Claims Analysis
Total Claims: 13
Claim 1
Independent Claim
76 words
A tracer unit for ammunition comprising (a) a base charge including about 75 to about 90 weight % strontium peroxide, about 5 to about 15 weight % calcium resinate and about 5 to about 10 weight % magnesium; and (b) an igniter charge covering said base charge and including about 40 to about 60 weight % calcium resinate, about 20 to about 30 weight % stontium nitrate and about 20 to about 30 weight % magnesium.
Claim 2
Dependent Claim
76 words
A tracer unit for ammunition comprising (a) a base charge including about 75 to about 90 weight % strontium peroxide, about 5 to about 15 weight % calcium resinate and about 5 to about 10 weight % magnesium; and (b) an igniter charge covering said base charge and including about 40 to about 60 weight % calcium resinate, about 20 to about 30 weight % stontium nitrate and about 20 to about 30 weight % magnesium.
Claim 3
Dependent Claim
25 words
A tracer composition according to claim 1 wherein the weight ratio of said igniter charge to said base charge is about 1:4 to about 1:20.
Claim 4
Dependent Claim
30 words
A tracer unit according to claim 1 wherein said base charge includes about 85 weight % strontium peroxide, about 9 weight % calcium resinate and about 6 weight % magnesium.
Claim 5
Dependent Claim
30 words
A tracer unit according to claim 1 wherein said igniter charge includes about 50 weight % calcium resinate, about 25 weight % strontium nitrate, and about 25 weight % magnesium.
Claim 6
Dependent Claim
22 words
A tracer unit according to claim 2 wherein the weight ratio of said igniter charge to said base charge is about 1:9.
Claim 7
Independent Claim
209 words
A method for producing ammunition having a tracer unit including a base charge and an igniter charge for igniting the base charge when the weapon is fired, said method including the steps of: (a) admixing a base charge including about 75 to about 90 weight % strontium peroxide, about 5 to about 15 weight % calcium resinate and about 5 to about 10 % magnesium with an anhydrous solvent to form a damp substantially homogenous mixture thereof: (b) admixing an igniter charge including about 40 to 60 weight % calcium resinate, about 20 to about 30 weight % strontium nitrate and about 20 to about 30 weight % magnesium with an anhydrous solvent to form a substantially homogenous mixture thereof; (c) partially filling a small cavity in the rear end of the ammunition projectile with a sufficient amount of the damp base charge mixture to illuminate the trajectory of the projectile for a desired distance when the weapon is fired; (d) tamping the damp base charge mixture into the projectile cavity by the application of a low pressure; and (e) adding to the projectile cavity a sufficient amount of the igniter charge mixture to cover the base charge and to ignite the base charge when the weapon is fired.
Claim 8
Independent Claim
209 words
A method for producing ammunition having a tracer unit including a base charge and an igniter charge for igniting the base charge when the weapon is fired, said method including the steps of: (a) admixing a base charge including about 75 to about 90 weight % strontium peroxide, about 5 to about 15 weight % calcium resinate and about 5 to about 10 % magnesium with an anhydrous solvent to form a damp substantially homogenous mixture thereof: (b) admixing an igniter charge including about 40 to 60 weight % calcium resinate, about 20 to about 30 weight % strontium nitrate and about 20 to about 30 weight % magnesium with an anhydrous solvent to form a substantially homogenous mixture thereof; (c) partially filling a small cavity in the rear end of the ammunition projectile with a sufficient amount of the damp base charge mixture to illuminate the trajectory of the projectile for a desired distance when the weapon is fired; (d) tamping the damp base charge mixture into the projectile cavity by the application of a low pressure; and (e) adding to the projectile cavity a sufficient amount of the igniter charge mixture to cover the base charge and to ignite the base charge when the weapon is fired.
Claim 9
Dependent Claim
34 words
A method according to claim 6 including the further steps of: (f) drying the base and igniter charges; and (g) covering the exposed surfaces of the igniter charge with a compatible moisture proofing material.
Claim 10
Dependent Claim
28 words
A method according to claim 7 wherein the base charge includes about 85 weight % strontium peroxide, about 90 % calcium resinate and about 6 weight % magnesium.
Claim 11
Dependent Claim
27 words
A method according to claim 8 wherein the igniter charge includes about 50 weight % calcium resinate, about 25% strontium nitrate and about 25 weight % magnesium.
Claim 12
Dependent Claim
24 words
A method according to claim 6 wherein the weight ratio of the igniter charge to the base charge is about 1:4 to about 1:20.
Claim 13
Dependent Claim
49 words
A method according to claim 6 wherein a sufficient amount of the solvent is added to and mixed with the igniter charge to form the resulting mixture into a creamy-like consistency; and step (e) includes filling the unfilled portion of the projectile cavity with the creamy-like igniter charge mixture.