Process for the production of aqueous dispersions and use thereof for the production of metal effect lacquer coatings

Assignee: Bayer AG
•
Filing: 1985-02-28
•
Granted: 1986-06-10
•
Expires: 2005-02-28
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Aqueous dispersions based on selected polyesters and/or acrylate resins, water-soluble aminoplast resins, emulsifiers, aluminium bronze, organic solvents and optionally further auxiliaries are suitable for the production of metal effect lacquer coatings by the two-layer wet-in-wet lacquering process.

Inventors

  • 👤 Hans-Georg Stahl
  • 👤 Jurgen Schwindt
  • 👤 Klaus Nachtkamp

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-27 12:27
CPC Classifications
B; B05; B05D; B05D7/00; B05D7/50; B05D7/52; B05D7/53; B05D7/532; B05D5/00; B05D5/06; B05D5/067; B05D5/068; C; C09; C09D; C09D133/00; C09D133/04; C09D133/06; C09D167/00; C09D5/00; C09D5/38; C08; C08L; C08L61/00; C08L61/20

Claims Analysis

Total Claims: 3
Claim 1
Independent Claim 175 words
Process for the production of an aqueous metal effect-base lacquer based on: (A) from 10 to 30 parts, by weight, oil-free polyester or alkyd resin having an average functionality per molecule of from 2.5 to 10, an average degree of condensation per molecule of from 10 to 25, an average urethane group content per molecule of from 3 to 6, and containing moietites of condensed 2,2-di(hydroxymethyl)carboxylic acids, hydroxypivalic acid, or both, corresponding to an acid number of from 15 to 30, up to at least 80% of which are neutralized; (B) from 2.5 to 15 parts, by weight, water-soluble aminoplast resin; (C) from 2 to 10 parts, by weight, aluminum bronze; (D) from 0.1 to 10 parts, by weight, non-ionic emulsifier; and (E) organic solvent; characterized in that a resin having a maximum acid number of 30 and a maximum hydroxyl number of 150 is used as component (A) and this is mixed with the other components in the form of an aqueous dispersion having a solids content of from 30 to 50%, by weight.
Claim 2
Dependent Claim 175 words
Process for the production of an aqueous metal effect-base lacquer based on: (A) from 10 to 30 parts, by weight, oil-free polyester or alkyd resin having an average functionality per molecule of from 2.5 to 10, an average degree of condensation per molecule of from 10 to 25, an average urethane group content per molecule of from 3 to 6, and containing moietites of condensed 2,2-di(hydroxymethyl)carboxylic acids, hydroxypivalic acid, or both, corresponding to an acid number of from 15 to 30, up to at least 80% of which are neutralized; (B) from 2.5 to 15 parts, by weight, water-soluble aminoplast resin; (C) from 2 to 10 parts, by weight, aluminum bronze; (D) from 0.1 to 10 parts, by weight, non-ionic emulsifier; and (E) organic solvent; characterized in that a resin having a maximum acid number of 30 and a maximum hydroxyl number of 150 is used as component (A) and this is mixed with the other components in the form of an aqueous dispersion having a solids content of from 30 to 50%, by weight.
Claim 3
Dependent Claim 19 words
The dispersions produced by the process according to claim 1 for the production of metal effect two-layer lacquer coatings.

References Cited (Backward Citations)

US4115338A Cited
US4102691A Cited
US4156667A Cited
US4265929A Cited
US4323600A Cited
EP0038127B1 Cited
US4459379A Cited
EP0069936A2 Cited
US4510275A Cited
US4436849A Cited
US4518724A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1989-06-09 1989-12-09 1990-06-10 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1993-06-09 1993-12-09 1994-06-10 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1997-06-09 1997-12-09 1998-06-10 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag