Patent US4668733A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4668733A Expired / Lapsed US ⏱️ 0.0 years remaining

Pour point depressants comprising polyolefins modified with side chains

Assignee: Henkel AG and Co KGaA
•
Filing: 1986-03-27
•
Granted: 1987-05-26
•
Expires: 2006-03-27
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A pour point depressant composition and a method for its use. The pour point depressant is a predominantly butadiene polymer epoxidized and then ring-opened with a C12-24 carboxylic acid, or ring-opened with an alcohol followed by esterification.

Inventors

  • 👤 Hermann Anzinger
  • 👤 Herbert Fischer
  • 👤 Claus-Peter Herold
  • 👤 Wolfgang Zoellner

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-29 12:44
CPC Classifications
C; C08; C08C; C08C19/00; C08C19/30; C08C19/34; C08C19/40; C08G; C08G59/00; C08G59/14; C08G59/1433; C08G59/1438

Claims Analysis

Total Claims: 29
Claim 1
Independent Claim 158 words
A modified polyolefin having saturated and predominantly unbranched alkyl side chains and a hydroxyl number below 25 mg KOH/g, whose backbone is a polyolefin containing at least 50% by weight butadiene and which is modified by epoxidation of the polyolefin ethylenic double bonds to an epoxide oxygen content of from about 1% to 8% by weight, followed by ring opening of the epoxide groups by reaction with: (a) at least one first saturated C 12-24 -carboxylic acid or a mixture of the first saturated C 12-24 -carboxylic acid with from 0-30 mol percent of at least one C 4-12 -monocarboxylic straight, brancid; oraromatic acid; or (b) at least one alcohol selected from (i) at least one saturated primary C 12-24 -alcohol; or (ii) at least one C 2-12 -polyol having 2 to 6 hydroxyl moieties; followed by esterification of any remaining hydroxyl moieties with at least one second saturated C 12-24 -carboxylic acid, to form said modified polyolefin.
Claim 2
Dependent Claim 158 words
A modified polyolefin having saturated and predominantly unbranched alkyl side chains and a hydroxyl number below 25 mg KOH/g, whose backbone is a polyolefin containing at least 50% by weight butadiene and which is modified by epoxidation of the polyolefin ethylenic double bonds to an epoxide oxygen content of from about 1% to 8% by weight, followed by ring opening of the epoxide groups by reaction with: (a) at least one first saturated C 12-24 -carboxylic acid or a mixture of the first saturated C 12-24 -carboxylic acid with from 0-30 mol percent of at least one C 4-12 -monocarboxylic straight, brancid; oraromatic acid; or (b) at least one alcohol selected from (i) at least one saturated primary C 12-24 -alcohol; or (ii) at least one C 2-12 -polyol having 2 to 6 hydroxyl moieties; followed by esterification of any remaining hydroxyl moieties with at least one second saturated C 12-24 -carboxylic acid, to form said modified polyolefin.
Claim 3
Dependent Claim 23 words
The composition of claim 1 wherein said polyolefin backbone is a homopolymer of butadiene or a copolymer of butadiene with styrene and/or acrylonitrile.
Claim 4
Dependent Claim 22 words
The composition of claim 1 wherein said butadiene is 1,4-polybutadiene containing more than 20% of its ethylenic bonds in a cis configuration.
Claim 5
Dependent Claim 22 words
The composition of claim 1 wherein said butadiene is 1,4-polybutadiene containing more than 70% of its ethylenic bonds in a cis configuration.
Claim 6
Dependent Claim 22 words
The composition of claim 1 wherein said butadiene is 1,4-polybutadiene containing more than 20% of its ethylenic bonds in a trans configuration.
Claim 7
Dependent Claim 22 words
The composition of claim 1 wherein said butadiene is 1,4-polybutadiene containing more than 50% of its ethylenic bonds in a trans configuration.
Claim 8
Dependent Claim 18 words
The composition of claim 1 wherein said polyolefin is 1,2-polybutadiene containing from 20 to 98% lateral ethylenic bonds.
Claim 9
Dependent Claim 25 words
The composition of claim 1 wherein, after epoxidation but before ring opening, said polyolefin has a number average molecular weight of about 500 to 10,000.
Claim 10
Dependent Claim 25 words
The composition of claim 1 wherein, after epoxidation but before ring opening, said polyolefin has a number average molecular weight of about 1,000 to 2,000.
Claim 11
Dependent Claim 20 words
The composition of claim 8 wherein said polyolefin has an epoxide oxygen content of about 2 to 6% by weight.
Claim 12
Dependent Claim 20 words
The composition of claim 8 wherein said polyolefin has an epoxide oxygen content of about 3 to 5% by weight.
Claim 13
Dependent Claim 29 words
The composition of claim 1 wherein said first and said second saturated C 12-24 carboxylic acid are each at least one fatty acid having an iodine number below 50.
Claim 14
Dependent Claim 12 words
The composition of claim 12 wherein said iodine number is below 10.
Claim 15
Dependent Claim 21 words
The composition of claim 13 wherein each said at least one fatty acid is a mixture of C 16-22 fatty acids.
Claim 16
Dependent Claim 35 words
The composition of claim 1 wherein said first and said second at least one saturated C 12-24 carboxylic acid are each a hydrogenated fatty acid mixture derived from vegetable oil, land-animal oil, and/or marine-animal oil.
Claim 17
Dependent Claim 35 words
The composition of claim 1 wherein said first and said second at least one saturated C 12-24 carboxylic acid are each a hydrogenated tallow fatty acid, hydrogenated rapeseed oil fatty acid, or any mixture thereof.
Claim 18
Dependent Claim 29 words
The composition of claim 1 wherein said ring-opening is effected by reaction with (b) and wherein said alkyl side chains are derived from at least one C 18-22 alcohol.
Claim 19
Dependent Claim 30 words
The composition of claim 1 wherein said ring-opening is effected by reaction with (b) and wherein said alkyl side chains are derived from stearyl alcohol, behenyl alcohol, or their mixture.
Claim 20
Dependent Claim 29 words
The composition of claim 16 wherein said ring-opening is effected by reaction with (b) and wherein said alkyl side chains are derived from at least one C 18-22 alcohol.
Claim 21
Dependent Claim 31 words
The composition of claim 1 wherein said ring-opening is effected by reaction with (b)(ii) and wherein said C 2-12 polyol contains up to 3 ether oxygen atoms as said hydroxyl moieties.
Claim 22
Dependent Claim 31 words
The composition of claim 16 wherein said ring-opening is effected by reaction with (b)(ii) and wherein said C 2-12 polyol contains up to 3 ether oxygen atoms as said hydroxyl moieties.
Claim 23
Dependent Claim 43 words
The composition of claim 1 wherein said ring-opening is effected by reaction with (b)(ii) and wherein said C 2-12 polyol is: ethylene glycol; propylene glycol; neopentyl glycol; diethylene glycol; glycerol; trimethylol ethane; trimethylol propane; pentaerythritol; ditrimethylol ethane, ditrimethylol propane, or any mixture thereof.
Claim 24
Dependent Claim 43 words
The composition of claim 16 wherein said ring-opening is effected by reaction with (b)(ii) and wherein said C 2-12 polyol is: ethylene glycol; propylene glycol; neopentyl glycol; diethylene glycol; glycerol; trimethylol ethane; trimethylol propane; pentaerythritol; ditrimethylol ethane, ditrimethylol propane, or any mixture thereof.
Claim 25
Dependent Claim 20 words
The composition of claim 1 wherein said polyolefin has a total number average molecular weight of about 1,500 to 10,000.
Claim 26
Dependent Claim 20 words
The composition of claim 1 wherein said polyolefin has a total number average molecular weight of about 2,500 to 7,000.
Claim 27
Dependent Claim 174 words
A pour point depressant composition comprising a carrier liquid and a pour point depressant consisting essentially of a pour point depressant effective amount of a modified polyolefin having saturated and predominantly unbranched alkyl side chains and a hydroxyl number below 25 mg KOH/g, whose backbone is a polyolefin containing at least 50% by weight butadiene which is modified by epoxidation of the polyolefin ethylenic double bonds to a epoxide oxygen content of from about 1% to 8% by weight, followed by ring-opening of the epoxide groups by reaction with: (a) at least one first saturated C 12-24 -carboxylic acid, or a mixture of the C 12-24 -carboxylic acid with from 0-30 mol percent of a least one C 4-12 -monocarboxylic straight, branched, or aromatic acid; or (b) at least one alcohol selected from (i) at least one saturated primary C 12-24 -alcohol; or (ii) at least one C 2-12 -polyol having 2 to 6 hydroxyl moieties; followed by esterification of any remaining hydroxyl moieties with at least one second saturated C 12-24 -carboxylic acid.
Claim 28
Dependent Claim 174 words
A pour point depressant composition comprising a carrier liquid and a pour point depressant consisting essentially of a pour point depressant effective amount of a modified polyolefin having saturated and predominantly unbranched alkyl side chains and a hydroxyl number below 25 mg KOH/g, whose backbone is a polyolefin containing at least 50% by weight butadiene which is modified by epoxidation of the polyolefin ethylenic double bonds to a epoxide oxygen content of from about 1% to 8% by weight, followed by ring-opening of the epoxide groups by reaction with: (a) at least one first saturated C 12-24 -carboxylic acid, or a mixture of the C 12-24 -carboxylic acid with from 0-30 mol percent of a least one C 4-12 -monocarboxylic straight, branched, or aromatic acid; or (b) at least one alcohol selected from (i) at least one saturated primary C 12-24 -alcohol; or (ii) at least one C 2-12 -polyol having 2 to 6 hydroxyl moieties; followed by esterification of any remaining hydroxyl moieties with at least one second saturated C 12-24 -carboxylic acid.
Claim 29
Dependent Claim 21 words
The composition of claim 26 wherein said carrier liquid is a high boiling, apolar, hydrocarbon solvent for said pour point depressant.

References Cited (Backward Citations)

US2692892A Cited
GB799719A Cited
US3397164A Cited
US3904385A Cited
US3951929A Cited
US4083834A Cited
JPS5138756A Cited
GB2125805A Cited
US4528340A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1990-05-25 1990-11-24 1991-05-26 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1994-05-25 1994-11-24 1995-05-26 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1998-05-25 1998-11-24 1999-05-26 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag