Claims Analysis
Total Claims: 11
Claim 1
Independent Claim
355 words
A process for the recovery of a blend of solvents in a spray coating system and for reintroducing the recovered blend of solvents back into the spray coating system, said system including a chamber for spray coating of workpieces, a coating supply system for supplying coating material containing hydrocarbon solvent blends to said chamber, an exhaust system for removing coating material overspray from the chamber including a water scrubber to remove airborne coating material particles, and a system for recovering coating material from the chamber and returning it to said coating supply system, said process comprising the steps of: (a) extracting a stream containing a mixture of air, water vapor and hydrocarbon solvent vapors from said exhaust system at a rate of about 500 to 50,000 standard cubic feet per minute; (b) subjecting said stream to an absorption process which employs a hydrophobic absorption medium to absorb all but about 200 ppm of said blend of solvent vapors in said stream while the air and water vapor contained in said stream passes through said absorption process; (c) separating said blend of solvent vapors from said hydrophobic absorption medium by stripping said solvent vapors therefrom with a dry inert gas; (d) returning the hydrophobic absorption medium to said absorption process, said medium now containing less than about 0.001 mole fraction of any one solvent; (e) recovering said blend of solvent vapors substantially free of water and said hydrophobic absorption medium; and (f) returning said recovered blend of solvents to said spray coating system (1) by introducing said recovered blend of solvent vapors into said chamber to increase the solvent humidity in said chamber to thereby retard the evaporation of solvent from said coating material supplied to said chamber, (2) by condensing said recovered blend of solvent vapors recovered in step (e) and introducing the condensed blend of solvents to said system as a liquid to return solvent lost in the coating process to the coating supply system, or (3) by a combination of steps (1) and (2), said blend of solvents being returned in substantially the same proportion as in the stream extracted in step (a).
Claim 2
Dependent Claim
355 words
A process for the recovery of a blend of solvents in a spray coating system and for reintroducing the recovered blend of solvents back into the spray coating system, said system including a chamber for spray coating of workpieces, a coating supply system for supplying coating material containing hydrocarbon solvent blends to said chamber, an exhaust system for removing coating material overspray from the chamber including a water scrubber to remove airborne coating material particles, and a system for recovering coating material from the chamber and returning it to said coating supply system, said process comprising the steps of: (a) extracting a stream containing a mixture of air, water vapor and hydrocarbon solvent vapors from said exhaust system at a rate of about 500 to 50,000 standard cubic feet per minute; (b) subjecting said stream to an absorption process which employs a hydrophobic absorption medium to absorb all but about 200 ppm of said blend of solvent vapors in said stream while the air and water vapor contained in said stream passes through said absorption process; (c) separating said blend of solvent vapors from said hydrophobic absorption medium by stripping said solvent vapors therefrom with a dry inert gas; (d) returning the hydrophobic absorption medium to said absorption process, said medium now containing less than about 0.001 mole fraction of any one solvent; (e) recovering said blend of solvent vapors substantially free of water and said hydrophobic absorption medium; and (f) returning said recovered blend of solvents to said spray coating system (1) by introducing said recovered blend of solvent vapors into said chamber to increase the solvent humidity in said chamber to thereby retard the evaporation of solvent from said coating material supplied to said chamber, (2) by condensing said recovered blend of solvent vapors recovered in step (e) and introducing the condensed blend of solvents to said system as a liquid to return solvent lost in the coating process to the coating supply system, or (3) by a combination of steps (1) and (2), said blend of solvents being returned in substantially the same proportion as in the stream extracted in step (a).
Claim 3
Dependent Claim
44 words
The process as claimed in claim 1 wherein said hydrophobic absorption medium comprises oil having a viscosity of less than about 10 cp at 87° F., a molecular weight of less than about 250, and a boiling point of greater than about 500° F.
Claim 4
Dependent Claim
21 words
The process of claim 1 wherein said stream extracted in step (a) is at least about 90% saturated with water vapor.
Claim 5
Dependent Claim
15 words
The process of claim 1 wherein said hydrophobic absorption medium is hydrogenated white mineral oil.
Claim 6
Dependent Claim
17 words
The process of claim 1 wherein said process is carried out between one to ten atmospheres pressure.
Claim 7
Dependent Claim
41 words
The process of claim 1 wherein a sufficient amount of said recovered blend of solvents is introduced into said chamber to raise the solvent humidity in the area where the workpiece is being coated to at least about 80% of saturation.
Claim 8
Dependent Claim
13 words
The process of claim 1 wherein said workpiece moves continuously through said system.
Claim 9
Dependent Claim
425 words
A process for the recovery of a blend of solvents in a spray coating system and for reintroducing the recovered blend of solvents back into the spray coating system, said system including a chamber for spray coating of a moving line of workpieces into and out of the coater, a coating supply system for supplying coating material containing hydrocarbon solvent blends to said chamber, an exhaust system for removing coating material overspray from the chamber including a water scrubber to remove airborne coating material particles, and a system for recovering coating material from the chamber and returning it to the coating supply system, said process comprising the steps of: (a) extracting a stream containing a mixture of air, water vapor in an amount of at least about 90% of saturation, and hydrocarbon solvent vapors from said exhaust system at a rate of about 500 to 50,000 standard cubic feet per minute; (b) subjecting said stream to an absorption process operated at about atmospheric pressure at about 85° F. which employs white mineral oil to absorb all but about 200 ppm of said blend of solvent vapors in said stream thereby forming an oil-solvent mixture while the air and water vapor contained in the stream passes through said process and is vented out of said process; (c) heating the oil-solvent mixture to a temperature of about 300° F.; (d) passing an upwardly flowing dry gas stream through a downwardly flowing stream of the oil-solvent mixture to separate said blend of solvents from said oil by stripping said solvents out of said oil; (e) cooling the oil to a temperature of about 85° F. and returning the oil to said absorption process, said oil containing less than about 0.001 mole fraction of any one solvent; (f) recovering said blend of solvent vapors stripped from said oil substantially free of water and oil; (g) returning said recovered blend of solvents to said spray coating system (1) by introducing said recovered blend of solvent vapors into said chamber to increase the solvent humidity in said chamber to thereby retard the evaporation of solvents from said coating material supplied to said chamber, (2) by condensing said recovered blend of solvent vapors recovered at step (f) and introducing the condensed blend of solvents to said system as a liquid to return solvent lost in the coating process to the coating supply system, or (3) by a combination of steps (1) and (2), said blend of solvents being returned in substantially the same proportion as in the stream extracted in step (a).
Claim 10
Dependent Claim
425 words
A process for the recovery of a blend of solvents in a spray coating system and for reintroducing the recovered blend of solvents back into the spray coating system, said system including a chamber for spray coating of a moving line of workpieces into and out of the coater, a coating supply system for supplying coating material containing hydrocarbon solvent blends to said chamber, an exhaust system for removing coating material overspray from the chamber including a water scrubber to remove airborne coating material particles, and a system for recovering coating material from the chamber and returning it to the coating supply system, said process comprising the steps of: (a) extracting a stream containing a mixture of air, water vapor in an amount of at least about 90% of saturation, and hydrocarbon solvent vapors from said exhaust system at a rate of about 500 to 50,000 standard cubic feet per minute; (b) subjecting said stream to an absorption process operated at about atmospheric pressure at about 85° F. which employs white mineral oil to absorb all but about 200 ppm of said blend of solvent vapors in said stream thereby forming an oil-solvent mixture while the air and water vapor contained in the stream passes through said process and is vented out of said process; (c) heating the oil-solvent mixture to a temperature of about 300° F.; (d) passing an upwardly flowing dry gas stream through a downwardly flowing stream of the oil-solvent mixture to separate said blend of solvents from said oil by stripping said solvents out of said oil; (e) cooling the oil to a temperature of about 85° F. and returning the oil to said absorption process, said oil containing less than about 0.001 mole fraction of any one solvent; (f) recovering said blend of solvent vapors stripped from said oil substantially free of water and oil; (g) returning said recovered blend of solvents to said spray coating system (1) by introducing said recovered blend of solvent vapors into said chamber to increase the solvent humidity in said chamber to thereby retard the evaporation of solvents from said coating material supplied to said chamber, (2) by condensing said recovered blend of solvent vapors recovered at step (f) and introducing the condensed blend of solvents to said system as a liquid to return solvent lost in the coating process to the coating supply system, or (3) by a combination of steps (1) and (2), said blend of solvents being returned in substantially the same proportion as in the stream extracted in step (a).
Claim 11
Dependent Claim
30 words
The process of claim 8 wherein said absorption step (a) employs a steel packing material having a surface area greater than about 500 square feet per cubic foot of packing.