin metal layer, the thickness of said dielectric layer being sufficiently thin to allow the surface of said dielectric layer to have negligible roughness resulting in good interference for selected frequencies of visible light, said thickness, taken into consideration with said metal layer reflecting factor and said dielectric layer refractive index, causing a required interference effect by light reflected from said first and second light-reflecting surface so that the reflecting factor of said mirror is from 38% to 65%.
Claim 2
Dependent Claim 158 words
A reflecting colored mirror for an automobile having anti-glare effects comprising: an opaque thin metal layer having a reflecting factor ranging from 50% to 70%, said metal layer defining a first light reflecting surface; and a thin layer made of a transparent dielectric material, said dielectric layer being formed on said surface of said thin metal layer, said dielectric layer forming a second light-reflecting surface on a surface of said dielectric layer opposite said first light-reflecting surface of said thin metal layer, the thickness of said dielectric layer being sufficiently thin to allow the surface of said dielectric layer to have negligible roughness resulting in good interference for selected frequencies of visible light, said thickness, taken into consideration with said metal layer reflecting factor and said dielectric layer refractive index, causing a required interference effect by light reflected from said first and second light-reflecting surface so that the reflecting factor of said mirror is from 38% to 65%.
Claim 3
Dependent Claim 27 words
A reflecting mirror according to claim 1, wherein said transparent dielectric material is one of WO 2 , ZrO 2 , CeO 2 and TiO 2 .
Claim 4
Dependent Claim 23 words
A reflecting mirror according to claim 2, wherein said transparent dielectric material is TiO 2 , and said metal layer is nickel-chrome alloy.
Claim 5
Dependent Claim 39 words
A reflecting mirror according to claim 1, further comprising a substratum layer having a surface, said thin metal layer and said dielectric layer being formed on said surface of said substratum layer by one of vacuum deposition and sputtering.
Claim 6
Dependent Claim 29 words
A reflecting mirror according to claim 1, further comprising a transparent substratum layer having a surface, and said dielectric layer being formed on said surface of said substratum layer.
Claim 7
Dependent Claim 218 words
A reflecting colored mirror for an automobile having an anti-glare characteristic comprising: a glass layer having a surface; a auxiliary dielectric layer having a reflective index lower than the reflective index of said glass layer and disposed on said surface of said glass layer; a auxiliary dielectric layer having a refractive index lower than the refractive index of said glass layer and disposed on said surface of said glass layer; a main dielectric layer having a refractive index which is greater than said glass layer and being disposed on said auxiliary dielectric layer, said main dielectric layer and said auxiliary dielectric layer defining a first light-reflecting boundary; and an opaque thin metal layer having a reflecting factor of from 50% to 70%, being formed on said main dielectric layer, said metal layer and said main dielectric layer defining a second light-reflecting boundary, the thickness of said main dielectric layer being sufficiently thin to allow the surface of said main dielectric layer to have negligible roughness resulting in good interference for selected frequencies of visible light, said thickness, taken into consideration with said metal layer reflecting factor and said main dielectric layer refractive index, causing a required interference effect by light reflected from said first and second light-reflecting boundaries so that the reflecting factor is from 38% to 65%.
Claim 8
Dependent Claim 218 words
A reflecting colored mirror for an automobile having an anti-glare characteristic comprising: a glass layer having a surface; a auxiliary dielectric layer having a reflective index lower than the reflective index of said glass layer and disposed on said surface of said glass layer; a auxiliary dielectric layer having a refractive index lower than the refractive index of said glass layer and disposed on said surface of said glass layer; a main dielectric layer having a refractive index which is greater than said glass layer and being disposed on said auxiliary dielectric layer, said main dielectric layer and said auxiliary dielectric layer defining a first light-reflecting boundary; and an opaque thin metal layer having a reflecting factor of from 50% to 70%, being formed on said main dielectric layer, said metal layer and said main dielectric layer defining a second light-reflecting boundary, the thickness of said main dielectric layer being sufficiently thin to allow the surface of said main dielectric layer to have negligible roughness resulting in good interference for selected frequencies of visible light, said thickness, taken into consideration with said metal layer reflecting factor and said main dielectric layer refractive index, causing a required interference effect by light reflected from said first and second light-reflecting boundaries so that the reflecting factor is from 38% to 65%.
Claim 9
Dependent Claim 45 words
A reflecting mirror according to claim 6 wherein said transparent main dielectric material is one of WO 2 , ZrO 2 , CeO 2 , and TiO 2 , and said auxiliary dielectric material is one of LiF, MgF 2 , and SiO 2 .

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-06-15 1990-12-15 1991-06-16 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-06-15 1994-12-15 1995-06-16 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-06-15 1998-12-15 1999-06-16 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag