← Back to Patent Explorer
US4244722A Expired / Lapsed US ⏱️ 0.0 years remaining

Method for manufacturing thin and flexible ribbon of dielectric material having high dielectric constant

Assignee: Individual
•
Filing: 1978-12-07
•
Granted: 1981-01-13
•
Expires: 1998-12-07
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract A method for manufacturing a thin and flexible ribbon of dielectric material comprises heating a raw material mainly consisting of dielectric material which can form a crystalline structure in a solid state and of a glass former which is included by 0 to 50 atomic percentages at a temperature above a melting point of the raw material to form a one phase melt; ejecting the melt thus formed through a nozzle against a cooling surface of a rotating disc, drum or belt, the ejection being carried out under a pressure of 0.01 to 1.5 atm. to form a continuous jet flow of the melt; and cooling instantaneously and rapidly the jet flow of the melt while it is in contact with the cooling surface at a cooling rate of 1,000 to 1,000,000° C./sec so as to form a thin and flexible ribbon of the dielectric material which contains the amorphous state more than 50% in an area ratio. The dielectric constant and breakdown voltage of the ribbon thus formed are very high. Further the mechanical property of the ribbon is also superior to that of known plate or chip of dielectric material. The dielectric constant and the breakdown voltage can be improved by heating the ribbon as grown at a temperature within 300° to 1,100° C.

Inventors

  • 👤 Noboru Tsuya
  • 👤 Kenichi Arai

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-10-26 12:16
CPC Classifications
C; C03; C03B; C03B17/00; C03B17/06; C03B32/00; C03B32/02; C03C; C03C3/00; C03C3/04; C03C3/076; C03C3/089; C03C3/12; C03C3/16; C03C3/23; C03C3/32; C03C3/325; H; H01; H01B; H01B3/00; H01B3/02; H01B3/08; H01B3/087; H01B3/088; H01G; H01G4/00; H01G4/002; H01G4/018; H01G4/06; H01G4/08; H10; H10N; H10N30/00; H10N30/01; H10N30/07; H10N30/074; H10N30/80; H10N30/85; H10N30/853; Y; Y10; Y10S; Y10S65/00; Y10S65/15

Claims Analysis

Total Claims: 19
Claim 1
Independent Claim 158 words
A method for manufacturing a thin and flexible ribbon of dielectric material comprising the steps of heating a raw material consisting essentially of a dielectric material which can form a crystalline structure in a solid state and up to 50 atomic percent of a glass former at a temperature from the melting point of the raw material to about 300° C. above the melting point to form a one phase melt of the raw material; ejecting the melt through a nozzle under a pressure in the form of a jet flow against a moving surface of a cooling substrate moving at a speed of more than about 5 m/sec; and cooling the jet flow of the melt on the cooling surface at a cooling rate of about 1,000° to 1,000,000° C./sec so as to form a thin and flexible ribbon of the dielectric material containing an amorphous texture in an amount of more than 50% by area ratio.
Claim 2
Independent Claim 158 words
A method for manufacturing a thin and flexible ribbon of dielectric material comprising the steps of heating a raw material consisting essentially of a dielectric material which can form a crystalline structure in a solid state and up to 50 atomic percent of a glass former at a temperature from the melting point of the raw material to about 300° C. above the melting point to form a one phase melt of the raw material; ejecting the melt through a nozzle under a pressure in the form of a jet flow against a moving surface of a cooling substrate moving at a speed of more than about 5 m/sec; and cooling the jet flow of the melt on the cooling surface at a cooling rate of about 1,000° to 1,000,000° C./sec so as to form a thin and flexible ribbon of the dielectric material containing an amorphous texture in an amount of more than 50% by area ratio.
Claim 3
Dependent Claim 27 words
A method as defined in claim 1, wherein the raw material is heated at a temperature from the melting point to 150° C. above the melting point.
Claim 4
Dependent Claim 93 words
A method as defined in claim 1, wherein the dielectric material is selected from the group consisting of BaTiO 3 , PbTiO 3 , Pb(Ti,Zr)O 3 , LiTaO 3 , NaNbO 3 , NaTaO 3 , AgNbO 3 , Pb(Zn 1/3 Nb 2/3 )O 3 , Pb(Fe 1/2 Nb 1/2 )O 3 , Ba 2 Nb 2 O 7 , Ca 2 Nb 2 O 7 , Ba 2 Ta 2 O 7 , BaBi 2 Ta 2 O 9 , K x WO 3 (0.43≦x≦0.51), PbNb 2 O 6 and composites thereof.
Claim 5
Dependent Claim 137 words
A method as defined in claim 1, wherein the glass former is selected from the group consisting of B 2 O 3 , PbO, Bi 2 O 3 , Li 2 O, K 2 O, MnO, Lu 2 O 3 , Cs 2 O, SnO, SnO 2 , GeO 2 , Sb 2 O 3 , P 2 O 5 , V 2 O 5 , In 2 O 3 , BeO, MgO, CaO, ZnO, CdO, SrO, BaO, ThO 2 , ZrO 2 , WO 3 , SiO 2 , Al 2 O 3 , As 2 O 3 , PbF 2 , LiF, NaF, BeF 2 , MgF 2 , ZnF 2 , CdF 2 , SrF 2 , BaF 2 , AlF 3 , BiF 3 , CeF 3 , SnF 4 and composites thereof.
Claim 6
Dependent Claim 26 words
A method as defined in claim 1, wherein the ejection of the melt against the cooling surface is effected in a reduced pressure or a vacuum.
Claim 7
Dependent Claim 25 words
A method as defined in claim 1, wherein the ejection of the melt against the cooling surface is conducted in a reduced inert gas atmosphere.
Claim 8
Dependent Claim 31 words
A method as defined in claim 1, wherein the ejection of the melt is carried out through the nozzle made of material selected from the group consisting of platinum and platinum-rhodium.
Claim 9
Dependent Claim 15 words
A method as defined in claim 7, wherein the nozzle is lined with boron nitride.
Claim 10
Dependent Claim 22 words
A method as defined in claim 1, wherein the ejection pressure is within the range of from about 0.01 to 1.5 atm.
Claim 11
Dependent Claim 22 words
A method as defined in claim 9, wherein the ejection pressure is within the range of from about 0.01 to 1.0 atm.
Claim 12
Dependent Claim 33 words
A method as defined in claim 1, wherein the moving surface of the cooling substrate is made of material selected from the group consisting of copper, copper-beryllium, brass, stainless steel and carbon steel.
Claim 13
Dependent Claim 21 words
A method as defined in claim 1, wherein the cooling substrate comprises a rotating disc which has a smooth peripheral edge.
Claim 14
Dependent Claim 21 words
A method as defined in claim 1, wherein the cooling substrate comprises a rotating drum which has a smooth inner surface.
Claim 15
Dependent Claim 19 words
A method as defined in claim 1, wherein the cooling substrate comprises an endless belt having a smooth surface.
Claim 16
Dependent Claim 17 words
A method as defined in claim 1, wherein the nozzle has a circular, elliptical or rectangular hole.
Claim 17
Dependent Claim 56 words
A method as defined in claim 1 further comprising the step of heating the thin and flexible ribbon as grown at a temperature within the range from 300° C. to 1,100° C. for such a time period that grains of crystalline texture of the dielectric material having sizes of 0.01-5.0 μm are grown in the ribbon.
Claim 18
Dependent Claim 24 words
A method as defined in claim 16, wherein the heating of the thin and flexible ribbon is effected in a vacuum or reduced atmosphere.
Claim 19
Dependent Claim 24 words
A method as defined in claim 16, wherein the heating of the thin and flexible ribbon is carried out in an inert gas atmosphere.

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1984-01-13 1984-07-14 1985-01-13 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1988-01-13 1988-07-14 1989-01-13 $3760.00 Window Closed / Lapsed
11.5 Years (Year 12) 1992-01-13 1992-07-14 1993-01-13 $7700.00 Window Closed / Lapsed

Assigned Categories & Tags

No categories assigned to this patent yet.

Assign Category Tag