Abstract
Abstract A process for selecting a C 5 -based hydrocarbon tackifying resin to be used in an adhesive composition with a monoalkenyl arene conjugated diene block copolymer is disclosed. Pursuant to the selection process, a novel tackifying resin having an unobvious balance of properties is also disclosed, along with its combination with an elastomeric block copolymer in an adhesive composition.
Inventors
- 👤 Earle E. Ewins, Jr.
- 👤 deceased Cocker Jr.
Bibliographic Details
Application Number
—
Jurisdiction
US
Data Source
google_patents
Last Synchronized
2026-11-05 10:55
CPC Classifications
C; C09; C09J; C09J153/00; C09J153/02; C08; C08L; C08L2666/00; C08L2666/02; C08L2666/04
Claims Analysis
Total Claims: 5
Claim 1
Independent Claim
131 words
An adhesive composition comprising 100 parts by weight of a block copolymer component and 20 to 300 parts by weight of a tackifying resin component wherein: (a) said block copolymer component comprises a mixture of a linear or radial ABA type block copolymer and an AB two block copolymer where the A blocks are polystyrene blocks and the B blocks are polybutadiene or polyisoprene blocks; and (b) said tackifying resin component has a softening point of 70° to 100° C., a number average molecular weight of 1,000 to 1,600, and comprises from about 80 to 91 percent by weight units derived from piperylene, from about 1 to about 8 percent by weight units derived from isobutylene and from about 8 to about 12 percent by weight units derived from alphamethyl styrene.
Claim 2
Dependent Claim
131 words
An adhesive composition comprising 100 parts by weight of a block copolymer component and 20 to 300 parts by weight of a tackifying resin component wherein: (a) said block copolymer component comprises a mixture of a linear or radial ABA type block copolymer and an AB two block copolymer where the A blocks are polystyrene blocks and the B blocks are polybutadiene or polyisoprene blocks; and (b) said tackifying resin component has a softening point of 70° to 100° C., a number average molecular weight of 1,000 to 1,600, and comprises from about 80 to 91 percent by weight units derived from piperylene, from about 1 to about 8 percent by weight units derived from isobutylene and from about 8 to about 12 percent by weight units derived from alphamethyl styrene.
Claim 3
Dependent Claim
57 words
The adhesive composition of claim 1 wherein said tackifying resin has a softening point of about 85° C., a number average molecular weight of about 1,400, and comprises about 84 percent by weight units derived from piperylene, about 11 percent by weight units derived from alphamethyl styrene, and about 5 percent by weight units derived from isobutylene.
Claim 4
Dependent Claim
35 words
The adhesive composition of claim 1 wherein said block copolymer component comprises 40 to 95 parts by weight of the ABA-type block copolymer and 60 to 5 parts by weight of the AB-type block copolymer.
Claim 5
Dependent Claim
14 words
An adhesive composition according to claim 1 wherein said B blocks are polyisoprene blocks.
References Cited (Backward Citations)
US3281383A
Cited
US3239478A
Cited
US3519585A
Cited
US3577398A
Cited
GB1426497A
Cited
US3932328A
Cited
US3817953A
Cited
US3865797A
Cited
US3893986A
Cited
US4104327A
Cited
US4136071A
Cited
USPTO Annuity & Maintenance Windows
| Annuity Stage | Window Opens | Payment Deadline | Surcharge Period Until | Estimated Fee | Status |
|---|---|---|---|---|---|
| 3.5 Years (Year 4) | 1984-02-10 | 1984-08-11 | 1985-02-10 | $2000.00 | Window Closed / Lapsed |
| 7.5 Years (Year 8) | 1988-02-10 | 1988-08-11 | 1989-02-10 | $3760.00 | Window Closed / Lapsed |
| 11.5 Years (Year 12) | 1992-02-10 | 1992-08-11 | 1993-02-10 | $7700.00 | Window Closed / Lapsed |