Abstract
Abstract An overstrike ribbon has its color transfer layer formed with an oleaginic face which includes a polyoxyethylene fatty acid ester of polyhydric alcohol which as increased ability to backup the fatty dyestuff, and also contains a filler from the pores of which the color paste can be released with successive impacts.
Inventors
- 👤 Ulrich Kohle
- 👤 Hans Paffhausen
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-07 11:50
CPC Classifications
B; B41; B41M; B41M5/00; B41M5/10; Y; Y10; Y10S; Y10S428/00; Y10S428/914
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
162 words
In an overstrike ribbon having enhanced strikeover capacity and comprising a polyester, polyethylene, polypropylene or polyamide carrier foil provided with a color transfer layer wherein the color transfer layer comprises a binder matrix of a synthetic resin in which a coloring paste is disposed for limited transfer to a print-receiving surface, the improvement wherein said coloring paste comprises at least one polyethoxylated fatty acid ester of a polyhydric alcohol forming an oleaginic phase in which a coloring agent in the form of an oleophilic dyestuff is dissolved, said polyethoxylated fatty acid ester being selected from the group which consists of polyoxyethylene-(40)-sorbite pentaoleate hexaoleate, heptaoleate and octaoleate and further contains a finely divided solid filler having a high internal surface area and a particle size distribution of 0.2 to 20 microns so that twelve and more strikeovers can be effected with high definition transfer, said filler being selected from the group which consists of diatomaceous earth, precipitated silica, active carbon and/or broken microspheres.
Claim 2
Dependent Claim
162 words
In an overstrike ribbon having enhanced strikeover capacity and comprising a polyester, polyethylene, polypropylene or polyamide carrier foil provided with a color transfer layer wherein the color transfer layer comprises a binder matrix of a synthetic resin in which a coloring paste is disposed for limited transfer to a print-receiving surface, the improvement wherein said coloring paste comprises at least one polyethoxylated fatty acid ester of a polyhydric alcohol forming an oleaginic phase in which a coloring agent in the form of an oleophilic dyestuff is dissolved, said polyethoxylated fatty acid ester being selected from the group which consists of polyoxyethylene-(40)-sorbite pentaoleate hexaoleate, heptaoleate and octaoleate and further contains a finely divided solid filler having a high internal surface area and a particle size distribution of 0.2 to 20 microns so that twelve and more strikeovers can be effected with high definition transfer, said filler being selected from the group which consists of diatomaceous earth, precipitated silica, active carbon and/or broken microspheres.
Claim 3
Dependent Claim
24 words
The improvement defined in claim 1 wherein the polyoxyethylene fatty acid ester is cut with up to 50% with a natural or synthetic oil.
Claim 4
Dependent Claim
17 words
The improvement defined in claim 1 wherein said color transfer layer further includes a cationic wetting agent.
References Cited (Backward Citations)
US3049457A
Cited
US2984582A
Cited
GB1000682A
Cited
US3336150A
Cited
GB958081A
Cited
GB1028618A
Cited
US3392042A
Cited
US3348651A
Cited
US3520495A
Cited
US3682683A
Cited
US3864181A
Cited
DE2232773A1
Cited
DE2418066A1
Cited
US3908063A
Cited
US4066585A
Cited
US4150187A
Cited
CH590784A5
Cited
US4217388A
Cited
US4321286A
Cited
US4299504A
Cited
US4427739A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1988-09-30 | 1989-04-01 | 1989-10-01 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1992-09-30 | 1993-04-01 | 1993-10-01 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1996-09-30 | 1997-04-01 | 1997-10-01 | $7700.00 | Window Closed / Lapsed |