Process for the preparation of bituminous compositions making use of a mother solution containing polymers and sulfur

Assignee: Koch Enterprises Inc
•
Filing: 1979-06-13
•
Granted: 1980-12-30
•
Expires: 1999-06-13
📄 Original PDF 🌐 Google Patents 🔄 Sync Now

Abstract

Abstract This invention relates to a new process for the preparation of improved polymeric bitumens. The process is characterized by preparing a first composition by admixing a petroleum fraction (160 DEG -230 DEG C.), while stirring, at a temperature of from 80 DEG C. to 120 DEG C., with a copolymer made of styrenic blocks and dienic blocks such as a styrenebutadiene disequenced or multisequenced or statistical copolymer having a molecular weight varying between 30,000 and 300,000 and crystallized sulfur which is not chemically bound. When homogeneity is obtained, a portion of said first composition is admixed for at least 15 minutes at a temperature of from 130 DEG C. to 230 DEG C., with a conventional bitumen (penetration 20-220) to form a fluid polymeric bitumen. The fluid polymeric bitumen obtained by the process of the present invention is an excellent product characterized by superior properties and this product can be used in conventional spreading means when applying coatings onto roads.

Inventors

  • 👤 Paul Maldonado
  • 👤 Henri Dayre
  • 👤 Germain Hagenbach

Bibliographic Details

Application Number —
Jurisdiction US
Data Source google_patents
Last Synchronized 2026-11-05 04:57
CPC Classifications
C; C10; C10C; C10C3/00; C10C3/02; C08; C08L; C08L95/00

Claims Analysis

Total Claims: 13
Claim 1
Independent Claim 101 words
A process for the preparation of a fluid bitumen-polymer composition which comprises: contacting, at a temperature of from 130° C. to 230° C., 85 to 95% by weight of a bitumen having a penetration of from 20 to 220 and 5 to 15% by weight of a second composition prepared by mixing a polystyrene-polydiene disequenced, multisequenced or statistical copolymer with a coal tar oil or a petroleum fraction having a distilling range at atmospheric pressure of about 100° to 350° C. and sulfur not chemically bonded and stirring the mixture of bitumen and said second composition for at least fifteen minutes.
Claim 2
Dependent Claim 101 words
A process for the preparation of a fluid bitumen-polymer composition which comprises: contacting, at a temperature of from 130° C. to 230° C., 85 to 95% by weight of a bitumen having a penetration of from 20 to 220 and 5 to 15% by weight of a second composition prepared by mixing a polystyrene-polydiene disequenced, multisequenced or statistical copolymer with a coal tar oil or a petroleum fraction having a distilling range at atmospheric pressure of about 100° to 350° C. and sulfur not chemically bonded and stirring the mixture of bitumen and said second composition for at least fifteen minutes.
Claim 3
Dependent Claim 57 words
A process according to claim 1, wherein said second composition is prepared by contacting, at a temperature of from 80° C. to 160° C., 75 to 80% by weight of a petroleum fraction, 20 to 25% by weight of a polystyrene-polydiene disequenced, multisequenced or statistical copolymer, and 0.5 to 1.5% by weight of sulfur not chemically bonded.
Claim 4
Dependent Claim 14 words
A process according to claim 2, wherein the temperature is 80° to 120° C.
Claim 5
Dependent Claim 29 words
A process according to claim 1 or 2, wherein the petroleum fraction is a naphthene-paraffinic petroleum fraction having an ASTM distillation range of from 150° C. to 250° C.
Claim 6
Dependent Claim 32 words
A process according to claim 1 or 2, wherein the polymer that forms part of said second composition is a polystyrene-polybutadiene disequenced copolymer having a molecular weight of from 70,000 to 200,000.
Claim 7
Dependent Claim 26 words
A process according to claim 1 or 2, wherein the chemically unbonded sulfur used for preparing said second composition is crystalline sulfur in the orthorhombic form.
Claim 8
Dependent Claim 26 words
A process according to claim 1 or 2, wherein the bitumen is an air blown direct distillation bitumen with initial penetration of from 20 to 220.
Claim 9
Dependent Claim 34 words
A process according to claim 1 or 2, wherein the sulfur is reacted in the presence of a vulcanization accelerator selected from the group consisting of a mercaptobenzothiazole, a di-orthotolylguanidine, and a metallic stearate.
Claim 10
Dependent Claim 12 words
A process according to claim 8, wherein the stearate is zinc stearate.
Claim 11
Dependent Claim 45 words
A process according to claim 1 or 2, wherein the fluid bitumen-polymer composition is obtained by adding said second composition to the bitumen to be modified and stirring the mixture for at least fifteen minutes at a temperature of from 130° C. to 230° C.
Claim 12
Dependent Claim 20 words
A process according to claim 10, wherein the mixture is stirred at a temperature of 140° to 180 ° C.
Claim 13
Dependent Claim 13 words
A fluid bitumen-polymer composition prepared by the process of claim 1 or 2.

References Cited (Backward Citations)

US3963659A Cited
US3992340A Cited
US4129542A Cited
US4130516A Cited

USPTO Annuity & Maintenance Windows

Annuity Stage Window Opens Payment Deadline Surcharge Period Until Estimated Fee Status
3.5 Years (Year 4) 1983-12-30 1984-06-30 1984-12-30 $2000.00 Window Closed / Lapsed
7.5 Years (Year 8) 1987-12-30 1988-06-30 1988-12-30 $3760.00 Window Closed / Lapsed