Abstract

Abstract Blends of (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/α-olefin copolymer are used to prepare peelable seals having nearly constant and predictable peel strength over an extended heat seal temperature range. Some of the seals so produced also show stress whitening.

Inventors

  • 👤 George L. Hoh

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-24 18:16
CPC Classifications
C; C08; C08L; C08L23/00; C08L23/02; C08L23/04; C08L23/08; C08L23/0846; C08L23/0869; C08L23/0876; B; B32; B32B; B32B27/00; B32B27/30; C09; C09J; C09J123/00; C09J123/02; C09J123/04; C09J123/08; C09J123/0846; C09J123/0869; C09J123/0876; C08L23/10; C08L23/14; C08L2666/00; C08L2666/02; C08L2666/04; C08L2666/06; Y; Y10; Y10T; Y10T428/00; Y10T428/31504; Y10T428/31678; Y10T428/31692; Y10T428/31855; Y10T428/3188; Y10T428/31895; Y10T428/31909; Y10T428/31913

Claims Analysis

Total Claims: 7
Claim 1
Independent Claim 70 words
Coextrusions for producing film characterized by a nearly constant peel strength over an extended heat seal temperature range, made from a molecular blend of polymeric materials comprising: (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/α-olefin copolymer, wherein the α-olefin comprises 1-12 weight percent of the copolymer, and wherein said coextrusion further comprises at least one extrudable material other than said molecular blend.
Claim 2
Dependent Claim 70 words
Coextrusions for producing film characterized by a nearly constant peel strength over an extended heat seal temperature range, made from a molecular blend of polymeric materials comprising: (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/α-olefin copolymer, wherein the α-olefin comprises 1-12 weight percent of the copolymer, and wherein said coextrusion further comprises at least one extrudable material other than said molecular blend.
Claim 3
Dependent Claim 8 words
Laminates made from the coextrusions of claim 1.
Claim 4
Dependent Claim 64 words
Laminates characterized by a nearly constant peel strength over an extended heat seal temperature range, made from a molecular blend of polymeric materials comprising: (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/α-olefin copolymer, wherein the α-olefin comprises 1-12 weight percent of the copolymer, and wherein said laminate further comprises a substrate other than said molecular blend.
Claim 5
Dependent Claim 64 words
Laminates characterized by a nearly constant peel strength over an extended heat seal temperature range, made from a molecular blend of polymeric materials comprising: (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/α-olefin copolymer, wherein the α-olefin comprises 1-12 weight percent of the copolymer, and wherein said laminate further comprises a substrate other than said molecular blend.
Claim 6
Dependent Claim 54 words
Packages having peelable seals characterized by a nearly constant peel strength over an extended heat seal temperature range made from a molecular blend of polymeric materials comprising: (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/α-olefin copolymer, wherein the α-olefin comprises 1--12 weight percent of the copolymer.
Claim 7
Dependent Claim 54 words
Packages having peelable seals characterized by a nearly constant peel strength over an extended heat seal temperature range made from a molecular blend of polymeric materials comprising: (a) 80-93 weight percent of an ethylene/acid ionomer, and (b) 7-20 weight percent of a propylene/α-olefin copolymer, wherein the α-olefin comprises 1--12 weight percent of the copolymer.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1988-09-02 1989-03-04 1989-09-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1992-09-02 1993-03-04 1993-09-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1996-09-02 1997-03-04 1997-09-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag