Claim 1
Independent Claim
394 words
A process for producing a strain sensitive element, comprising the steps of (a) selecting a silicon crystal wafer with the plane of said wafer oriented (110); (b) depositing in a first depositing step an oxide layer on both sides of said wafer selected from said selecting step; (c) establishing coordinated indices on both sides of said wafer obtained from said depositing step; the improvement characterized by (d) on at least one side of said wafer, in a first defining step, defining on said oxide layer unsupported gages indexed [111] and the conductors therefore which are integral with said wafer by opening apertures in said oxide deposit corresponding to said defined gages and conductors; (e) said defining step for each strain sensitive element providing for at least one groove over which said integral gages will extend; (f) said defining step defining the entire bodies of said integral gages as being the only material extending over said groove without any separate support; (g) said groove dividing each said strain sensitive element into two parts with an integral hinge portion extending therebetween; (h) said integral hinge portion being spaced from said unsupported integral gages; (i) depositing in a second depositing step boron into said apertures from said first defining step; (j) subjecting said wafer to sufficiently elevated temperatures for a sufficient period of time to anneal said wafer; (k) opening an etching pattern on at least one side of said wafer to define said groove to be formed in said wafer over which said defined gages will extend and through which said integral hinge portion will extend; (l) said etching step being to a depth within the range of between about 0.0022 inches and 0.005 inches to undercut said defined gages, and form said defined groove; (m) said etching step being carried out to a point short of piercing said wafer for defining said hinge portion; (n) stripping from said wafer all residual oxide; (o) depositing in a third depositing step a thin oxide layer on said wafer to protect all positive-negative junctions thereon; (p) depositing in a fourth depositing step a metallic layer on at least one side of said wafer; (q) defining in a second defining step, said conductors for said gages in said metallic layer; and (r) cutting said wafer into strain sensitive elements containing said defined gages, conductors, groove or grooves, and hinge.
Claim 2
Dependent Claim
394 words
A process for producing a strain sensitive element, comprising the steps of (a) selecting a silicon crystal wafer with the plane of said wafer oriented (110); (b) depositing in a first depositing step an oxide layer on both sides of said wafer selected from said selecting step; (c) establishing coordinated indices on both sides of said wafer obtained from said depositing step; the improvement characterized by (d) on at least one side of said wafer, in a first defining step, defining on said oxide layer unsupported gages indexed [111] and the conductors therefore which are integral with said wafer by opening apertures in said oxide deposit corresponding to said defined gages and conductors; (e) said defining step for each strain sensitive element providing for at least one groove over which said integral gages will extend; (f) said defining step defining the entire bodies of said integral gages as being the only material extending over said groove without any separate support; (g) said groove dividing each said strain sensitive element into two parts with an integral hinge portion extending therebetween; (h) said integral hinge portion being spaced from said unsupported integral gages; (i) depositing in a second depositing step boron into said apertures from said first defining step; (j) subjecting said wafer to sufficiently elevated temperatures for a sufficient period of time to anneal said wafer; (k) opening an etching pattern on at least one side of said wafer to define said groove to be formed in said wafer over which said defined gages will extend and through which said integral hinge portion will extend; (l) said etching step being to a depth within the range of between about 0.0022 inches and 0.005 inches to undercut said defined gages, and form said defined groove; (m) said etching step being carried out to a point short of piercing said wafer for defining said hinge portion; (n) stripping from said wafer all residual oxide; (o) depositing in a third depositing step a thin oxide layer on said wafer to protect all positive-negative junctions thereon; (p) depositing in a fourth depositing step a metallic layer on at least one side of said wafer; (q) defining in a second defining step, said conductors for said gages in said metallic layer; and (r) cutting said wafer into strain sensitive elements containing said defined gages, conductors, groove or grooves, and hinge.
Claim 3
Dependent Claim
29 words
The process of claim 1, further characterized by (a) said first defining step, said open step, and said fourth depositing are carried out on both sides of said wafer.
Claim 4
Dependent Claim
49 words
The process of claim 2, further characterized by (a) said second depositing step is carried out in an amount sufficient to obtain diffused boron in the amount of at least 5×10 19 atoms per cubic centimeter, and a depth within the range of between about 0.1 to 3 micrometers.
Claim 5
Dependent Claim
28 words
The process of claim 1, further characterized by (a) said subjecting step is carried out by subjecting said wafer to a temperature of 920° C. for one hour.
Claim 6
Dependent Claim
25 words
The process of claim 1, further characterized by (a) said etching step being carried out with a bath containing potassium hydroxide, water, and isopropyl alcohol.
Claim 7
Dependent Claim
24 words
The process of claim 1, further characterized by (a) said etching step being carried out with a bath containing ethylene diamine, pyrocatechol and water.
Claim 8
Dependent Claim
30 words
The process of claim 1, further characterized by (a) said first defining step, said open step, and said fourth depositing step are carried out on one side of said wafer.
Claim 9
Dependent Claim
34 words
The process of claim 7, further characterized by (a) said second depositing step being carried out in an amount sufficient to obtain diffused boron in the amount of 10 20 boron per cubic centimeter.