US4411059A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for manufacturing a charge splitting resistive layer for a semiconductor gamma camera

Assignee: Philips Nuclear Medicine Inc
•
Filing: 1980-08-18
•
Granted: 1983-10-25
•
Expires: 2000-08-18
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract An improved semiconductor gamma camera is disclosed. The gamma camera includes a p-i-n semiconductor diode which detects the presence and energy of gamma radiation from a source. Typically the source is radioactive material in a patient organ which is detected and then interpreted by a doctor while diagnosing the condition of that organ. The detector includes an improved electrical connection technique to allow the p-i-n diode to be connected to electronic circuitry necessary to provide spatial and energy information. In the improved camera first a passivation layer is deposited on both faces of the p-i-n diode and then a resistive layer is applied to form a reliable easily reproduced electrical contact to the junction. These two layers in combination prevent foreign matter from contacting the semiconductor material comprising the detector while providing interconnection to the electronic circuitry.

Inventors

  • 👤 Philip A. Schlosser
  • 👤 Don W. Miller

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-09 08:39
CPC Classifications
G; G01; G01T; G01T1/00; G01T1/29; G01T1/2914; G01T1/2921; G01T1/2928; H; H10; H10F; H10F30/00; H10F30/20; H10F30/29; H10F30/292; H10F39/00; H10F39/10; H10F39/12; H10F39/18

Claims Analysis

Total Claims: 4
Claim 1
Independent Claim 149 words
A method for manufacturing a solid state gamma ray detector comprising: (a) providing a portion of high purity intrinsic semiconductor material having two opposed surfaces; (b) regionally doping at spaced intervals both surfaces of the semiconductor material portion with parallel bands of p type material on one surface and orthogonal parallel bands of n type material on an opposed surface; (c) applying a passivation layer over at least a portion of the regionally doped surfaces and providing an opening through the passivation layer communication with the doped intervals on each surface; (d) applying a resistive layer over at least a portion of the passivation layer, including application of material of the resistive layer within the opening of the passivation layer for conductive communication between the doped intervals on each surface and the resistive layer, and (e) providing at least one electrical contact on said resistive layer for each surface.
Claim 2
Independent Claim 149 words
A method for manufacturing a solid state gamma ray detector comprising: (a) providing a portion of high purity intrinsic semiconductor material having two opposed surfaces; (b) regionally doping at spaced intervals both surfaces of the semiconductor material portion with parallel bands of p type material on one surface and orthogonal parallel bands of n type material on an opposed surface; (c) applying a passivation layer over at least a portion of the regionally doped surfaces and providing an opening through the passivation layer communication with the doped intervals on each surface; (d) applying a resistive layer over at least a portion of the passivation layer, including application of material of the resistive layer within the opening of the passivation layer for conductive communication between the doped intervals on each surface and the resistive layer, and (e) providing at least one electrical contact on said resistive layer for each surface.
Claim 3
Independent Claim 166 words
A method for constructing a gamma camera detector comprising the steps of: (a) fabricating a high purity germanium crystal with two exposed opposite surfaces; (b) doping selected portions of said germanium crystal with p type impurities; said selected portions aligned in parallel configurations and forming a portion of a first exposed surface; (c) doping other selected portions of said germanium crystal with n type impurities, said other portions aligned parallel to each other and orthogonal to the p type impurities and forming a portion of a second exposed surface; (d) covering all but selected portions of the doped and all the nondoped portions of said exposed surfaces with a passivation layer; (e) covering said passivation layer with a resistive layer, said resistive layer extending through the passivation layer to contact the doped portions of the germanium; and (f) providing electrical contacts to said resistive layer to transmit electrical signals to an electrical interpreting circuit for determining spatial positioning and energy content of radiation entering said detector.
Claim 4
Independent Claim 166 words
A method for constructing a gamma camera detector comprising the steps of: (a) fabricating a high purity germanium crystal with two exposed opposite surfaces; (b) doping selected portions of said germanium crystal with p type impurities; said selected portions aligned in parallel configurations and forming a portion of a first exposed surface; (c) doping other selected portions of said germanium crystal with n type impurities, said other portions aligned parallel to each other and orthogonal to the p type impurities and forming a portion of a second exposed surface; (d) covering all but selected portions of the doped and all the nondoped portions of said exposed surfaces with a passivation layer; (e) covering said passivation layer with a resistive layer, said resistive layer extending through the passivation layer to contact the doped portions of the germanium; and (f) providing electrical contacts to said resistive layer to transmit electrical signals to an electrical interpreting circuit for determining spatial positioning and energy content of radiation entering said detector.

References Cited (Backward Citations)

US3570114A Cited
US3761711A Cited
US3748549A Cited
US3890506A Cited
US3898686A Cited
US4029965A Cited
US4055765A Cited
US4208781A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1986-10-24 1987-04-25 1987-10-25 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1990-10-24 1991-04-25 1991-10-25 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1994-10-24 1995-04-25 1995-10-25 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag