Patent US4446281A successfully refreshed from Google Patents.
← Back to Patent Explorer
US4446281A Expired / Lapsed US ⏱️ 0.0 years remaining

Modified cis-1,4-polyisoprene rubber, a process for manufacturing the same, and a composition containing the same

Assignee: Kuraray Co Ltd
•
Filing: 1982-05-19
•
Granted: 1984-05-01
•
Expires: 2002-05-19
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract Modified cis-1,4-polyisoprene rubber obtained by incorporating into cis-1,4-polyisoprene rubber a side chain formed by succinimide residue containing in the N position a hydrocarbon residue having at least one tertiary nitrogen atom. This rubber is excellent in green strength at ordinary room temperature, and flowability at an elevated temperature. Its vulcanizate is comparable to, or better than natural rubber in breaking strength and hardness.

Inventors

  • 👤 Hideo Takamatsu
  • 👤 Shobu Minatono

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-31 08:10
CPC Classifications
C; C08; C08C; C08C19/00; C08C19/30; C08C19/34; C08C19/36; C08C19/28

Claims Analysis

Total Claims: 14
Claim 1
Independent Claim 124 words
A modified cis-1,4-polyisoprene rubber, comprising: a solid synthetic cis-1,4-polyisoprene rubber having a side chain functional group of the formula (I) incorporated into said synthetic rubber, said modified rubber containing at least 0.01 mole of said functional group per 100 recurring units of isoprene monomer in said synthetic rubber: ##STR10## wherein R 1 represents hydrogen, or a covalent bond with a rubber molecule, R 2 represents a hydrocarbon residue having not more than 20 carbon atoms, optionally containing an oxygen or sulfur atom in its principal chain, and A represents a dihydrocarbylamino residue having not more than 20 carbon atoms, or a heterocyclic residue having not more than 20 carbon atoms and containing at least one tertiary nitrogen atom alone as a hetero nitrogen atom.
Claim 2
Dependent Claim 124 words
A modified cis-1,4-polyisoprene rubber, comprising: a solid synthetic cis-1,4-polyisoprene rubber having a side chain functional group of the formula (I) incorporated into said synthetic rubber, said modified rubber containing at least 0.01 mole of said functional group per 100 recurring units of isoprene monomer in said synthetic rubber: ##STR10## wherein R 1 represents hydrogen, or a covalent bond with a rubber molecule, R 2 represents a hydrocarbon residue having not more than 20 carbon atoms, optionally containing an oxygen or sulfur atom in its principal chain, and A represents a dihydrocarbylamino residue having not more than 20 carbon atoms, or a heterocyclic residue having not more than 20 carbon atoms and containing at least one tertiary nitrogen atom alone as a hetero nitrogen atom.
Claim 3
Dependent Claim 14 words
The modified cis-1,4-polyisoprene rubber of claim 1, wherein R 2 is an alkylene residue.
Claim 4
Dependent Claim 18 words
The modified cis-1,4-polyisoprene rubber of claim 1, wherein R 2 in said formula (I) is an alkoxyalkylene residue.
Claim 5
Dependent Claim 17 words
The modified cis-1,4-polyisoprene rubber of claim 1, wherein A in said formula (I) is a dialkylamino residue.
Claim 6
Dependent Claim 153 words
A process for manufacturing modified cis-1,4-polyisoprene rubber, which comprises: adding a compound selected from the group consisting of maleic anhydride, maleic acid, maleic acid monoesters and maleic acid diesters to solid synthetic cis-1,4-polyisoprene rubber having a molecular weight ranging from 200,000 to 2,000,000 in the quantity of at least 0.01 mole per 100 recurring units of isoprene monomer in said synthetic rubber; reacting the resulting product with an amine of formula (II) H.sub.2 N--R.sup.2 --A (II) wherein R 2 represents a hydrocarbon residue having not more than 20 carbon atoms, optionally containing an oxygen or sulfur atom in its principal chain, and A represents a dihydrocarbylamino residue having not more than 20 carbon atoms, or a heterocyclic residue having not more than 20 carbon atoms and containing at least one tertiary nitrogen atom alone as a hetero nitrogen atom; and subjecting the reaction product to dehydration or dealcoholization to form an imide ring.
Claim 7
Dependent Claim 153 words
A process for manufacturing modified cis-1,4-polyisoprene rubber, which comprises: adding a compound selected from the group consisting of maleic anhydride, maleic acid, maleic acid monoesters and maleic acid diesters to solid synthetic cis-1,4-polyisoprene rubber having a molecular weight ranging from 200,000 to 2,000,000 in the quantity of at least 0.01 mole per 100 recurring units of isoprene monomer in said synthetic rubber; reacting the resulting product with an amine of formula (II) H.sub.2 N--R.sup.2 --A (II) wherein R 2 represents a hydrocarbon residue having not more than 20 carbon atoms, optionally containing an oxygen or sulfur atom in its principal chain, and A represents a dihydrocarbylamino residue having not more than 20 carbon atoms, or a heterocyclic residue having not more than 20 carbon atoms and containing at least one tertiary nitrogen atom alone as a hetero nitrogen atom; and subjecting the reaction product to dehydration or dealcoholization to form an imide ring.
Claim 8
Dependent Claim 10 words
The method of claim 5, wherein said amine is (dialkylamino)alkylamine.
Claim 9
Dependent Claim 105 words
A process for manufacturing a modified cis-1,4-polyisoprene rubber, which comprises: reacting a solid synthetic cis-1,4-polyisoprene rubber with at least 0.01 mole of a maleimide derivative of the formula (I) per 100 recurring units of isoprene monomer in said synthetic rubber: ##STR11## wherein R 2 represents a hydrocarbon residue having not more than 20 carbon atoms, and optionally containing an oxygen or sulfur atom in its principal chain, and A represents a dihydrocarbylamino residue having not more than 20 carbon atoms, or a heterocyclic residue having not more than 20 carbon atoms and containing at least one tertiary nitrogen atom alone as a hetero nitrogen atom.
Claim 10
Dependent Claim 105 words
A process for manufacturing a modified cis-1,4-polyisoprene rubber, which comprises: reacting a solid synthetic cis-1,4-polyisoprene rubber with at least 0.01 mole of a maleimide derivative of the formula (I) per 100 recurring units of isoprene monomer in said synthetic rubber: ##STR11## wherein R 2 represents a hydrocarbon residue having not more than 20 carbon atoms, and optionally containing an oxygen or sulfur atom in its principal chain, and A represents a dihydrocarbylamino residue having not more than 20 carbon atoms, or a heterocyclic residue having not more than 20 carbon atoms and containing at least one tertiary nitrogen atom alone as a hetero nitrogen atom.
Claim 11
Dependent Claim 25 words
The method of claim 7, wherein said maleimide derivative is a compound selected from the group consisting of N-(β-dimethylamino)ethylmaleimide, N-(β-diethylamino)ethylmaleimide, N-(γ-dimethylamino)propylmaleimide, N-(γ-diethylamino)propylmaleimide, N-(δ-dimethylamino)butylmaleimide and N-(δ-diethylamino)butylmaleimide.
Claim 12
Dependent Claim 136 words
A vulcanized rubber composition, comprising: as its rubber constituent, modified cis-1,4-polyisoprene rubber comprising solid synthetic cis-1,4-polyisoprene rubber having a side chain functional group of formula (I) incorporated in said synthetic rubber, said modified rubber containing at least 0.01 mole of said functional group per 100 recurring units of isoprene monomer in said synthetic rubber: ##STR12## wherein R 1 represents hydrogen, or a covalent bond representing bonding of the functional group to the rubber molecule, R 2 represents a hydrocarbon residue having not more than 20 carbon atoms, optionally containing an oxygen or sulfur atom in its principal chain, and A represents an N,N-dihydrocarbylamino residue having not more than 20 carbon atoms or a heterocyclic residue having not more than 20 carbon atoms, and containing at least one tertiary nitrogen atom alone as a hetero nitrogen atom.
Claim 13
Dependent Claim 136 words
A vulcanized rubber composition, comprising: as its rubber constituent, modified cis-1,4-polyisoprene rubber comprising solid synthetic cis-1,4-polyisoprene rubber having a side chain functional group of formula (I) incorporated in said synthetic rubber, said modified rubber containing at least 0.01 mole of said functional group per 100 recurring units of isoprene monomer in said synthetic rubber: ##STR12## wherein R 1 represents hydrogen, or a covalent bond representing bonding of the functional group to the rubber molecule, R 2 represents a hydrocarbon residue having not more than 20 carbon atoms, optionally containing an oxygen or sulfur atom in its principal chain, and A represents an N,N-dihydrocarbylamino residue having not more than 20 carbon atoms or a heterocyclic residue having not more than 20 carbon atoms, and containing at least one tertiary nitrogen atom alone as a hetero nitrogen atom.
Claim 14
Dependent Claim 35 words
The rubber composition of claim 9, wherein said composition is vulcanized with a vulcanizing agent in the amount of 0.01 to 10 parts per weight per 100 parts per weight of said modified cis-1,4-polyisoprene rubber.

References Cited (Backward Citations)

US3778418A Cited
US3965076A Cited
FR2300108A1 Cited
US4137282A Cited
DE2944082A1 Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1987-05-01 1987-10-31 1988-05-01 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1991-05-01 1991-10-31 1992-05-01 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1995-05-01 1995-10-31 1996-05-01 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag