← Back to Patent Explorer
US2772190A Expired / Lapsed US ⏱️ 0.0 years remaining

Method of increasing the electrical conductivity of tin oxide films

Assignee: Hartford National Bank and Trust Co
•
Filing: 1952-09-25
•
Granted: 1956-11-27
•
Expires: 1972-09-25
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

No abstract record available.

Inventors

  • 👤 Haayman Pieter Willem
  • 👤 Veeneman Dirk
  • 👤 Janssen Gerardus Hendricus

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-07 23:57
CPC Classifications
H; H01; H01C; H01C7/00; H01C7/006; C; C03; C03C; C03C17/00; C03C17/22; C03C17/23; C03C17/25; C03C17/253; H01B; H01B1/00; H01B1/06; H01B1/08; C03C2217/00; C03C2217/20; C03C2217/21; C03C2217/211; C03C2217/24; C03C2218/00; C03C2218/10; C03C2218/11; C03C2218/112

Claims Analysis

Total Claims: 2
Claim 1
Independent Claim 108 words
IN A METHOD OF PRODUCING TRANSPARENT ELECTRICALLY CONDUCTING FILMS CONSISTING SUBSTANTIALLY OF TIN OXIDE BY APPLYING A FILMING MATERIAL IN FLUID FORM AND WHICH COMPRISES AN ELECTRICALLY-CONDUCTING FILM-FORMING COMPOUND OF TIN TO A HOT VITREOUS SURFACE, HEATED TO A TEMPERATURE OF AT LEAST 300* C.; THE STEP OF INCREASING THE ELECTRICAL CONDUCTIVITY OF SUCH FILMS WHICH COMPRISES ADDING TO SAID FILMING MATERIAL, BY PUTTING INTO SOLUTION THEREWITH, AN AMOUNT OF A COMPOUND OF PHOSPHORUS TO YIELD AN AMOUNT OF PHOSPHORUS NOT LESS THAN ABOUT 0.033% TO NOT MORE THAN ABOUT 12.4% BY WEIGHT OF THE TIN IN SAID FILMING MATERIAL, BEFORE APPLYING SAID FILMING MATERIAL TO SAID SURFACE.
Claim 2
Dependent Claim 108 words
IN A METHOD OF PRODUCING TRANSPARENT ELECTRICALLY CONDUCTING FILMS CONSISTING SUBSTANTIALLY OF TIN OXIDE BY APPLYING A FILMING MATERIAL IN FLUID FORM AND WHICH COMPRISES AN ELECTRICALLY-CONDUCTING FILM-FORMING COMPOUND OF TIN TO A HOT VITREOUS SURFACE, HEATED TO A TEMPERATURE OF AT LEAST 300* C.; THE STEP OF INCREASING THE ELECTRICAL CONDUCTIVITY OF SUCH FILMS WHICH COMPRISES ADDING TO SAID FILMING MATERIAL, BY PUTTING INTO SOLUTION THEREWITH, AN AMOUNT OF A COMPOUND OF PHOSPHORUS TO YIELD AN AMOUNT OF PHOSPHORUS NOT LESS THAN ABOUT 0.033% TO NOT MORE THAN ABOUT 12.4% BY WEIGHT OF THE TIN IN SAID FILMING MATERIAL, BEFORE APPLYING SAID FILMING MATERIAL TO SAID SURFACE.

References Cited (Backward Citations)

US2490825A Cited
US2564706A Cited
US2692836A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1959-11-27 1960-05-28 1960-11-27 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1963-11-27 1964-05-28 1964-11-27 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1967-11-27 1968-05-28 1968-11-27 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag