Method of fixing a ferrite to a metal piece

Assignee: Thales SA
•
Filing: 1982-01-07
•
Granted: 1984-07-03
•
Expires: 2002-01-07
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract In a method for fixing a ferrite to a metal piece such as a pole-piece of a magnetic polarizing circuit of a microwave device, a first step consists in depositing a nonresistive metal on the ferrite face to be fixed. A second step consists in applying a very thin layer of heat-conducting adhesive on the metallized ferrite face and bonding the ferrite to the metal piece, thus ensuring low thermal resistance, very low insertion loss and high power capability.

Inventors

  • 👤 Gerard Forterre
  • 👤 Pierre Hartemann

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-25 12:44
CPC Classifications
H; H01; H01P; H01P1/00; H01P1/32; H01P1/38; H01P1/383; C; C04; C04B; C04B37/00; C04B37/02; C04B37/023; C04B37/026; C04B37/028; H01P1/39; C04B2235/00; C04B2235/02; C04B2235/50; C04B2235/54; C04B2235/5418; C04B2235/5445; C04B2235/65; C04B2235/656; C04B2235/6562; C04B2237/00; C04B2237/02; C04B2237/12; C04B2237/121; C04B2237/124; C04B2237/125; C04B2237/30; C04B2237/32; C04B2237/34; C04B2237/40; C04B2237/405; C04B2237/406; C04B2237/50; C04B2237/70; C04B2237/708; C04B2237/72; Y; Y10; Y10S; Y10S228/00; Y10S228/903

Claims Analysis

Total Claims: 10
Claim 1
Independent Claim 51 words
A method of fixing a ferrite to a metal piece for a high-power microwave device, comprising the following steps: deposit of a nonresistive metal on the face of the ferrite to be fixed; bonding of the metallized face of said ferrite to the metal piece by means of a heat-conducting adhesive.
Claim 2
Independent Claim 51 words
A method of fixing a ferrite to a metal piece for a high-power microwave device, comprising the following steps: deposit of a nonresistive metal on the face of the ferrite to be fixed; bonding of the metallized face of said ferrite to the metal piece by means of a heat-conducting adhesive.
Claim 3
Dependent Claim 22 words
A method as claimed in claim 1, wherein deposit of a nonresistive metal is performed by cathode sputtering of the triode type.
Claim 4
Dependent Claim 15 words
A method as claimed in claim 1 or 2, wherein said nonresistive metal is aluminium.
Claim 5
Dependent Claim 23 words
A method as claimed in claim 1, wherein the thickness of the nonresistive metal deposit is within the range of 5 to 10μ.
Claim 6
Dependent Claim 24 words
A method as claimed in claim 1, wherein said heat-conducting adhesive constitutes a thin layer having a thickness of the order of 0.03 mm.
Claim 7
Dependent Claim 23 words
A method as claimed in claim 1, wherein said metal piece is the pole-piece of a magnet which serves to polarize the ferrite.
Claim 8
Dependent Claim 14 words
A method as claimed in claim 6, wherein said ferrite is a lithium ferrite.
Claim 9
Independent Claim 116 words
A method of fixing a ferrite to a metal piece for a high-power microwave device in which the behavior of the ferrite microwave device as a function of power is dependent on the temperature finally attained by the ferrite, comprising the steps of depositing a non-resistive metal on the face of the ferrite to be fixed; bonding the metalized face of said ferrite to the metal piece by means of a heat conducting adhesive, whereby said fixed ferrite in said high power microwave device is not subject to microwave losses and minimizes such losses at the surface of the ferrite and is capable of operating at said temperature finally attained in said high power microwave device.
Claim 10
Independent Claim 116 words
A method of fixing a ferrite to a metal piece for a high-power microwave device in which the behavior of the ferrite microwave device as a function of power is dependent on the temperature finally attained by the ferrite, comprising the steps of depositing a non-resistive metal on the face of the ferrite to be fixed; bonding the metalized face of said ferrite to the metal piece by means of a heat conducting adhesive, whereby said fixed ferrite in said high power microwave device is not subject to microwave losses and minimizes such losses at the surface of the ferrite and is capable of operating at said temperature finally attained in said high power microwave device.

References Cited (Backward Citations)

US3662291A Cited
US3886025A Cited
US3873944A Cited
US4034377A Cited
US4172318A Cited
US4260966A Cited
FR2443750A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-07-03 1988-01-02 1988-07-03 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-07-03 1992-01-02 1992-07-03 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-07-03 1996-01-02 1996-07-03 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag