Method for releasing printed wiring boards from printed wiring board racks
Assignee: Lockheed Martin Corp
•
Filing: 1979-12-10
•
Granted: 1981-07-21
•
Expires: 1999-12-10
Abstract
Abstract A release coating for printing wiring board racks comprises 100 parts by weight of a polyethylene glycol having a molecular weight range of from about 3000 to 3700, about 20 to about 200 parts by weight of a liquid polyethylene glycol having a molecular weight range of from about 380 to about 420, and from 0 to about 35 parts by weight of water.
Inventors
- 👤 Marvin Packer
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-06 15:31
CPC Classifications
H; H05; H05K; H05K3/00; H05K3/30; H05K3/32; H05K3/34; H05K3/3489; B; B23; B23K; B23K35/00; B23K35/22; B23K35/224; C; C08; C08L; C08L71/00; C08L71/02; Y; Y10; Y10T; Y10T29/00; Y10T29/49; Y10T29/49002; Y10T29/49117; Y10T29/49124; Y10T29/4913; Y10T29/49144; Y10T428/00; Y10T428/28; Y10T428/2839
Claims Analysis
Total Claims: 6
Claim 1
Independent Claim
166 words
In a process of assembling printed circuit boards without lead clinching of the components to the printed circuit board which comprises coating a side of the printed circuit board into which the electronic components are inserted with a sprayable, non-flowing, water soluble adhesive composition, inserting the coated board in a printed circuit board rack, removing the printed circuit board, inserting the electronic components therein, and storing the printed circuit board containing the components in the printed circuit board rack prior to soldering the components thereto, the improvement comprises: coating the printed circuit board racks with a water rinsable, non-corrosive composition which is compatible with the non-flowing water-soluble adhesive composition comprising about 100 parts by weight of a polyethylene glycol having a molecular weight range of from about 3000 to about 3700, 20 to about 200 parts by weight of a polyethylene glycol having a molecular weight range of from about 380 to about 420 and from about 0 to about 35 parts by weight of water.
Claim 2
Dependent Claim
166 words
In a process of assembling printed circuit boards without lead clinching of the components to the printed circuit board which comprises coating a side of the printed circuit board into which the electronic components are inserted with a sprayable, non-flowing, water soluble adhesive composition, inserting the coated board in a printed circuit board rack, removing the printed circuit board, inserting the electronic components therein, and storing the printed circuit board containing the components in the printed circuit board rack prior to soldering the components thereto, the improvement comprises: coating the printed circuit board racks with a water rinsable, non-corrosive composition which is compatible with the non-flowing water-soluble adhesive composition comprising about 100 parts by weight of a polyethylene glycol having a molecular weight range of from about 3000 to about 3700, 20 to about 200 parts by weight of a polyethylene glycol having a molecular weight range of from about 380 to about 420 and from about 0 to about 35 parts by weight of water.
Claim 3
Dependent Claim
16 words
The process according to claim 1 wherein the composition contains about 30 parts by weight water.
Claim 4
Dependent Claim
35 words
The process according to claim 1 wherein the composition contains from about 20 to about 100 parts by weight of a polyethylene glycol having a molecular weight range of from about 380 to about 420.
Claim 5
Dependent Claim
17 words
The process according to claim 3 wherein the composition contains about 30 parts by weight of water.
Claim 6
Dependent Claim
59 words
The process according to claim 4 wherein the composition comprises about 100 parts by weight of a polyethylene glycol having a molecular weight range of from about 3000 to about 3700, about 30 parts by weight of a polyethylene glycol having a molecular weight range of from about 380 to about 420, and about 30 parts by weight water.
References Cited (Backward Citations)
US3443988A
Cited
US3625715A
Cited
US3745028A
Cited
US3829319A
Cited
US3973322A
Cited
US4127692A
Cited
US4166150A
Cited
US4215025A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-07-20 | 1985-01-19 | 1985-07-21 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-07-20 | 1989-01-19 | 1989-07-21 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-07-20 | 1993-01-19 | 1993-07-21 | $7700.00 | Window Closed / Lapsed |