Homogenous alloy powder
Assignee: General Electric Co
•
Filing: 1983-09-28
•
Granted: 1984-10-23
•
Expires: 2003-09-28
Abstract
Abstract A powder mixture for use in a method of repairing a superalloy article includes first and second Ni base superalloy powders. The first powder, characterized by superior hot corrosive resistance along with good oxidation resistance and the substantial absence of melting point depressants selected from Si and B greater than normal impurity levels, is included in the range of 30-70 wt % of the mixture. The second powder has a composition substantially within the same composition range as that of the first powder with the inclusion, by wt, of 0.5-5% B and up to 6% Si.
Inventors
- 👤 Murray S. Smith, Jr.
- 👤 Roger J. Perkins
- 👤 Robert E. Fryxell
- 👤 William R. Young
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-04 20:14
CPC Classifications
B; B23; B23P; B23P6/00; B23P6/002; B22; B22F; B22F1/00; B22F1/09; B23K; B23K35/00; B23K35/22; B23K35/24; B23K35/30; B23K35/3033; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49718; Y10T29/49746
Claims Analysis
Total Claims: 4
Claim 1
Independent Claim
246 words
A mixture of a Ni base superalloy first powder and a Ni base superalloy second powder, the combination defining a homogenous powder system; the first powder characterized by superior hot corrosion resistance along with good oxidation resistance and mechanical properties, and the substantial absence of melting point depressant elements selected from the group consisting of Si and B in amounts greater than 1 wt % Si and 0.05 wt % B; the first powder consisting essentially of, by weight, 0.01-0.2% C, 16-23% Cr, 2-10% Mo, 15-21% Fe, up to 6% of the sum of Cb and Ta, up to 2% Ti, less than 2% Al, less than 3% Co, up to 2% W, with the balance Ni and incidental impurities; and the second powder having a composition which includes all of the elements of the first powder each, except for elements selected from the group consisting of Si and B, within the respective percentage range of that of the first powder, the second powder consisting essentially of, by weight, 0.01-0.2% C, 16-23% Cr, 2-10% Mo, 15-21% Fe, up to 6% of the sum of Cb and Ta, up to 2% Ti, less than 2% Al, less than 3% Co, up to 2% W, 0.5-5% B, up to 6% Si, with the balance Ni and incidental impurities, and having a melting temperature lower than that of the first powder; the mixture consisting essentially of, by weight, 30-70% of the firt powder and 30-70% of the second powder.
Claim 2
Dependent Claim
246 words
A mixture of a Ni base superalloy first powder and a Ni base superalloy second powder, the combination defining a homogenous powder system; the first powder characterized by superior hot corrosion resistance along with good oxidation resistance and mechanical properties, and the substantial absence of melting point depressant elements selected from the group consisting of Si and B in amounts greater than 1 wt % Si and 0.05 wt % B; the first powder consisting essentially of, by weight, 0.01-0.2% C, 16-23% Cr, 2-10% Mo, 15-21% Fe, up to 6% of the sum of Cb and Ta, up to 2% Ti, less than 2% Al, less than 3% Co, up to 2% W, with the balance Ni and incidental impurities; and the second powder having a composition which includes all of the elements of the first powder each, except for elements selected from the group consisting of Si and B, within the respective percentage range of that of the first powder, the second powder consisting essentially of, by weight, 0.01-0.2% C, 16-23% Cr, 2-10% Mo, 15-21% Fe, up to 6% of the sum of Cb and Ta, up to 2% Ti, less than 2% Al, less than 3% Co, up to 2% W, 0.5-5% B, up to 6% Si, with the balance Ni and incidental impurities, and having a melting temperature lower than that of the first powder; the mixture consisting essentially of, by weight, 30-70% of the firt powder and 30-70% of the second powder.
Claim 3
Dependent Claim
88 words
The mixture of claim 1 in which: the first powder consists essentially of, by weight, 0.02-0.08% C, 16-21% Cr, 2.5-3.5 Mo, 15-21% Fe, 4.5-5.5% of the sum of Cb and Ta, 0.7-1.2% Ti, 0.3-0.7% Al, up to 1% Co, with the balance Ni and incidental impurities; and the second powder consists essentially of, by weight, 0.02-0.08% C, 16-21% Cr, 2.5-3.5% Mo, 15-21% Fe, 4.5-5.5% of the sum of Cb and Ta, 0.7-1.2% Ti, 0.3-0.7% Al, up to 1% Co, 2-2.5% B, with the balance Ni and incidental impurities.
Claim 4
Dependent Claim
64 words
A mixture of claim 1 in which: the first powder consists essentially of, by weight, 0.05-0.15% C, 19-23% Cr, 7-10% Mo, 16-20% Fe, 0.5-2.5% Co, 0.2-1% W, with the balance Ni and incidental impurities; and the second powder consists essentially of, by weight, 0.05-0.15% C, 19-23% Cr, 7-10% Mo, 16-20% Fe, 0.5-2.5% Co, 0.2-1% W, 3-4% B, with the balance Ni and incidental impurities.
References Cited (Backward Citations)
US2714760A
Cited
US3024109A
Cited
US3073269A
Cited
US3012903A
Cited
US3197858A
Cited
US3108861A
Cited
US3155491A
Cited
US3246981A
Cited
US3632319A
Cited
US3717442A
Cited
US4008844A
Cited
US4059217A
Cited
US4098450A
Cited
US4176433A
Cited
US4299629A
Cited
EP0024142A1
Cited
US4285459A
Cited
US4389251A
Cited
FR2511908A1
Cited
US4381944A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1987-10-23 | 1988-04-23 | 1988-10-23 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1991-10-23 | 1992-04-23 | 1992-10-23 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1995-10-23 | 1996-04-23 | 1996-10-23 | $7700.00 | Window Closed / Lapsed |